Recently, glasses have gained great interest for use as scintillators owing to lots of industrial benefits such as ease of producing customizable shapes and low production cost. Herein, the Er3+-activated BaO–Nb2O5–TeO2 glasses were fabricated for the development of NIR glass scintillators. The Er3+-activated BaO–Nb2O5–TeO2 glasses exhibited efficient photoluminescence and scintillation that originated from the 4f→4f transition of Er3+. Their quantum yields in photoluminescence were 80% (0.1%Er2O3), 81% (0.5%Er2O3), and 61% (1.0%Er2O3). Further, an almost linear correlation between an X-ray dose rate and NIR scintillation intensity was observed in the 0.5–5000 mGy h−1 dose rate range. Interestingly, the lowest detectable dose rate limit (0.5 mGy h−1) was lower than that of Er-doped Bi4Ge3O12 and Nd-doped GdVO4 single crystals. Further, afterglow levels of the non-doped and Er3+-activated BaO–Nb2O5–TeO2 glasses were about 600 ppm. The observed NIR scintillation properties indicated that the Er3+-activated tellurite glasses should be promising compounds for NIR-emitting scintillators.
The photoluminescence (PL), scintillation, and dosimetric properties of Tb-doped MgAl 2 O 4 single crystals were evaluated. In terms of PL and scintillation properties, the Tb-doped crystals showed some emission peaks ascribed to the 4f–4f transitions of the Tb 3+ ion. In addition, the optically and thermally stimulated luminescence (OSL and TSL) spectra showed emission peaks considered to be due to the Tb 3+ ion. TSL dose response functions were also evaluated, and the Tb-doped crystals showed linear responses from 0.01 mGy.
Undoped, 0.5, 1.0, and 2.0% Nd-doped Bi4Si3O12 (BSO) crystals were synthesized by the floating zone method. Regarding photoluminescence (PL) properties, all samples had emission peaks due to the 6p–6s transitions of Bi3+ ions. In addition, the Nd-doped samples had emission peaks due to the 4f–4f transitions of Nd3+ ions as well. The PL quantum yield of the 0.5, 1.0, and 2.0% Nd-doped samples in the near-infrared range were 67.9, 73.0, and 56.6%, respectively. Regarding X-ray-induced scintillation properties, all samples showed emission properties similar to PL. Afterglow levels at 20 ms after X-ray irradiation of the undoped, 0.5, 1.0, and 2.0% Nd-doped samples were 192.3, 205.9, 228.2, and 315.4 ppm, respectively. Dose rate response functions had good linearity from 0.006 to 60 Gy/h for the 1.0% Nd-doped BSO sample and from 0.03 to 60 Gy/h for the other samples.
9 April 2020 in Journal of Materials Science: Materials in Electronics