This study provides novel insights into the nuanced impact of time gaps on the buildability of cement mixtures within the 3D printing process. In contrast to studies predominantly focused on rheological properties, this research addresses essential factors such as printed structure size, which inevitably affect the temporal intervals between layer depositions and consequently shape the buildability outcome. The investigation encompasses cement mixtures with diverse water-to-cement ratios (ranging from 0.26 to 0.36), varied setting accelerator concentrations (1.0 to 2.0 wt.%), and superplasticizer contents (0.25 and 0.5 wt.%), all explored across different time gaps (ranging from 5 to 25 min). The evaluation of buildability involves a meticulous assessment of the deformation of the bottom layer induced by adjacent layers. The findings underscore the substantial role played by chemical admixtures in fine-tuning rheological properties specific to each time gap, thereby influencing the size of the printed structure. The impact of the accelerator admixture is evident in its ability to reduce the minimum time gap required for optimal buildability while the superplasticizer emerges as a key player in enhancing fluidity without compromising the load-bearing capacity of the printed structures. To predict buildability for a given time gap, the study leverages the results of spreading diameter from the flow table test and the setting time from the Vicat test. Lastly, this study extends its scope to unveil insights into the intricate interplay between time gap and printing speed for 3D printed real-scale constructions by examining the relationship among these parameters across constructions with diverse built areas.
Durability is crucial for reinforced concrete, directly influencing the service life of structures. The presence of aggressive agents, especially chloride ions, significantly impacts durability. This study investigates the differences between ASTM C1202 and IBRACON/NT Build 492 standards in concrete containing various types of cement designed for a characteristic compressive strength of 40 MPa. Forty-eight cylindrical samples were prepared using eight types of Portland cement, including those with blast furnace slag, filler, and pozzolanic materials. Chloride migration tests were performed according to the ASTM C1202/2022 and IBRACON/NT Build 492/1999 methodologies. At a 95% confidence level, the results indicated that concrete made with filler-containing cement (PCII F-SR and PC II F) showed the poorest chloride resistance, with charge passing values exceeding 4000 coulombs (ASTM C1202) and diffusion coefficients above 10 × 10−12 m2/s (IBRACON/NT Build 492). In contrast, concrete containing high slag cement (PC III-SR) and pozzolan cement (PC IV) demonstrated superior resistance to chloride penetration, with charge passing values below 1500 coulombs and diffusion coefficients under 5 × 10−12 m2/s. Notably, discrepancies in classification were observed, as PC II Z (fly-ash based) and PC II E-SR (slag-based) received different ratings under the two methods. ASTM C1202 was found to be more stringent than NT Build 492, highlighting significant variations in the classification criteria between these standards. Based on the findings, new interval values are proposed for classifying concrete regarding the risk of chloride ion penetration, particularly for the ASTM C1202 standard, in order to better align with performance-based durability criteria and improve classification accuracy.
1 January 2022 in Revista IBRACON de Estruturas e Materiais
This work aims to present a methodology for the elaboration of a deformation map in a Portland cement concrete specimen to predict fractures caused by axial compression stresses, using the technique of Digital Image Correlation - DIC 2D. For this purpose, 5 concrete specimens with compressive strength expected at 28 days fck of 40 MPa were analyzed, which were tested in the ABNT NBR 5739/2018 standard - compression test of cylindrical concrete specimens. During the test, the necessary digital images were acquired in the DIC-2D array. These images were subsequently processed, and the results interpreted statistically. According to the result of the correlation of images obtained, it was found that 67% of the specimens had regions of accumulation of stresses that indicated in advance the location of the rupture, which enabled the development of a fracture prediction map. The results obtained in the research showed that the methodology used by means of the DIC-2D arrangement was able to predict the place where the rupture in the specimens occurred.
Chloride ion penetration is one of the most aggressive threats to reinforced concrete, as it triggers the electrochemical corrosion of steel reinforcement, compromising structural integrity and durability. Chloride ingress occurs through the porous structure of concrete, making permeability control crucial for enhancing structural longevity. Fiber-reinforced concrete (FRC) is widely used to improve durability; however, the effects of different fiber types on chloride resistance remain unclear. This study examines the influence of glass and polypropylene fibers on concrete’s microstructure and chloride penetration resistance. Cylindrical specimens were prepared, including a reference mix without fibers and mixes with 0.25% and 0.50% fiber content by volume. Both fiber types were tested for chloride resistance. The accelerated non-steady-state migration method was employed to determine the resistance coefficients to chloride ion penetration, while X-ray macrofluorescence (MacroXRF) mapped the chlorine infiltration depth in the samples. Compressive strength decreased in all fiber-reinforced samples, with 0.50% glass fiber leading to a 56% reduction in strength. Nevertheless, the XRF results showed that a 0.25% fiber content significantly reduced chloride penetration, with polypropylene fibers outperforming glass fibers. These findings highlight the critical role of fiber type and volume in improving concrete durability, offering insights for designing long-lasting FRC structures in chloride-rich environments.
Engineers commonly use the 28-day characteristic strength of concrete for project calculations, but this may not reflect the full-strength potential, especially in concretes with supplementary cementitious materials (SCMs). SCMs, known for their slow reactivity, often delay optimal strength beyond 28 days, requiring higher cement content to speed up early strength development, thus increasing production costs. This study examined the relationship between concrete age and mechanical strength across eight cement types, including tests for axial compression, water absorption, void index, and specific mass. The findings showed that pozzolan and slag cements gained significant long-term strength due to slow pozzolanic reactions. Conversely, limestone filler mixes had lower initial strength and slower progress, likely due to increased porosity from fine fillers. A correlation was found between higher pozzolan content and improved durability, including reduced water absorption and void index. Cost analysis indicated that optimizing cement mix designs for targeted strength levels could reduce production costs, especially for concretes with high SCM content. Using long-term characteristic strength rather than the traditional 28-day strength resulted in approximately 14% savings, particularly for slag- and pozzolan-based cements. The savings were less significant for other cement types, emphasizing the importance of adjusting mix designs based on both performance and financial considerations.
The problems generated by the ornamental stone extraction and processing industry caused by the inadequate disposal of this waste can negatively affect rivers, lakes, streams, and even natural water reservoirs. This study discusses and evaluates the potentiality and challenges of dimension stone waste (DSW) recycling generated from a Brazilian dimension stone processing industry in Portland cement formulations. Cement pastes with different amounts of DSW (10–30 wt.%), quartz (10 wt.%), and calcium carbonate (10 wt.%) were prepared and characterized in the fresh and hardened states. The results showed that DSW can be used in cement formulations, and its reactivity is governed by the size of the particles. With up to 10% DSW in place of cement, the samples had greater workability and compressive strength at 28 days compared with the reference mix. However, the strength was lower at early ages (3 and 7 days). When DSW is milled, the strength of the samples containing the waste matched the reference values at all ages, and the recommended replacement limit rose to 20%. On the other hand, the particle size reduction significantly decreased the workability. The use of DSW in cement-based formulations is encouraged due to the strong presence of stone processing and cement companies in Brazil and worldwide.