Electrospun polymer nanofibers (EPNF) constitute one of the most important nanomaterials with diverse applications. An overall review of EPNF is presented here, starting with an introduction to the most attractive features of these materials, which include the high aspect ratio and area to volume ratio as well as excellent processability through various production techniques. A review of these techniques is featured with a focus on electrospinning, which is the most widely used, with a detailed description and different types of the process. Polymers used in electrospinning are also reviewed with the solvent effect highlighted, followed by a discussion of the parameters of the electrospinning process. The mechanical properties of EPNF are discussed in detail with a focus on tests and techniques used for determining them, followed by a section for other properties including electrical, chemical, and optical properties. The final section is dedicated to the most important applications for EPNF, which constitute the driver for the relentless pursuit of their continuous development and improvement. These applications include biomedical application such as tissue engineering, wound healing and dressing, and drug delivery systems. In addition, sensors and biosensors applications, air filtration, defense applications, and energy devices are reviewed. A brief conclusion is presented at the end with the most important findings and directions for future research.
Conventional mechanical machining of composite is a challenging task, and thus, electric discharge machining (EDM) was used for the processing of the developed material. The processing of developed composite using different electrodes on EDM generates different surface characteristics. In the current work, the effect of tool material on the surface characteristics, along with other input parameters, is investigated as per the experimental design. The experimental design followed is an RSM-based Box–Behnken design, and the input parameters in the current research are tool material, current, voltage, pulse-off time, and pulse-on time. Three levels of each parameter are selected, and 46 experiments are conducted. The surface roughness (Ra) is investigated for each experimental setting. The machine learning approach is used for the prediction of surface integrity by different techniques, namely Xgboost, random forest, and decision tree. Out of all the techniques, the Xgboost technique shows maximum accuracy as compared to other techniques. The analysis of variance of the predicted solutions is investigated. The empirical model is developed using RSM and is further solved with the help of a teaching learning-based algorithm (TLBO). The SR value predicted after RSM and integrated approach of RSM-ML-TLBO are 2.51 and 2.47 µm corresponding to Ton: 45 µs; Toff: 73 µs; SV:8V; I: 10A; tool: brass and Ton: 47 µs; Toff: 76 µs; SV:8V; I: 10A; tool: brass, respectively. The surface integrity at the optimized setting reveals the presence of microcracks, globules, deposited lumps, and sub-surface formation due to different amounts of discharge energy.
In the present research, AISI P20 mold steel was processed using the milling process. The machining parameters considered in the present work were speed, depth of cut (DoC), and feed (F). The experiments were designed according to an L27 orthogonal array; therefore, a total of 27 experiments were conducted with different settings of machining parameters. The response parameters investigated in the present work were material removal rate (MRR), surface roughness (Ra, Rt, and Rz), power consumption (PC), and temperature (Temp). The machine learning (ML) approach was implemented for the prediction of response parameters, and the corresponding error percentage was investigated between experimental values and predicted values (using the ML approach). The technique for order of preference by similarity to ideal solution (TOPSIS) approach was used to normalize all response parameters and convert them into a single performance index (Pi). An analysis of variance (ANOVA) was conducted using the design of experiments, and the optimized setting of machining parameters was investigated. The optimized settings suggested by the integrated ML–TOPSIS approach were as follows: speed, 150 m/min; DoC, 1 mm; F, 0.06 mm/tooth. The confirmation results using these parameters suggested a close agreement and confirmed the suitability of the proposed approach in the parametric evaluation of a milling machine while processing P20 mold steel. It was found that the maximum percentage error between the predicted and experimental values using the proposed approach was 3.43%.
