This paper focuses on the multi-objective optimization of friction stir welding process parameters. Three input variables, including the axial load (AL), tool rotation speed (RS), and tool tilt angle (TA), were selected to optimize the mechanical characteristics of Al-2024 friction stir-welded (FSW) joints. The ultimate tensile strength (UTS) and impact energy (IE) were selected as output responses to measure the mechanical characteristics of Al-2024 FSW joints. A total of nine experiments, using the L9 orthogonal array as part of the Taguchi method, were performed to determine the significance of the process parameters. Gray relational analysis (GRA) was employed to conduct the multi-objective optimization of these combinations of process parameters. The results of the analysis of variance (ANOVA) showed that the AL has the most significant effect on the UTS and IE of Al-2024 FSW joints, followed by the TA and RS. The Taguchi-based GRA analysis revealed that an AL of 10 KN, a TA of 2 degrees, and an RS of 1500 rpm resulted in an optimal UTS of 333.06 MPa and an IE of 40.62 Joules. In these optimal experimental settings, optical microscopy analysis revealed the presence of a recrystallized fine-grain structure in the heat-affected zone of the welded region.
This study aims to evaluate the microstructure and mechanical behavior of aluminum 2024 and stainless steel 304 dissimilar joints. The gas tungsten arc welding (GTAW) process has been employed to weld base metals by inserting copper-nickel-based (Cu-10%Ni) filler metal. The effects of GTAW parameters such as welding current, welding speed, and gas flow on microstructure and tensile strength have been analyzed through the Taguchi method. Results revealed that tensile strength is primarily influenced by welding current, followed by speed and gas flow rate. The excellent joint strength of 138 MPa has been achieved by using Cu-10%Ni filler metal. The optimal combination of parameters, i.e., welding current of level 2 (80 A), welding speed of level 1 (100 mm/min), and gas flow rate of level 3 (10 l/min), has been obtained through SN ratio optimization. Microstructure and EDS analysis depicted that the weld zone of a high-strength joint contained fine dendrites and CuAl and NiAl solid solutions, while the weld zone of a low-strength joint featured coarse dendrites and brittle FeAl phases.