In the current study, the synthesis of hydroxyapatite-ceria (HAP-CeO2) scaffolds is attempted through a bioinspired chemical approach. The utilized colloidal CeO2 suspension presents antifungal activity against the Aspergillus flavus and Aspergillus fumigatus species at concentrations higher than 86.1 ppm. Three different series of the composite HAP-CeO2 suspensions are produced, which are differentiated based on the precursor suspension to which the CeO2 suspension is added and by whether this addition takes place before or after the formation of the hydroxyapatite phase. Each of the series consists of three suspensions, in which the pure ceria weight reaches 4, 5, and 10% (by mass) of the produced hydroxyapatite, respectively. The characterization showed that the 2S series’s specimens present the greater alteration towards their viscoelastic properties. Furthermore, the 2S series’s sample with 4% CeO2 presents the best mechanical response. This is due to the growth of needle-like HAP crystals during lyophilization, which—when oriented perpendicular to the direction of stress application—enhance the resistance of the sample to deformation. The 2S series’s scaffolds had an average pore size equal to 100 μm and minimum open porosity 89.5% while simultaneously presented the lowest dissolution rate in phosphate buffered saline.
In this work, zirconia ceramic structures were fabricated by Direct Ink Writing (DIW) using water-based, yttria-stabilized nano-zirconia pastes. The pastes were prepared from 3 mol% yttria-stabilized zirconia nanopowders synthesized by sol–gel and co-precipitation routes. The effects of dispersant concentration and organic additives on paste preparation and printability were investigated, and the rheological behavior of the printable formulations was evaluated. The microstructure of the sintered 3D-printed specimens was examined by scanning electron microscopy (SEM), while apparent porosity, density, and compressive strength were determined. All printable pastes exhibited shear-thinning behavior. After sintering at 1500 °C, the printed specimens showed submicron grain sizes and apparent porosities as low as 3%. The formulation prepared without acrylamide and crosslinking agent (O12X) exhibited an apparent porosity of 3% and a compressive strength of 350 ± 25 MPa. The co-precipitated-powder formulation (2N) reached compressive-strength values of up to 360 ± 25 MPa. These results demonstrate the feasibility of using high-solids, water-based nano-zirconia pastes for DIW fabrication of dense zirconia structures and support further investigation of this approach for dental applications.