Integrating class-C and class-F fly ash (FA) as supplementary cementitious materials (SCMs) in concrete offers a promising pathway for sustainable construction practices. This study explores the pivotal role of FA in reducing carbon dioxide (CO2) emissions and improving concrete’s durability and mechanical properties through a comprehensive life cycle analysis (LCA). By blending FA with cement, significant reductions in CO2 emissions are achieved, alongside enhancements in the workability, compressive strength, and permeability resistance of the concrete matrix. This research elucidates the pozzolanic reaction between FA and calcium hydroxide (CH) during cement hydration, highlighting its contribution to concrete strength and durability. Through a range of comprehensive analysis techniques, including mechanical testing and environmental impact assessment, this study demonstrates the substantial benefits of prioritizing the utilization of class-C and class-F FA in sustainable construction. The findings underscore the industry’s commitment to environmentally conscious practices, promoting structural integrity and reducing ecological impacts. Overall, this research emphasizes class-C and class-F FA as critical components in achieving sustainable construction goals and advancing towards a more environmentally responsible built environment.
31 August 2024 in Construction and Building Materials
This study compares the workability, mechanical, and thermal characteristics of structural self-compacting lightweight concrete (SCLWC) formulations using pumice aggregate (PA), expanded perlite aggregate (EPA), fly ash (FA), and silica fume (SF). FA and SF were used as partial substitutes for cement at a 10% ratio in various mixes, impacting different aspects: According to the obtained results, FA enhanced the workability but SF reduced it, while SF improved the compressive and splitting tensile strengths more than FA. EPA, used as a fine aggregate alongside PA, decreased the workability, compressive strength, and splitting tensile strength compared to the control mix (K0). The thermal properties were altered by FA and SF similarly, while EPA notably reduced the thermal conductivity coefficients. The thermal conductivity coefficients (TCCs) of the K0–K4 SCLWC mixtures ranged from 0.275 to 0.364 W/mK. K0 had a TCC of 0.364 W/mK. With 10% FA, K1 achieved 0.305 W/mK; K2 with 10% SF reached 0.325 W/mK. K3 and K4, using EPA instead of PA, showed significantly lower TCC values: 0.275 W/mK and 0.289 W/mK, respectively. FA and SF improved the thermal conductivity compared to K0, while EPA further reduced the TCC values in K3 and K4 compared to K1 and K2. The compressive strength (CS) values of the K0–K4 SCLWC mixtures at 7 and 28 days reveal notable trends. Using 10% FA in K1 decreased the CS at both 7 days (12.16 MPa) and 28 days (22.36 MPa), attributed to FA’s gradual pozzolanic activity. Conversely, K2 with SF showed increased CS at 7 days (17.88 MPa) and 28 days (29.89 MPa) due to SF’s rapid pozzolanic activity. Incorporating EPA into K3 and K4 reduced the CS values compared to PA, indicating EPA’s lower strength contribution due to its porous structure.
17 February 2024 in Construction and Building Materials