Representative Publications

View All Publications
9 June 2021 in Metals
Verified
Journal Article
Open access
PDF file
MCMukti Chaturvedi
Mukti Chaturvedi
Elena SCUTELNICUElena SCUTELNICU
Elena SCUTELNICU
CRCarmen Catalina Rusu
Carmen Catalina Rusu
LMLuigi Renato Mistodie
Luigi Renato Mistodie
DMDanut Mihailescu
Danut Mihailescu
ASArungalai Vendan S
Arungalai Vendan S
Wire arc additive manufacturing (WAAM) is a fusion manufacturing process in which the heat energy of an electric arc is employed for melting the electrodes and depositing material layers for wall formation or for simultaneously cladding two materials in order to form a composite structure. This directed energy deposition-arc (DED-arc) method is advantageous and efficient as it produces large parts with structural integrity due to the high deposition rates, reduced wastage of raw material, and low consumption of energy in comparison with the conventional joining processes and other additive manufacturing technologies. These features have resulted in a constant and continuous increase in interest in this modern manufacturing technique which demands further studies to promote new industrial applications. The high demand for WAAM in aerospace, automobile, nuclear, moulds, and dies industries demonstrates compatibility and reflects comprehensiveness. This paper presents a comprehensive review on the evolution, development, and state of the art of WAAM for non-ferrous materials. Key research observations and inferences from the literature reports regarding the WAAM applications, methods employed, process parameter control, optimization and process limitations, as well as mechanical and metallurgical behavior of materials have been analyzed and synthetically discussed in this paper. Information concerning constraints and enhancements of the wire arc additive manufacturing processes to be considered in terms of wider industrial applicability is also presented in the last part of this paper.

16 May 2021 in Metals
Verified
Journal Article
Open access
PDF file
Elena SCUTELNICUElena SCUTELNICU
Elena SCUTELNICU
MIMihaela Iordachescu
Mihaela Iordachescu
CRCarmen Catalina Rusu
Carmen Catalina Rusu
DMDanut Mihailescu
Danut Mihailescu
José L. OCAÑAJosé L. OCAÑA
José L. OCAÑA
This paper addresses the metallurgical and mechanical characterization of dissimilar joints made by laser autogenous welding between thin sheets of low-carbon steel (CS) and austenitic stainless steel (SS). The welding technology applied, previously optimized to produce sound dissimilar joints, is based on the heat source displacement from the weld gap centerline towards CS, in order to reduce the SS overheating. The research includes optical microscopy observations, energy dispersive X-ray analysis (EDX) to assess the wt% of Cr, Ni, and Fe in all regions of the dissimilar welded joint, hardness measurements, and tensile tests of transverse-welded flat specimens. In comparison with classical determination of the joint overall mechanical characteristics, the novelty of this research consists of experimental assessment of the local mechanical behavior of the fusion and heat affected zones by using a digital image correlation technique (VIC-2D). This is an efficient tool for determining the constitutive properties of the joint, useful for modelling the mechanical behavior of materials and for verifying the engineering predictions. The results show that the positive difference in yielding between the weld metal and the base materials protects the joint from being plastically deformed. As a consequence, the tensile loading of flat transverse specimens generates the strain localization and failure in CS, far away from the weld.

5 April 2017 in Materials and Manufacturing Processes
Verified
Journal Article
Closed access
TCT. Chinnadurai
T. Chinnadurai
SVS. Arungalai Vendan
S. Arungalai Vendan
CRCarmen Catalina Rusu
Carmen Catalina Rusu
Elena SCUTELNICUElena SCUTELNICU
Elena SCUTELNICU
The polypropylene material meets the needs and requirements in automotive industry due to its features such as wide range of physical properties, ease of processing, and low cost. This research has focused on the investigation of the behavior of polypropylene during ultrasonic welding process. The lap welded samples were examined by modern methods such as Differential Scanning Calorimetry (DSC), Thermogravimetric Analysis (TGA), and Fourier Transform Infrared Spectroscopy (FTIR). Also, the morphology of the non-welded and welded regions of the polypropylene samples was analyzed by Scanning Electronic Microscopy (SEM) method. TGA and DSC results showed a negligible difference between the mass loss of the molded and the welded propylene materials. Furthermore, the SEM images revealed the formation of voids in close correlation with vibration amplitude. The weld strength and bond integrity appears to be higher for higher vibrations, emphasizing that the lap joint interface strength is higher when the tendency of voids formation is decreasing. The stress-strain curve of the material, plotted for three ultrasonic welding variants, illustrated that increasing the main process parameters (pressure, time, and vibration amplitude) makes the weld strength higher, but a decrease in plasticity was noticed in the welded polypropylene samples.

