The effects of the combined addition of B and Ti, as well as the influence of different strain rates on the hot ductility behavior of low carbon, continuously cast, microalloyed steels were investigated in this work. Tensile tests, microstructure analyses, and thermokinetic simulations were performed with in situ melted samples. Furthermore, prior austenite grain evaluations were carried out for the two different microalloyed steels. Increasing the strain rate brought improvements to the ductility, which was more significant in the steel with the leanest composition. The steel containing more B and Ti presented a better hot ductility behavior under all conditions tested. The main causes for the improvements rely on the precipitation behavior and the austenite–ferrite phase transformation. The preferential formation of TiN instead of fine BN and AlN was seen to be beneficial to the ductility, as well as the absence of MnS. Grain boundary segregation of free B that did not form BN retarded the ferrite formation, avoiding the brittleness brought by the thin ferrite films at the austenite grain boundaries. Furthermore, it was revealed that for the steels in question, the prior austenite grains have less influence on the hot ductility behavior than the precipitates and ferrite formation.
20 February 2025 in High Temperature Corrosion of Materials
Nowadays the production of steel from scrap in electric arc furnaces is the most common bridging technology to reduce CO2 emissions. Depending on scrap quality, a non-negligible content of tramp elements such as Cu, Sn, or Ni is introduced into the steel. As their affinity to oxygen is lower than that of iron, they typically enrich at the steel/scale interface area and along grain boundaries during oxidation, which may result in quality problems. Oxidation processes are unavoidable in solid steel processing, and therefore, a deeper understanding of the occurring phenomena, such as intergranular oxidation and liquid metal infiltration of grain boundaries, is essential to continuously improve the product quality. In this study, oxidation experiments for slab reheating were performed by simultaneous thermal analysis under near-process conditions. For a clear statement on the role of tramp elements during oxidation, steel grades with and without tramp elements were investigated. The addition of the expected future contents of Cu and Sn does not affect external oxidation, but at the interface the presence of Cu and Sn leads to the formation of liquid Cu phases and infiltration of grain boundaries. The additional presence of Ni counteracts this formation, but due to its huge impact on iron activity it favors the formation of a rough steel/scale interface. In contrast with Ni, Cu and Sn hardly have any influence on iron activity. Numerical calculations based on a diffusion model and results of the well-known thermochemical software FactSage confirm these effects.
Since steel cleanness comes to the fore of steel producers worldwide, it is necessary to understand the formation mechanism and modification of non-metallic inclusions (NMIs) in more detail. One central point is the identification of the source of especially interfering NMIs to prevent their evolution in the future. The present study applies two approaches to determine the source of NMIs in Ti-stabilized ultra-low carbon (ULC) steels—the active and the passive tracing. Both approaches are applied to an industrial experiment. The active tracing technique is focused on investigating the clogging layer formation in submerged entry nozzles and, hence, the origin of alumina particles. This method adds rare earth elements (REEs) directly to the melt to mark pre-existing deoxidation products at a certain point of the steelmaking process. The main concern of the passive method, the so-called REE fingerprint, is the determination of the source of mesoscopic NMIs. For the REE fingerprint, the pre-existing concentration of REEs in different potential sources and the investigated NMIs are measured by using an inductively coupled plasma mass spectrometer (ICP-MS). The resulting patterns are compared after normalizing the contents to chondrites, and the NMIs’ origins are identified. Concerning the EDS analysis and the resulting patterns from the REE fingerprint, the mold slag and, respectively, the casting powder were the sources of the investigated NMIs.
Cracking during the continuous casting process is undesirable and continuous work is being carried out to find further improvements and understand the mechanisms that lead to failure. Investigations on the hot ductility behavior of a continuously cast low alloyed steel using different holding times before straining were done in the present work. Samples were heated to melting temperature in a vacuum atmosphere and then cooled to one of the three test temperatures chosen: 750, 850, and 900 °C. When the desired temperature was reached, the sample was isothermally held for either 10, 90, 300, or 3600 s before the tensile test started, with a strain rate of 10−3 s−1. The reduction of area was measured, SEM images of the fractured surfaces were taken plus LOM images for the analysis of the microstructure. The results show that there was no significant change in the ductility at any of the temperatures until 300 s, with a change in behavior at 3600 s. This was further confirmed with the images and precipitation kinetics simulations. The results are described and compared.
The continuous casting of Al-killed Ti-stabilized interstitial free steels is often affected by clogging. By today, the mechanism behind this phenomenon is not entirely clarified. The active tracing method, which involves the direct addition of rare-earth elements (REEs), enables tracking of nonmetallic inclusions (NMIs) over process time. Due to the high oxygen affinity of these elements, preexisting NMIs are partially reduced and marked by this tracer. Using scanning electron microscopy with energy-dispersive spectroscopy, it is possible to differentiate such labeled NMIs from particles formed at later stages in the process by the absence of these tracing elements. Active tracing is used in industrial and laboratory settings to trace preexisting alumina NMIs with La or Ce. In the investigation, it is revealed that the number of small NMIs increases after the addition of REEs, and subsequently, the size increases again after FeTi is alloyed. In both settings, traced and untraced Al–Ti oxides are found. The separation tendency of traced NMIs is studied over time by analyzing the composition of the slags. Furthermore, the impact of deoxidation products on the formation of the clogging layer within the submerged entry nozzle is investigated, indicating that these NMIs contribute to its formation.