The aim of this study was to investigate the pozzolanic effect (PE) and filler effect (FE) of rice husk ash (RHA) on the mechanical properties and microstructure of brick aggregate concrete (BAC). For this, concrete cylinders (100 mm × 200 mm) were prepared with 0-25% RHA with water-to-binder ratios of 0.50 at a constant mix-ratio of 1:1.5:3 and cured in water. Test results revealed that the mean particle size of RHA decreases with increasing grinding time. The compressive strength ( f c ' ) of BAC due to filler effect are 58.56-94.62% less compared to the pozzolanic effect of RHA for the 10%-25% replacement of cement. Meanwhile, the 15% RHA showed the maximum f c ' of BAC due to pozzolanic effect of RHA. The tensile strength ( f s p ) and flexural strength ( f r ) of BAC due to pozzolanic effect are 60%-150% and 25%-150% higher than that of filler effect of RHA for the 10%-25% replacement of cement respectively. The modulus of elasticity ( E c ) and Poisson's ratio ( ν ) of BAC due to pozzolanic effect are 2%-29% and 27%-43% greater than that of filler effect of RHA for the 10%-25% replacement of cement respectively. BAC with 10-20% RHA shows a dense and homogeneous microstructure. Therefore, inclusion of RHA as a partial replacement of cement possesses a significant pozzolanic effect than the filler effect on the mechanical properties and microstructure of BAC.
1 June 2018 in Journal of Materials in Civil Engineering
The objective of this research was to determine the mechanical properties, including among others compressive strength , tensile strength , flexural strength , modulus of elasticity , and Poisson’s ratio of a brick aggregate concrete (BAC) containing rice husk ash (RHA) as a partial replacement of cement. Concrete cylinders with 100-mm diameter and 200-mm height were cast using 0–25% RHA as a partial replacement of cement with water-to-binder ratios of 0.45, 0.50, and 0.55, with a mix ratio of 1:1.5:3, and cured in water at room temperature. The experimental results indicated that and increased gradually with the increasing RHA up to 15%. However, the maximum values of these were observed with 10% RHA. By contrast, of BAC containing up to 25% RHA was found lower than that of control concrete. and of BAC with RHA were higher than those of control concrete. It was observed that mechanical properties of BAC were influenced significantly due to the inclusion of 15% RHA as a partial replacement of cement with a water-to-binder ratio of 0.50.
In response to environmental concerns, researchers explore fly ash as a cement replacement material, and crushed bricks as a cost-effective and load-reducing aggregate, particularly where stone chips are scarce. Therefore, this study investigates the mechanical properties and microstructure of brick aggregate concrete (BAC) with raw fly ash (FA) as a partial replacement of cement. The research involved casting raw FA based BAC (FBAC) cylinders (100 mm diameter and 200 mm height) and prism (100 × 100 × 500 mm) with varying levels of FA (0–25%) using a constant mix proportion by volume of 1:1.5:3 (cement : fine aggregate : coarse aggregate) with a water to binder (w/b) ratio of 0.50 and three curing ages (7, 28, and 90 days). Tests for mechanical properties, including compressive strength, split tensile strength, flexural strength, modulus of elasticity, and Poisson's ratio were conducted to assess the behavior of FBAC, and microstructure were then investigated at 28 days. The results indicated that increasing the FA content up to 15% led to gradual improvement in compressive strength and tensile strength values. At 28 days, the highest values of compressive strength and split tensile strength were observed at 10% FA, with 7.9% and 14.2% increase, respectively, compared to the control concrete. However, the flexural strength of FBAC decreased gradually with cement replacement. On the other hand, modulus of elasticity and Poisson's ratio increased gradually up to 20% and 25% cement replacement, respectively. Up to 15% FA enhanced a more uniform and compact microstructure than that of control concrete. Several equations have been developed to express relationship between compressive strength and other mechanical properties of FBAC. Hence, up to 15% raw FA as a partial replacement of cement improved the mechanical properties and microstructure of BAC.
The uses of ceramic products are expanding day by day in different forms like tiles, sanitary fittings, wall linings, electrical insulations etc. Due to its brittle nature, huge number of ceramic materials turn into waste during processing, transporting and fixing. The direct dumping of these waste materials leads to environmental and dust pollution in addition to occupation of vast and useable land area. The aim of the study was to investigate the effect of ceramic waste powder (CWP) on the strength development of brick aggregate concrete (BAC). A total of 180 nos. Cylindrical specimens (100mm dia. × 200mm height) were cast for compressive and split tensile strength tests and 45 nos. Prism (100mm × 100mm × 500mm) for flexural strength test from concrete with mix ratio of 1:1:5:3 (by weight) using three different water-to-binder ratios (i.e., 0.40, 0.45 and 0.50 by weight). In concrete mix, cement was replaced by CWP at various replacement levels of 0, 5, 10, 15 and 20% and specimens were cured in plain water for 7, 14, 28 and 56 days. The specimens were tested for compressive, split tensile and flexural strengths at the end of different curing ages. The test results indicate that the strength of concrete decreases with the increase of CWP contents in the mix that ranges from 2 to 30%. However, the decrease in strength is observed to be lower up to 10% cement replacement levels that lies in the range of 11 to 13%. Hence CWP can be utilized as partial replacement of cement up to 10% without significantly affecting the strength performance of BAC.