Environmentally friendly biopolymer nanofibrous composite membranes with enhanced mechanical properties and thermal stability were fabricated via electrospinning with different compositions of polylactic acid (PLA) and cellulose acetate (CA). Firstly, PLA and CA composite membranes were prepared and optimized. Then, the optimized membranes were annealed at temperatures ranging from 80 °C to 140 °C, for annealing times between 30 and 90 min. The developed membranes were characterized by FE-SEM, XRD, FR-IT, TGA, DSC, tensile testing, water contact angle, and resistance to hydrostatic pressure. PLA 95-CA 5 was the optimum composite, with a tensile strength 9.3 MPa, an average fiber diameter of 432 nm, a water contact angle of 135.7°, and resistance to a hydrostatic pressure of 16.5 KPa. Annealing resulted in further improvements in different properties. The annealed membranes had thermally stable microporous structures, without shrinkage or deterioration in nanofiber structure, even at an annealing time of 90 min and an annealing temperature of 140 °C. By increasing either the annealing time or temperature, the crystallinity and rigidity of the nanofiber composite membranes were increased. The annealed membrane demonstrated a tensile strength of 12.3 MPa, a water contact angle of 139.2°, and resistance to a hydrostatic pressure of 36 KPa. Electrospinning of PLA-CA composite membranes with enhanced mechanical properties and thermal stability will pave the way for employing PLA-based membranes in various applications.
In this study, multifunctional nanocomposite membranes were fabricated using biopolymeric polylactic acid (PLA) and cellulose acetate (CA) composites via electrospinning. The hydrophobic nanocomposite membranes were reinforced with varying concentrations of silicon dioxide (silica/SiO2) nanoparticles. The developed PLA–CA–SiO2 nanofibrous membranes are characterized using field emission scanning electron microscopy (FE- energy-dispersive SEM), energy-dispersive X-ray (EDX), elemental mapping, X-ray diffraction analysis (XRD), Fourier-transform infrared spectroscopy (FT–IR), thermal gravimetric analysis (TGA), and differential scanning calorimetry (DSC) techniques. Various physical and mechanical properties of the bio-nanocomposite membrane, such as tensile testing, infrared thermal imaging, ultraviolet–visible spectroscopy (UV–Vis), water contact angle, hydrostatic pressure resistance, and breathability are also investigated. The analysis revealed that a small concentration of silica nanoparticles improves the morphological, mechanical, and thermal characteristics of nanocomposite membranes. The addition of silica nanoparticles improves the UV (A & B), visible and infrared blocking efficiency while also enhancing the waterproofness of protective textiles. The PLA–CA–SiO2 biopolymer nanocomposite membrane has a fibrous microstructure and demonstrated the tensile strength of 11.2 MPa, a Young’s modulus of 329 MPa, an elongation at break of 98.5%, a hydrostatic pressure resistance of 27 kPa, and a water contact angle of 143.7°. The developed electrospun composite membranes with improved properties provide strong potential to replace petroleum-based membranes with biopolymer-based alternatives, promising improved and wider usage for bio-related applications.
Casting-related microstructural variations can affect the mechanical performance of Al–Cu–Mg–Ag alloys. This study examines a novel processing route in which a single equal channel angular pressing (ECAP) pass was introduced before solution treatment (Route 2) and compares it with conventional heat treatment (Route 1) for alloys containing 0.3 and 0.6 wt.% Ag. Increasing the Ag content from 0.3 to 0.6 wt.% increased the hardness after solution treatment from 93 to 109 HV. Ageing at 190 °C further increased strength, with the 0.3 wt.% Ag alloy processed by Route 2 showing the highest tensile performance, with a UTS of 317 MPa and an approximately 14% elongation. Optical and electron microscopy showed a finer and more uniform microstructure in the ECAP-processed condition, together with differences in the morphology and distribution of second-phase constituents. The fracture surfaces also differed markedly between the two routes. The peak-aged Route 1 condition showed predominantly intergranular fracture associated with precipitate-free zones and coarse grain-boundary intermetallic particles, whereas Route 2 showed a more ductile fracture surface with numerous deep, equiaxed dimples formed by microvoid coalescence. These results show that introducing ECAP before solution treatment can improve the mechanical and fracture behavior of Al–Cu–Mg–Ag alloys and offers a useful alternative to the conventional processing sequence.