Electrostriction is an intriguing behaviour of dielectric materials, characterized by stable electrostrain with minimal hysteresis. (Na0.5Bi0.5)TiO3-based ceramics show promising electrostrictive behaviour, particularly the 0.90(Na0.5Bi0.5)TiO3-0.08KNbO3-0.02SrTiO3 composition located near the morphotropic phase boundary between ferroelectric rhombohedral and relaxor pseudocubic phases. The templated grain growth method has been effectively used to control the grain orientation of NBT-based systems, thereby enhancing their electrical properties. In this study, texturing was introduced to 0.90(Na0.5Bi0.5)TiO3-0.08KNbO3-0.02SrTiO3 ceramics through homoepitaxial NBT platelets prepared via a three-step molten salt/topochemical microcrystal conversion method. By adding 4 wt% of NBT platelets combined with optimized sintering conditions, textured ceramics were prepared exhibiting a high Lotgering factor of 83% with enhancement of strain (0.02%) and polarization (3 µC/cm2) at an electric field of 40 kV/cm, as well as stable dielectric permittivity between 130 and 300 °C. Moreover, the electrostrictive coefficient of textured ceramics increased by ~0.004 C2m−4 compared to that of untextured ceramics, confirming the improvement of the electrostrictive response. These results demonstrate that homoepitaxial templating effectively improves the electrical properties of NBT-KN-ST ceramics while preserving their electrostrictive nature, which offers a viable route for designing lead-free electrostrictive materials.
Electrostrictive materials based on (Na0.5Bi0.5)TiO3 are promising lead-free candidates for high-precision actuation applications, yet their properties require further improvement. This study aims to enhance the electromechanical properties of a predominantly electrostrictive composition, 0.685(Na0.5Bi0.5)TiO3-0.065BaTiO3-0.25SrTiO3, by using templated grain growth. Textured ceramics were prepared with 1~9 wt% NaNbO3 templates. A high Lotgering factor of 95% was achieved with 3 wt% templates and sintering at 1200 °C for 12 h. Polarization and strain hysteresis loops confirmed the ergodic nature of the system at room temperature, with unipolar strain significantly improving from 0.09% for untextured ceramics to 0.23% post-texturing. A maximum normalized strain, Smax/Emax (d33*), of 581 pm/V was achieved at an electric field of 4 kV/mm for textured ceramics. Textured ceramics also showed enhanced performance over untextured ceramics at lower electric fields. The electrostrictive coefficient Q33 increased from 0.017 m4C−2 for untextured ceramics to 0.043 m4C−2 for textured ceramics, accompanied by reduced strain hysteresis, making the textured 0.685(Na0.5Bi0.5)TiO3-0.065BaTiO3-0.25SrTiO3 composition suitable for high-precision actuation applications. Dielectric properties measured between −193 °C and 550 °C distinguished the depolarization, Curie–Weiss and Burns temperatures, and activation energies for polar nanoregion transitions and dc conduction. Dispersive dielectric constants were found to observe the “two” law exhibiting a temperature dependence double the value of the Curie–Weiss constant, with shifts of about 10 °C per frequency decade where the non-dispersive THz limit was identified.
The thickness of the piezoelectric single crystals is known to have a significant impact on their piezoelectric properties. For high-performance transducers used in high-frequency medical diagnostic applications, the thickness of the piezoelectric single crystals must be reduced. However, the scaling effect, where the piezoelectric and dielectric properties deteriorate as the thickness decreases, remains insufficiently understood, and the mechanisms underlying this phenomenon are unclear. To address this issue, we investigated the changes in polarization and dielectric properties and the underlying mechanism of the scaling effect in alternating current (AC)-poled rhombohedral [001]-oriented 0.72Pb(Mg1/3Nb2/3)O3–0.28PbTiO3 (PMN–28PT) single crystals with respect to the sample thickness. The typical scaling effects, commonly observed with decreasing sample thickness, were confirmed through the degradations in polarization and dielectric properties of AC-poled crystals. The AC-poled crystals exhibited 109.5° domain walls parallel to the (001) plane, and the domain sizes in the surface layer were more than double those in the inner region regardless of thickness. The larger domain size in the surface layer reduces the density of the relatively soft 109.5° domain boundaries, thereby it causes an increase in the coercive field and degradation of the dielectric properties as the thickness decreases. The accumulated space charge on the surface induced an internal bias field for the thin samples, which is considered the origin of the large 109.5° domain size in the surface layer by applying the clamping pressure on the domains within that layer. This unexplored mechanism could contribute to solving the scaling effect problem in PMN–28PT single crystals for high-frequency ultrasound biomicroscope applications.