The combination of Additive Manufacturing (AM) and Hot Isostatic Pressing (HIP) offers great potential for industrial applications. Skilfully connecting AM and HIP creates a manufacturing process that unites the advantages of the two approaches. We demonstrate a production route for composite components by combining AM and HIP: a HIP capsule made of corrosion resistant steel is additively manufactured using Powder Bed Fusion with Laser Beam (LPBF). Before LPBF, the distortion and shrinkage of the capsule due to HIP is compensated by optimising the capsule’s geometry using Finite Element (FE) simulation of the HIP process. The capsule is filled with steel powder and manufactured by a conventional powder HIP. After HIP, the capsule remains as an outer layer on the component, so that a functional net-shape composite component is produced. Subsequent investigations show that a complex extruder screw segment can be successfully produced with a geometrical deviation smaller than 1.5%.
Powder metallurgical (PM) parts usually benefit from more homogenous and finer microstructures as opposed to conventionally processed material. In particular, hot isostatic pressing (HIP) combined with near-net-shape technologies can produce almost defect free PM tools with complex geometries. Recent advances in the plant technology of smaller HIP units allow the integration of hardening heat treatments in HIP processes. Thus, additional processing steps, transportation, energy consumption and cost are reduced. However, it is known that high pressure influences phase stability and transformation temperatures. Still, knowledge of the martensite start temperature (MS) is crucial for the design of hardening heat treatment. Since the influence of pressure on MS in HIP heat treatment is insufficiently investigated, it is the aim of this study to deploy a measurement method that allows to record MS as a function of pressure, temperature and cooling rate. Taking the hot working tool steel AISI H11 (X37CrMoV5-1, 1.2343) as the reference material, in this study for the first time the method of an in-situ electrical resistivity measurement was used to measure MS within a HIP. To investigate the influence of HIP pressure on Ms, resulting microstructures and hardness, specimens were austenitized at a temperature of TAUS = 1050 °C for tAUS = 30 min at pAUS = 25, 50, 100 or 150 MPa. Additionally, the MS temperature of the same material was determined by quenching dilatometry at ambient pressure for comparison purposes. Characterization of microstructures was conducted by scanning electron microscopy while hardness as an important technological property of tool steels was measured according to the Vickers method. Furthermore, the CALPHAD method was used to compute the thermodynamic influence of pressure on phase stabilities. The experimental results indicate that the method of in-situ resistivity measurement can be used to measure MS during an integrated HIP heat-treatment process. Besides, a stabilizing effect of pressure on the close packed crystal structure of the austenitic fcc phase is clearly detected, resulting in a reducing influence on the MS temperature of AISI H11 by up to 90 K.
The potential combinations of favorable properties give metal–ceramic laminates (MCLs) a high degree of application flexibility. However, the different thermal expansion coefficients (CTEs) and shrinkage rates of the metals and ceramics during the co-sintering process often lead to large internal stresses that cause undesired deformation or even production failures. In practice, the identification of manufacturable MCLs relies on the “trial and error” principle, which usually requires a long development period. Therefore, there is a great demand for analytic and numerical methods that allow the prediction of the deformation and manufacturability of MCLs during the co-sintering process. The main objective of this study is to investigate the curvature and stress distribution in the MCLs (steel 17-4PH/ ceramic 3Y-TZP) based on the analytic solution and finite element (FE) simulation. To achieve this, the Young’s moduli (E) and shear moduli (G) at high temperatures and the CTEs of both materials were measured. In addition, the curvatures and stress distributions of the two-layer and three-layer laminates were obtained based on the analytic method and FE simulation, which were in very good agreement. Furthermore, the influence of the CTE, Young’s modulus, height ratio, and interface on the curvature were studied. The results showed that the CTE and height ratio have a higher influence on the curvature in comparison to the Young’s modulus. The interface prevents the curvature significantly by assuming it to be a cohesive surface in the FE simulation. This provides hints to avoid delamination during the manufacturing process.
Recent studies have focused on the alloying of nitrogen (N) in high‐alloy stainless steels by powder bed fusion–laser beam/metal (PBF‐LB/M). However, N‐induced pore formation remains a challenge. To overcome this, a combined PBF‐LB/M and hot isostatic pressing (HIP) process is developed. AISI 304L stainless steel powder was mixed with silicon nitride (Si3N4) powder and processed by PBF‐LB/M, allowing partial retention of Si3N4. This helps to maintain sufficient N content while reducing pore formation. The microstructure is then homogenised by HIP. A major challenge of this process is to maintain the homogeneity of the deposited powder mixture on the powder bed to ensure a consistent N content in the final products. This study combines experimental and numerical methods to address this issue: scanning electron microscopy is used to characterize the microstructure and map the local N content, while various numerical studies based on the discrete element method are carried out to investigate the effects of layer thickness, substrate surface roughness, and powder properties on the intermediate product. The numerical approach effectively predicts the N content distribution and homogeneity on the powder bed. The models are validated with experimental data and optimal process conditions for PBF‐LB/M are identified.