Far-ultraviolet-C (far-UVC) light-emitting diodes (LEDs) with an emission wavelength of 234 nm with different polarization-doped AlGaN hole injection layers (HILs) are compared regarding their emission power, voltage, and leakage current. The influence of the thickness of the polarization-doped layer (PDL), an additional Mg doping of the PDL, as well as a combination of a PDL with a conventionally Mg-doped AlGaN HIL will be discussed. The different PDL thicknesses show nearly no influence on the emission power or voltage. However, the leakage current of the LEDs below the turn-on voltage decreases with an increasing thickness of the PDL. In contrast, an additional Mg doping of the PDL ([Mg] ∼ 1.5 × 1019 cm−3) results in a fivefold decrease in the emission power at an unchanged voltage and leakage current. Finally, a combination of a PDL and a conventionally Mg-doped AlGaN layer ([Mg] ∼ 1.5 × 1019 cm−3) as a HIL shows also a similar emission power and voltage compared to the single PDL, but the leakage current increases. Based on these optimizations, 234 nm LEDs were realized with a maximum external quantum efficiency of 1% at 20 mA, an emission power of 4.7 mW, and a voltage of 9.0 V at 100 mA. This shows that the polarization doping concept is well suited to realize far-UVC LEDs with improved performance compared to LEDs with a conventionally Mg-doped p-side.
AlGaN-based far-UVC light emitting diodes (LEDs) with an emission wavelength of 233 nm were fabricated in the form of micro-LED arrays with emitter diameters ranging from 1.5 to 50 μm. The mesa was plasma etched with a sidewall angle of 45°–50°, and insulator layers made of SiNx or SiO2 were deposited. While the external quantum efficiency (EQE) of the LEDs with SiNx showed only a small dependency on the micro-LED diameter, the LEDs using SiO2 showed an increase in the peak EQE by a factor of four as compared to large area devices. This enhancement is attributed to a strong increase in the light extraction efficiency due to total internal reflection and re-direction at the inclined mesa, allowing TM-polarized light emitted in the plane of the quantum well to be extracted through the sapphire backside of the chips.
High temperature annealed AlN/sapphire templates exhibit a reduced in-plane lattice constant compared to conventional non-annealed AlN/sapphire grown by metalorganic vapor phase epitaxy (MOVPE). This leads to additional lattice mismatch between the template and the AlGaN-based ultraviolet-C light emitting diode (UVC LED) heterostructure grown on these templates. This mismatch introduces additional compressive strain in AlGaN quantum wells resulting in enhanced transverse electric polarization of the quantum well emission at wavelengths below 235 nm compared to layer structures deposited on conventional MOVPE-grown AlN templates, which exhibit mainly transverse magnetic polarized emission. In addition, high temperature annealed AlN/sapphire templates also feature reduced defect densities leading to reduced non-radiative recombination. Based on these two factors, i.e., better outcoupling efficiency of the transverse electric polarized light and an enhanced internal quantum efficiency, the performance characteristic of far-UVC LEDs emitting at 231 nm was further improved with a cw optical output power of 3.5 mW at 150 mA.
The effects of composition and p-doping profile of the AlGaN:Mg electron blocking layer (EBL) in 310 nm ultraviolet B (UV-B) light emitting diodes (LEDs) have been investigated. The carrier injection and internal quantum efficiency of the LEDs were simulated and compared to electroluminescence measurements. The light output power depends strongly on the temporal biscyclopentadienylmagnesium (Cp Mg) carrier gas flow profile during growth as well as on the aluminum profile of the AlGaN:Mg EBL. The highest emission power has been found for an EBL with the highest Cp Mg carrier gas flow and a gradually decreasing aluminum content in direction to the p-side of the LED. This effect is attributed to an improved carrier injection and confinement that prevents electron leakage into the p-doped region of the LED with a simultaneously enhanced carrier injection into the active region.
The performance of vertical-cavity surface-emitting lasers (VCSELs) is strongly dependent on the spectral detuning between the gain peak and the resonance wavelength. Here, we use angle-resolved photoluminescence spectroscopy to investigate the emission properties of AlGaN-based VCSELs emitting in the ultraviolet-B spectral range with different detuning between the photoluminescence peak of the quantum-wells and the resonance wavelength. Accurate setting of the cavity length, and thereby the resonance wavelength, is accomplished by using doping-selective electrochemical etching of AlGaN sacrificial layers for substrate removal combined with deposition of dielectric spacer layers. By matching the resonance wavelength to the quantum-wells photoluminescence peak, a threshold power density of 0.4 MW/cm2 was achieved, and this was possible only for smooth etched surfaces with a root mean square roughness below 2 nm. These results demonstrate the importance of accurate cavity length control and surface smoothness to achieve low-threshold AlGaN-based ultraviolet VCSELs.