Titanium and its alloys have excellent corrosion resistance, heat, and fatigue tolerance, and their strength-to-weight ratio is one of the highest among metals. This combination of properties makes them ideal for aerospace applications; however, high manufacturing costs hinder their widespread use compared to other metals such as aluminum alloys and steels. Powder metallurgy (PM) is a greener and more cost and energy-efficient method for the production of near-net-shape parts compared to traditional ingot metallurgy, especially for titanium parts. In addition, it allows us to synthesize special microstructures, which result in outstanding mechanical properties without the need for alloying elements. The most commonly used Ti alloy is the Ti6Al4V grade 5. This workhorse alloy ensures outstanding mechanical properties, demonstrating a strength which is at least twice that of commercially pure titanium (CP-Ti) grade 2 and comparable to the strength of hardened stainless steels. In the present research, different mixtures of both milled and unmilled Cp-Ti grade 2 powder were utilized using the PM method, aiming to synthesize samples with high mechanical properties comparable to those of high-strength alloys such as Ti6Al4V. The results showed that the fine nanoparticles significantly enhanced the strength of the material, while in several cases the material exceeded the values of the Ti6Al4V alloy. The produced sample exhibited a maximum compressive yield strength (1492 MPa), contained 10 wt.% of fine (milled) particles (average particle size: 3 μm) and was sintered at 900 °C for one hour.
Nanocrystalline/amorphous powder was produced by ball milling of Ti50Cu25Ni20Sn5 (at.%) master alloy. Both laser diffraction particle size analyzer and scanning electron microscope (SEM) were used to monitor the changes in the particle size as well as in the shape of particles as a function of milling time. During ball milling, the average particle size decreased with milling time from >320 µm to ~38 µm after 180 min of milling. The deformation-induced hardening and phase transformation caused the hardness value to increase from 506 to 779 HV. X-ray diffraction (XRD) analysis was used to observe the changes in the phases/amorphous content as a function of milling time. The amount of amorphous fraction increased continuously until 120 min milling (36 wt % amorphous content). The interval of crystallite size was between 1 and 10 nm after 180 min of milling with 25 wt % amorphous fractions. Cubic Cu(Ni,Cu)Ti2 structure was transformed into the orthorhombic structure owing to the shear/stress, dislocations, and Cu substitution during the milling process.
Novel amorphous/crystalline composites were developed combining the ductile copper matrix with hard CuZr-based amorphous powder. The amorphous powders of two compositions, Cu39.2Zr36All4.8Ni10Ti10 and Cu39.2Zr35.2Al5.6Ni10Ti10, produced by ball milling were used for reinforcement of the composites. Different mixing techniques, magnetic mixing, ultrasonic mixing and high-energy ball milling, were applied in order to create a homogenous mixture of the powders. The composites were produced by hot pressing under a purified argon atmosphere. Their microstructure, homogeneity and mechanical properties were investigated. It was observed that before hot pressing, minimal porosity had been obtained for the composite blended for 15 min by the ball-mill with a ball-to-powder ratio of 80:1. Its copper content was 50 wt %, which is the minimum to produce a compact composite. Reinforcing the copper by amorphous powders, the maximal compressive strength was enhanced to 490 MPa and 470 MPa, respectively, for the abovementioned composites. The yield strength of the copper due to reinforcement increased drastically from 150 MPa to 400 MPa and 420 MPa.
18 October 2018 in IOP Conference Series: Materials Science and Engineering
Properties of powders made from Ti50Cu27,5Ni10Zr10Co2,5 alloy, milled under different conditions for only 3600 s in total were investigated. For this purpose two different milling atmospheres and two different Process Control Agents (PCA) were tested: argon without PCA, air without PCA, argon combined with stearic acid, argon combined with petroleum spirit. Results showed that the size and shape of particles, and the microstrucutre and hardness of partcicles were highly depended on the milling conditions. According to XRD analysis, the maximal amorphous fraction has been achieved in the air atmosphere withouth PCA milled sample (57 wt. %) powder. However the extent of Fe contamination and weight loss during milling powder resulted bigger values. As a result, the optimal combination of morphology, contamination amount and weight lost level has been observed in the case of powder milled in argon atmosphere using stearic acid.
The mechanical behavior, microstructures, as well as the crystallographic textures of the Ti57-Nb43 alloy were investigated on cylindrical specimens compressed at high temperatures, in the range of 700–1000 °C, and strain rates between 0.001 and 1.0 s−1. Hardening, followed by softening behaviors, were observed as a function of strain due to the occurrence of dynamic recrystallization/recovery in hot deformation. The modified five-parameter Voce-type equation described well the stress–strain curves, but, for the present alloy, it was also possible with only four parameters. A new two-variables polynomial function was employed on the four parameters that described well the flow curves as a direct function of temperature and strain rate. It permitted the reduction in the number of parameters and had the predictive capacity for the flow stress at any temperature, strain, and strain rate in the investigated range. The crystallographic textures were similar at all temperatures, with an increase in intensity from 900 °C. The textures could be characterized by a double and fiber and a unique component of (001) , the latter inherited from the initial hot-rolling texture. Viscoplastic polycrystal self-consistent deformation modeling reproduced the measured textures showing that dynamic recrystallization did not alter the development of the deformation texture, only increased its intensity.
The mechanical behavior, microstructures as well as the crystallographic textures of the Ti57-Nb43 alloy were investigated on cylindrical specimens compressed at high temperatures, in the range of 700-1000 °C, and strain rates between 0.001 and 1.0 s-1. Hardening, followed by softening behaviours were observed as a function of strain, due to the occurrence of dynamic recrystallization/recovery in hot deformation. The modified five-parameter Voce type equation described well the stress-strain curves, but for the present alloy, it was also possible with only four parameters. A new two-variables polynomial function was employed on the four parameters that described well the flow curves as a direct function of temperature and strain rate. It permitted to reduce the number of parameters and had the predictive capacity for the flow stress at any temperature, strain, and strain rate in the investigated range. The crystallographic textures were similar at all temperatures with an increase of intensity from 900 °C. The textures could be characterized by a double and fiber and a unique component of (001), the latter inherited from the initial hot rolling texture. Viscoplastic polycrystal self-consistent deformation modeling reproduced the measured textures showing that dynamic recrystallization did not alter the development of the deformation texture, only increased it intensity.