Measuring temperatures in the material during laser metal deposition (LMD) has an inherent challenge caused by the laser. When thermocouples are radiated by the high intensity laser light overheating occurs which causes the thermocouple to fail. Another identified difficulty is that when the laser passes a thermocouple, emitted light heats the thermocouple to a higher temperature than the material actually experience. In order to cope with these challenges, a method of measuring temperatures during LMD of materials using protective sheets has been developed and evaluated as presented in this paper. The method has substantially decreased the risk of destroying the thermocouple wires during laser deposition. Measurements using 10 mm2 and 100 mm2 protective sheets have been compared. These measurements show small variations in the cooling time (∼0.1 s from 850°C to 500°C) between the small and large protective sheets which indicate a negligible effect on the temperature measurement.
The weldability in terms of susceptibility towards hot cracking of selective laser melted (SLM) Alloy 718 was investigated and wrought Alloy 718 was used as reference material. Varestraint testing was carried out by means of investigating the weldability in three conditions; (1) SLM as-built, (2) hot isostatic pressing at 1160°C at 105 MPa for 3 h and (3) wrought Alloy 718 in the mill-annealed condition. The material exhibited intergranular cracking in all three conditions; however, the SLM HIPed condition had an increased magnitude of crack susceptibility at all strain levels. The increased sensitivity of the HIPed material was due to the significantly larger grain size in comparison. The SLM as-built condition showed the same degree of cracking as the wrought material.
The weldability of additive manufactured Alloy 718 was investigated in various heat-treated conditions. The microstructure of the base metal was examined in detail in order to understand the effect of different pre-weld heat treatments; i.e., solution, solution and aging, and hot isostatic pressing. After welding, the variation in total crack lengths, maximum crack length and the total number of cracks in the heat affected zone (HAZ) were used as criteria for the cracking susceptibility of each material condition where wrought Alloy 718 was used as the reference material. Selective laser melting (SLM) manufactured Alloy 718 was susceptible to HAZ cracking in all material conditions. Total crack lengths in HAZ were highest in the SLM as-built condition and lowest in the SLM hot isostatic pressed condition. The cracks that were found in the HAZ of the welded materials consisted of liquation cracks, with eutectic product surrounding the cracks, as well as cracks from which liquation products were absent.
Evaluation of residual stress in the weld toe region is of critical importance. In this paper, the residual stress distribution both near the surface and in depth around the weld toe was investigated using neutron diffraction, complemented with X-ray diffraction. Measurements were done on a 1300 MPa yield strength steel welded using a Low Transformation Temperature (LTT) consumable. Near surface residual stresses, as close as 39 µm below the surface, were measured using neutron diffraction and evaluated by applying a near surface data correction technique. Very steep surface stress gradients within 0.5 mm of the surface were found both at the weld toe and 2 mm into the heat affected zone (HAZ). Neutron results showed that the LTT consumable was capable of inducing near surface compressive residual stresses in all directions at the weld toe. It is concluded that there are very steep stress gradients both transverse to the weld toe line and in the depth direction, at the weld toe in LTT welds. Residual stress in the base material a few millimeters from the weld toe can be very different from the stress at the weld toe. Care must, therefore, be exercised when relating the residual stress to fatigue strength in LTT welds.