Gasification technology enables the clean and efficient utilization of coal. However, the process generates a significant amount of solid waste—coal gasification slag. This paper focuses on the Jinhua furnace coal gasification slag (fine slag, FS; coarse slag, CS) as the research subject, analyzing its composition and structural characteristics, and discussing the thermochemical conversion performance of both under different atmospheres (N2 and air). The results show that the fixed carbon content in FS is as high as 35.82%, while it is only 1% in CS. FS has a large number of fluffy porous carbon on its surface, which wraps around or embeds into smooth and variously sized spherical inorganic components, with a specific surface area as high as 353 m2/g, and the pore structure is mainly mesoporous. Compared to the raw coal (TYC), the types of organic functional groups in FS and CS are significantly reduced, and the graphitization degree of the carbon elements in FS is higher. The ash in FS is mainly amorphous and glassy, while in CS, it mainly has crystalline structures. The weight loss rates of TYC and FS under an inert atmosphere are 27.49% and 10.38%, respectively; under an air atmosphere, the weight loss rates of TYC and FS are 81.69% and 44.40%, respectively. Based on the analysis of the thermal stability of FS and its high specific surface area, this paper suggests that FS can be used to prepare high-value-added products such as porous carbon or high-temperature-resistant carbon materials through the method of carbon–ash separation.
Transition metal oxides show high activity while still facing the challenges of low mineralization and poor durability in the ozone catalytic oxidation (OCO) of volatile organic compounds (VOCs). Improving the oxygen mobility and low-temperature reducibility of transition metal oxides was found to be an effective way to address the above challenges. Here, highly dispersed Ag was added to Mn3O4 via the co-precipitation oxalate route, and the obtained Ag/Mn3O4 exhibited higher mineralization and stability in benzene catalytic ozonation at room temperature. Compared to Mn3O4, the concentration of CO2 formed from benzene oxidation over Ag/Mn3O4 was significantly increased, from 585.4 ppm to 810.9 ppm, while CO generation was greatly suppressed to only one tenth of its original value (194 ppm vs. 19 ppm). In addition, Ag/Mn3O4 exhibited higher catalytic stability than Mn3O4. The introduction of Ag obviously improved the oxygen mobility and low-temperature reducibility of Mn3O4. Moreover, the highly dispersed Ag also promoted the activity of surface oxygen species and the chemisorption of benzene on Mn3O4. The above physicochemical properties contributed to the excellent catalytic performance and durability of Ag/Mn3O4. This research could shed light on the improvement in VOC mineralization via ozone catalytic oxidation.
Coal-fired power plants produce large amounts of fly ash that occupy large land areas when stored and pose potential environmental risks. Hence, considerable attention has been drawn to the valorisation of this bulk solid waste, e.g., through CO2 mineralisation. High-alkali Xinjiang Zhundong coal fly ash has a high-silica, low-calcium composition and exhibits a low direct CO2 mineralisation efficiency due to the extensive polymerisation of silicon and aluminium components into an inert glass phase and the very low contents of active calcium and magnesium. In this study, this fly ash was thermochemically modified with a CaSO4 composite flux and used as a CO2 capture agent. The modification and mineralisation conditions were systematically varied to optimise the corresponding parameters (calcination temperature, calcination time, flux loading and flux ratio for modification; solid–liquid ratio, initial CO2 partial pressure and reaction temperature for mineralisation). Thermochemical modification promoted the transformation of inert fly ash components into active calcium silicate phases, with stable CaCO3 generated after mineralisation. Control experiments confirmed that the enhanced CO2 uptake primarily arises from the thermochemical reconstruction of fly ash silicates via calcium incorporation, rather than simple physical mixing with CaSO4. Under optimal mineralisation conditions (60 °C, 2 MPa and a solid–liquid ratio of 200 g/L), the modified fly ash achieved an apparent CO2 conversion rate of 95.82% and an apparent carbon sequestration capacity of 214.6 g CO2 kg−1 modified sample (429.2 g CO2 kg−1 original fly ash). The developed process overcomes the bottleneck of the insufficient carbon sequestration activity of high-silica, low-calcium fly ash, reduces the use of chemical reagents and provides a potential pathway for the valorisation of Xinjiang Zhundong coal fly ash and stable CO2 sequestration.