Undoped, 0.5, 1.0, and 2.0% Nd-doped Bi4Si3O12 (BSO) crystals were synthesized by the floating zone method. Regarding photoluminescence (PL) properties, all samples had emission peaks due to the 6p–6s transitions of Bi3+ ions. In addition, the Nd-doped samples had emission peaks due to the 4f–4f transitions of Nd3+ ions as well. The PL quantum yield of the 0.5, 1.0, and 2.0% Nd-doped samples in the near-infrared range were 67.9, 73.0, and 56.6%, respectively. Regarding X-ray-induced scintillation properties, all samples showed emission properties similar to PL. Afterglow levels at 20 ms after X-ray irradiation of the undoped, 0.5, 1.0, and 2.0% Nd-doped samples were 192.3, 205.9, 228.2, and 315.4 ppm, respectively. Dose rate response functions had good linearity from 0.006 to 60 Gy/h for the 1.0% Nd-doped BSO sample and from 0.03 to 60 Gy/h for the other samples.
Mg4Ta2O9 single crystals doped with 0.01, 0.1, and 1% Er were grown using the floating zone method, and their photoluminescence and scintillation properties were studied. X-ray diffraction analysis confirmed that all samples had a hexagonal structure of Mg4Ta2O9. The samples showed that the emission peak at 1550 nm was due to 4f−4f transitions of Er3+ ions, with quantum yields of 32.9, 46.6, and 18.0% for 0.01, 0.1, and 1% doping concentrations, respectively. All samples showed scintillation with a broad emission band at 350 nm due to charge transfer from Ta5+ to O2− ions and emission peak at 1550 nm due to 4f−4f transition of Er3+ ions. The dose rate response functions showed that the detection limit for all samples was 0.06 Gy/h for scintillation detector applications.
13 September 2022 in Radiation Physics and Chemistry