In this study, novel Fe2O3/TiO2 photocatalytic composites were synthesised by combining traditional oxidation roasting with the sol-gel method, using low-cost metallurgical waste (iron scales) as the raw material. The characterisation results revealed that the oxidised iron scales could be transformed into high-purity and porous Fe2O3 particles through oxidation roasting, thereby providing additional sites for the adsorption process and thus serving as an effective carrier for TiO2-based photocatalytic materials. During the sol-gel process, TiO2 was loaded onto the synthesised Fe2O3 particles, generating core-shell heterostructure Fe2O3/TiO2 photocatalytic composites. Under visible light irradiation for 90 min, the Fe2O3/TiO2 photocatalytic composites achieved a remarkable methylene blue removal rate (97.71%). This reaction process followed the quasi-first-order kinetic model with a rate constant of 0.038 min−1. The results have demonstrated that this combination of various components in the Fe2O3/TiO2 photocatalytic composites improved the adsorption, light utilisation, and charge separation effect of the photocatalysts. Moreover, the material exhibited favourable stability and recyclability, making it a decent candidate for the treatment of wastewater from the biochemical industry. Therefore, this study provides a new strategy for improving the photocatalytic activity of TiO2 and expanding the high value-added utilisation of iron scales.
In the fabrication of soft magnetic composites, the lattice mismatch between the inorganic insulation layer and the iron matrix often leads to the formation of cracks during the molding process, which significantly impairs the operational performance of the materials. Consequently, it is imperative to develop novel strategies for inorganic insulation coatings that offer high electrical resistivity and thermal stability and are less susceptible to cracking during formation. This paper presents a new structure for soft magnetic composites that incorporates FePO4 as an intermediate transition layer between the iron-based soft magnetic particles and the inorganic ceramic insulation layer. This configuration is designed to provide insulation coatings with superior voltage and thermal resistance, as well as high electrical resistivity. The research details the processes forming the FePO4 intermediate transition layer and the SiO2 insulation layer on the iron powder surface, along with their interaction mechanisms. An analysis comparing the scenarios with and without the FePO4 intermediate transition layer shows its beneficial impact on the magnetic properties and mechanical strength of the soft magnetic composites. Further investigations reveal that at a phosphoric acid concentration of 1 wt.%, the FePO4 layer significantly enhances the interface compatibility between the Fe powder matrix and the SiO2 insulation layer. Under these conditions, the Fe@ FePO4/SiO2 soft magnetic composites demonstrate outstanding overall performance: the saturation magnetization stands at 215.60 emu/g, effective permeability at 83.2, resistivity at 57.42 Ω·m, power loss at 375.0 kW/m3 under 30 mT/100 kHz, and radial compressive strength at 15.95 Kgf. These findings offer novel insights and practical approaches for advancing inorganic insulation coating strategies and provide vital scientific support for further enhancing the magnetic and mechanical properties of soft magnetic composites.
Iron-based soft magnetic composites (SMCs) are the key components of high-frequency electromagnetic systems. Selecting a suitable insulating oxide layer and ensuring the integrity and homogeneity of the heterogeneous core–shell structure of SMCs are essential for optimizing their magnetic properties. In this study, four types of SMCs—Fe-Si-Cr/ZrO2, Fe-Si-Cr/TiO2, Fe-Si-Cr/MgO, and Fe-Si-Cr/CaO—were prepared via ball milling, followed by hot-press sintering. The differences between the microscopic morphologies and magnetic fproperties of the Fe-Si-Cr/AOx SMCs prepared using four different metal oxides were investigated. ZrO2, TiO2, MgO, and CaO were successfully coated on the surface of the Fe-Si-Cr alloy powders through ball milling, forming a heterogeneous Fe-Si-Cr/AOx core–shell structure with the Fe-Si-Cr alloy powder as the core and the metal oxide as the shell. ZrO2 is relatively hard and less prone to breakage and refinement during ball milling, resulting in a lower degree of agglomeration on the surface of the composites and prevention of peeling and collapse during hot-press sintering. When ZrO2 was used as the insulation layer, the magnetic dilution effect was minimized, resulting in the highest resistivity (4.2 mΩ·cm), lowest total loss (580.8 kW/m3 for P10mt/100kHz), and lowest eddy current loss (470.0 kW/m3 for Pec 10mt/100kHz), while the permeability stabilized earlier at lower frequencies.
Soft magnetic composites (SMCs) are composed of alloy materials with the core and insulating layers as the shell. These composites exhibit high saturation magnetic sensitivity and low hysteresis loss, making them a promising material for various applications. The investigation of double layers is considered valuable as it can effectively address the issues of low resistivity and high dynamic loss that arise from non-uniform insulating layers in SMCs. In this study, Fe-Si-Cr/SiO2 particles with a core–shell heterostructure were produced via chemical vapor deposition (CVD). The Fe-Si-Cr/SiO2 materials were coated with different weight percentages (1–6%) of sodium silicate (SS). Subsequently, Fe-Si-Cr-based SMCs were synthesized through high-pressure molding and heat treatment. The effect of the SS weight percentage on microscopic changes and magnetic characteristics was investigated. These findings indicated that a concentration of 4 wt% of SS was the most effective at enhancing magnetic characteristics. The resultant SMCs exhibited high resistivity (21.07 mΩ·cm), the lowest total loss (P10 mt/300 kHz of 44.23 W/kg), a relatively high saturation magnetization (181.8 emu/g), and permeability (35.9). Furthermore, it was observed that the permeability exhibited stabilization at lower frequencies. According to these findings, the combination of CVD and double layers could lead to the further development of SMCs in a variety of applications.
22 October 2025 in Journal of Electronic Materials