Buildings utilize both inorganic and organic insulation materials to conserve energy and prevent heat loss. However, while exhibiting excellent thermal insulation performance, organic insulation materials increase the risk of fire due to the emission of intense heat and toxic smoke in the event of a fire. Conversely, inorganic insulation materials are characterized by a lower thermal insulation performance, leading to an increase in the weight of the building with extensive use. Therefore, the necessity for research into new insulation materials that address the drawbacks of existing ones, including reducing weight, enhancing fire resistance, and improving thermal insulation performance, has been recognized. This study focuses on evaluating the enhancement of the thermal insulation performance using novel building materials compared to conventional ones. The research methodology involved the incorporation of porous aerogel powders into paper-based cellulose insulation to improve its insulating properties. Samples were prepared in standard 100 × 100 mm2 panel forms. Two control groups were utilized: a pure control group, where specimens were fabricated using 100% recycled cardboard for packaging, and a mixed control group, where specimens were produced using a mixture ratio of 30 wt% ceramic binder and 40 wt% expandable graphite. Experimental group specimens were prepared by increasing the aerogel content from 200 to 1000 mL under each condition of the control groups (pure and mixed) after mixing. The thermal insulation performance of the specimens was evaluated in terms of thermal conductivity and thermal diffusivity according to ISO 22007-2 (for solids, paste, and powders). Through this study, it was found that the thermal insulation performances of the pure control and experimental groups improved by 16.66%, while the mixed control and experimental groups demonstrated a 17.06% enhancement in thermal insulation performance with the addition of aerogel.
The increase in non-face-to-face lifestyles due to COVID-19 worldwide have shown an increase in delivery services. The number of parcels in 2020 was 3.373 billion, an increase of 20.9% from 2.788 billion in 2019. This phenomenon increased delivery box waste. Against this background, this study attempted to develop building materials from the recycling of delivery boxes. In this study, the self-developed WC (wet cellulose) 3D printer confirmed the standardization and uniform performance of the sample by filling the material supply cylinder with cellulose filaments and spraying the composite material through a 10 mm nozzle. The cellulose filament for a WC 3D printer is based on cellulose extracted from wastepaper, and a cellulose filament composite material is used by mixing additives. After manufacturing a specimen using the WC 3D printer, a reliability test for the flame-retardant performance of the material was conducted according to the ISO 11925-2 test method. As a result of the experiment, flame-retardant performance was confirmed at a 40 wt% or greater ceramic binder content. In addition, the WC 3D printer achieved accurate test results by producing specimens with uniform physical properties. In addition, we confirmed that 3D-printed WC can be used to develop customized building materials that can prevent fire spread.
The impact of non-face-to-face contact following the COVID-19 pandemic has emerged as a social problem and has increased the amount of wastepaper, mainly in home delivery boxes. The appropriate recycling of paper waste is an area where sustainable growth is required in terms of the net environment system and carbon neutrality practice. Therefore, in this study, a specimen of building finishing material using wastepaper was produced using a custom-made large wet cellulose (LWC) 3D printer, and the site applicability of the fire performance was evaluated. The specimen of the building finish material was a mixture of wastepaper and ceramic binder, and the molding of the specimen was uniformly produced by a cylinder injection-type LWC 3D printer. The production reliability of the 3D printer was analyzed by measuring the mass and density of the specimen. The uniformity of the mass and density of the manufactured building finishes were confirmed to have standard deviations of ±0.05 g and ±0.01 g/cm3, respectively. The uniformity of the fire performance of specimens was confirmed by checking the relative standard deviation (RSD) value of ±3% under the same ceramic addition conditions from ISO 5660-1. Through the mass and density analysis and fire performance analysis of the building finishing materials, it was confirmed that the same mass, density, and fire performance can be produced simultaneously, and manufacturing using LWC 3D printers has been confirmed to be effective in developing uniform semi-non-combustible and retardant building materials.
This study focuses on the increased risk of high heat release and asphyxiation (toxic gas poisoning) in the event of a fire involving polyurethane (PU)- and MDF-based building materials, which are commonly used in buildings. Among them, polyurethane (PU) building materials are very commonly used in buildings, except in Europe and some other countries, due to their excellent thermal insulation performance. Still, problems of short-term heat release and the spread of toxic gases in the event of a fire continue to occur. To overcome these problems, researchers are actively working on introducing various flame retardants into building materials. Therefore, in this study, we produced a laboratory-sized (500 mm × 500 mm) plate-like flame-retardant board that can be utilized as a building material with a lower heat release rate and a lower toxicity index. The material was made by mixing expanded graphite and ceramic binder as flame retardants in a material that is formulated based on the cellulose of waste paper, replacing the existing building materials with a hot-press method. According to the ISO-5660-1 test on the heat release rate of the plate-like flame-retardant board, the Total Heat Release (THR) value was 2.9 (MJ/m2) for 10 min, showing an effect of reducing the THR value by 36.3 (MJ/m2) compared to the THR value of 39.2 (MJ/m2) of the specimen made using only paper. In addition, the toxicity index of the flame-retardant board was checked through the NES (Naval Engineering Standards)-713 test. As a result, the test specimen showed a toxicity index of 0.7, which is 2.4 lower than the toxicity index of 3.1 of MDF, which is utilized as a conventional building material. Based on the results of this study, the cellulose fire-retardant board showed the effect of reducing the heat release rate and toxicity index of building materials in a building fire, which reduces the risk of rapid heat spread and smoke toxicity. This has the potential to improve the evacuation time (A-SET) of evacuees in fires. It is also important to show that recycling waste paper and utilizing it as the main material for building materials can be an alternative in terms of sustainable development.
This study focuses on the increased risk of high heat release and asphyxiation (toxic gas poisoning) in the event of a fire of polyurethane (PU) and MDF-based building materials, which are commonly used in building fires. Among them, polyurethane (PU) building materials are essential for buildings except in Europe and some other countries due to their excellent thermal insulation performance, but problems of short-term heat release and spread of toxic gases in the event of a fire continue to occur. To overcome these problems, researchers are actively working on introducing various flame retardants into building materials. Therefore, in this study, we produced a laboratory-sized (500mm*500mm) plate flame retardant board that can be utilized as a building material with a lower heat release rate and a lower toxicity index by mixing expanded graphite and ceramic binder as flame retardants in a main material based on the cellulose of waste paper by replacing the existing building materials with a hot-press method. According to the ISO-5660-1 test on the heat release rate of the plate flame retardant board, the THR value was 2.9 (MJ/m2) for 10 minutes, showing an effect of reducing the THR value by 36.3 (MJ/m2) compared to the THR value of 39.2 (MJ/m2) of the specimen made using only paper. In addition, the toxicity index of the flame retardant board was checked through the NES 713 test. As a result, the test specimen showed a toxicity index of 0.7, which is 2.4 lower than the toxicity index of 3.1 of MDF, which is utilized as a conventional building material. Based on the results of this study, the cellulose fire retardant board showed the effect of reducing the heat release rate and toxicity index of building materials in a building fire, which reduces the risk of rapid heat spread and smoke toxicity. This has the potential to improve the evacuation time (A-SET) of evacuees in fires. It is also important to show that recycling waste paper and utilizing it as the main material for building materials can be an alternative in terms of sustainable development.