Recently, glasses have gained great interest for use as scintillators owing to lots of industrial benefits such as ease of producing customizable shapes and low production cost. Herein, the Er3+-activated BaO–Nb2O5–TeO2 glasses were fabricated for the development of NIR glass scintillators. The Er3+-activated BaO–Nb2O5–TeO2 glasses exhibited efficient photoluminescence and scintillation that originated from the 4f→4f transition of Er3+. Their quantum yields in photoluminescence were 80% (0.1%Er2O3), 81% (0.5%Er2O3), and 61% (1.0%Er2O3). Further, an almost linear correlation between an X-ray dose rate and NIR scintillation intensity was observed in the 0.5–5000 mGy h−1 dose rate range. Interestingly, the lowest detectable dose rate limit (0.5 mGy h−1) was lower than that of Er-doped Bi4Ge3O12 and Nd-doped GdVO4 single crystals. Further, afterglow levels of the non-doped and Er3+-activated BaO–Nb2O5–TeO2 glasses were about 600 ppm. The observed NIR scintillation properties indicated that the Er3+-activated tellurite glasses should be promising compounds for NIR-emitting scintillators.
Undoped, 0.5, 1.0, and 2.0% Nd-doped Bi4Si3O12 (BSO) crystals were synthesized by the floating zone method. Regarding photoluminescence (PL) properties, all samples had emission peaks due to the 6p–6s transitions of Bi3+ ions. In addition, the Nd-doped samples had emission peaks due to the 4f–4f transitions of Nd3+ ions as well. The PL quantum yield of the 0.5, 1.0, and 2.0% Nd-doped samples in the near-infrared range were 67.9, 73.0, and 56.6%, respectively. Regarding X-ray-induced scintillation properties, all samples showed emission properties similar to PL. Afterglow levels at 20 ms after X-ray irradiation of the undoped, 0.5, 1.0, and 2.0% Nd-doped samples were 192.3, 205.9, 228.2, and 315.4 ppm, respectively. Dose rate response functions had good linearity from 0.006 to 60 Gy/h for the 1.0% Nd-doped BSO sample and from 0.03 to 60 Gy/h for the other samples.
Nd-doped CaWO4 single crystals with dopant concentrations of 0.1, 0.5, and 1% were synthesized by the floating zone method. The transmission, photoluminescence, and scintillation properties were evaluated from ultraviolet to near-infrared (NIR) ranges. An emission peak due to transitions of the host was observed at 400 nm, and several sharp peaks originating from Nd3+ 4f–4f transitions were confirmed at 900, 1060, and 1300 nm. The quantum yields of 0.1, 0.5, and 1% Nd-doped samples were 70.7, 79.5, and 61.2%, respectively, when monitored, and excited wavelengths were 750–1500 nm and 590 nm. Decay times consistent with typical Nd3+ transitions were obtained when NIR ranges were monitored. Additionally, the energy transfer between the host and Nd3+ occurred according to the decay measurement. The relationship between X-ray irradiated dose rate and intensity in the range of NIR was investigated by combining the crystals with an InGaAs-photodiode. The lowest detectable dose rate retaining the linearity of the present crystals was 0.3–0.06 Gy/h.
Mg4Ta2O9 single crystals doped with 0.01, 0.1, and 1% Er were grown using the floating zone method, and their photoluminescence and scintillation properties were studied. X-ray diffraction analysis confirmed that all samples had a hexagonal structure of Mg4Ta2O9. The samples showed that the emission peak at 1550 nm was due to 4f−4f transitions of Er3+ ions, with quantum yields of 32.9, 46.6, and 18.0% for 0.01, 0.1, and 1% doping concentrations, respectively. All samples showed scintillation with a broad emission band at 350 nm due to charge transfer from Ta5+ to O2− ions and emission peak at 1550 nm due to 4f−4f transition of Er3+ ions. The dose rate response functions showed that the detection limit for all samples was 0.06 Gy/h for scintillation detector applications.