6 May 2022 in Engineering Failure Analysis
Verified
Journal Article
Closed access
MIMihaela Iordachescu
Mihaela Iordachescu
AVAndrés Valiente
Andrés Valiente
MAMaricely De Abreu
Maricely De Abreu
PSPatricia Santos
Patricia Santos
Elena SCUTELNICUElena SCUTELNICU
Elena SCUTELNICU

11 August 2022 in Materials
Verified
Journal Article
Open access
PDF file
AMAndrei Mitru
Andrei Mitru
ASAugustin Semenescu
Augustin Semenescu
GSGeorge Simion
George Simion
Elena SCUTELNICUElena SCUTELNICU
Elena SCUTELNICU
Ionelia VoiculescuIonelia Voiculescu
Ionelia Voiculescu
The welding process of dissimilar metals, with distinct chemical, physical, thermal, and structural properties, needs to be studied and treated with special attention. The main objectives of this research were to investigate the weldability of the dissimilar joint made between the 99.95% Cu pipe and the 304L stainless steel plate by robotic Gas Tungsten Arc Welding (GTAW), without filler metal and without preheating of materials, and to find the optimum welding regime. Based on repeated adjustments of the main process parameters—welding speed, oscillation frequency, pulse frequency, main welding current, pulse current, and decrease time of welding current at the process end—it was determined the optimum process and, further, it was possible to carry out joints free of cracks and porosity, with full penetration, proper compactness, and sealing properties, that ensure safety in operating conditions. The microstructure analysis revealed the fusion zone as a multi-element alloy with preponderant participation of Cu that has resulted from mixing the non-ferrous elements and iron. Globular Cu- or Fe-rich compounds were developed during welding, being detected by Scanning Electron Microscope (SEM). Moreover, the Energy Dispersive X-ray Analysis (EDAX) recorded the existence of a narrow double mixing zone formed at the interface between the fusion zone and the 304L stainless steel that contains about 66 wt.% Fe, 18 wt.% Cr, 8 wt.% Cu, and 4 wt.% Ni. Due to the formation of Fe-, Cr-, and Ni-rich compounds, a hardness increase up to 127 HV0.2 was noticed in the fusion zone, in comparison with the copper material, where the average measured microhardness was 82 HV0.2. The optimization of the robotic welding regime was carried out sequentially, by adjusting the parameters values, and, further, by analyzing the effects of welding on the geometry and on the appearance of the weld bead. Finally, employing the optimum welding regime—14 cm/min welding speed, 125 A main current, 100 A pulse current, 2.84 Hz oscillation frequency, and 5 Hz pulse frequency—appropriate dissimilar joints, without imperfections, were achieved.

24 March 2022 in Metals
Verified
Journal Article
Open access
PDF file
Ionelia VoiculescuIonelia Voiculescu
Ionelia Voiculescu
VGVictor Geantă
Victor Geantă
ESElena Violeta Stefanescu
Elena Violeta Stefanescu
GSGeorge Simion
George Simion
Elena SCUTELNICUElena SCUTELNICU
Elena SCUTELNICU
This research focused on the investigation of the metallurgical behavior of the Al0.8CoCrFeNi high-entropy alloy and S235JR structural steel, welded with (Ni, Fe)-rich filler metal, by the Gas Tungsten Arc Welding (GTAW) method. The electric arc and the welding pool were protected against the contamination with gases from the environment, by employing high-purity Ar 4.8 inert gas that plays an important role in reducing the oxidation effects and the development of cracks in the weld and the adjacent areas. The microstructure and microhardness analysis did not reveal the existence of fragile phases, cracks, inadequate penetration, or other imperfections, showing an appropriate adhesion between the deposited metal and the substrates. At the interface between the Ni-rich weld metal and the high-entropy alloy, a higher hardness (448 HV0.2) than in the base material (358 HV0.2) was measured. Energy-dispersive X-ray analysis (EDS), performed at the interface between the weld metal and the base materials, did not show significant modifications of Co, Fe, and Cr percentages. However, during the investigation, significant variations in Al and Ni concentrations were observed, caused by the fast diffusion of chemical elements, and the development of hard (Ni, Al)-rich compounds. In some areas of the deposited metal, located at a distance of about 10 µm from the interface, the percentages of Ni and Al were higher than in the high-entropy alloy base material, being around 41% by weight Ni and over 13% by weight Al, while the concentrations of the Co, Cr, and Fe elements proportionally decreased (i.e., approximately 14% by weight Co, 12% by weight Cr, and 17% by weight Fe). The development of Ni3Al and NiAl compounds was also noticed, whose formation was determined by the local chemical concentration and the temperature reached in the vicinity of the diffusion zone. The XRD analysis showed a group of X-ray peaks in the Al0.8CrFeCoNi alloy that corresponded to both α-type—BCC and FCC phases. The crystallite size of the high-entropy alloy investigated was found to be 22.05 nm. Despite the diffusion phenomenon, if filler materials and process parameters are appropriately selected, quality joints of high-entropy alloys and structural steels can be carried out under good welding conditions.