During the service life of offshore pipelines, many start-up and shut-down cycles take place, possibly leading to significant cyclic loads. Fatigue failure may occur, resulting in serious environmental pollution and loss of property. The study aims to assess the fatigue strength of single-sided girth welds in offshore pipelines under these specific fatigue loads. The longitudinal stress range caused by the variation of the pipeline’s internal pressure and temperature is calculated. The effective notch strain approach is used to assess the fatigue strength of welds. The plastic behaviour of the weld root is investigated for a study case to justify the use of low-cycle fatigue assessment approaches. The effect of weld root geometry on the notch stress factor is studied to identify the dominant geometrical parameters. The fatigue strength of the study case is assessed, and some limitations of the assessment are discussed. The results show that the plastic behaviour of the weld root is only significant for severe local stress concentrations, which is mainly governed by the axial misalignment, weld root angle and the weld root bead width. If the fatigue damage at failure is 0.1, a limited number of start-up and shut-down cycles are allowed during the service life of the pipeline for the study case, indicating the necessity of fatigue strength assessment.
The study aims to investigate the impact of uniform, grooving and non-uniform corrosion degradation on the hot-spot stresses of a T-shaped tubular joint using the finite element method. The through-thickness linearization method is employed to estimate the hot-spot stresses, allowing a more reasonable consideration of the effect of grooving corrosion and non-unform corrosion. The grooving corrosion degradation is modelled assuming that the corrosion rate of the weld metal is 1.4 times that of the base metal. The non-uniform corrosion is modelled by moving the nodes around the weld by a random distance along the direction perpendicular to the surface. The random distances are generated based on the surface roughness parameter Ra. The results indicate that the stress concentration factor (SCF) increases with the uniform corrosion depth. The grooving corroded tubular joint results in a higher SCF than those of the corresponding uniformly corroded tubular joint. The non-uniform corrosion can lead to SCF deviations from the SCF of the uniformly corroded tubular joint. The SCF deviation at the critical region follows the normal distribution, and its standard deviation increases with Ra.
Currently, magnesium alloys are extensively used owing to their excellent comprehensive mechanical properties. Rolling is a primary method used to produce magnesium alloy plates. However, so far, only few reports have been investigated about the straightening of rolled magnesium alloy plates. In this study, multi-roller straightening of the magnesium alloy plate is theoretically analyzed and simulated using the finite element method. Multi-roller straightening process of the magnesium alloy plate was performed as follows: the original bending curvature that exhibited large numerical differences in different directions was gradually reduced through reasonable distribution of the plastic deformation rate of each straightening roller system. Finite element simulation and experimental results are obtained for room-temperature magnesium alloy plate straightening at four different plastic deformation rates. However, the straightening effect is minimal when the micro plastic deformation rate is used for straightening the magnesium alloy plate with an initial curvature, this is because the reverse bending rate required for straightening is not attained. Straightening effect can be achieved with low, moderate, or high plastic deformation rates, and the flatness achieved after straightening at a low plastic deformation rate is relatively better than that obtained using moderate and high deformation rates. Both perpendicular to and along the straightening direction, the residual stress after straightening is less than that observed before straightening. Furthermore, the residual stress after straightening at a low plastic deformation rate is the lowest and uniformly distributed.
Hollow mesoporous Fe3O4 microspheres are attractive as corrosion inhibitor carriers for their structural stability, and strong superparamagnetic properties. Here, the morphology-controlled magnetic hollow mesoporous Fe3O4 nanocarriers (MHMNs) with saturation magnetization of ca. 77 emu/g were fabricated by self-template etching route. Serial characterization results showed that the sample (MHMNs-7.0), obtained by etching MHMNs with 7.0 mg/mL of the oxalic acid solution, presented the largest cavity volume and a rich pore structure, which promotes its high loading capacity of 77.6% for 2-mercaptobenzothiazole (MBT) inhibitor. The resulting material could be used as the carrier for loading various types of inhibitors, e.g., MBT, Ce3+, benzotriazole (BTA), and under negative vacuum treatment. The release behavior of the obtained composite inhibitors was detected by UV-vis spectroscopy, and the inhibition behavior of the composite inhibitors for mild steel in 3.5% NaCl solution was evaluated by electrochemical impedance spectroscopy and immersion tests. The results showed that all of the as-obtained composites presented magnetic-controlled release properties and good inhibition performance. Without the external magnetic field (no MF mode), the release of MBT from MHMNs-7.0/MBT mainly involved Fickian diffusion. Under the application of a magnetic field (MF ON mode), the release behavior was dominated by a swelling mechanism, Fickian diffusion, and diffusion between magnetic particles. The nanocomposite inhibitor had good inhibition efficiency for carbon steel in 3.5% NaCl solution with a maximum of 93.66%, and its continuous release properties enabled it to exhibit long-term corrosion inhibition performance.
3 July 2019 in Journal of Chemical & Engineering Data