This paper addresses the mechanical characterization of dissimilar overlap joints made by autogenous laser welding between thin sheets of low-carbon steel (CS) and austenitic stainless steel (SS) with an optimized welding technology able to produce sound overlap joints. This involved applying the laser beam from the CS-side to reduce the SS overheating. The research is focused on the analysis of combined tensile-shear behavior of the weld and of the heat-affected zones. During testing, the applied tensile-shear load rotates the weld connecting the CS and SS plates. The rotation angle transmitted to the free ends of the plates, together with relevant strain fields, were measured by using a digital image correlation system, VIC-2D. Thus, it was found that the weld acts as a non-linear hinge which experiences a sudden loss of stiffness when strain concentrations develop from the weld ligament edges towards the loaded sides of the plates. The welded joint fails by yielding localization and necking in the CS plate, far from the weld. This mode of failure is a consequence of the weld and heat-affected zone strength mismatches of 1.09 and 1.33, respectively. These values are consistent with the hardness profile and the documented microstructural heterogeneities.
The paper addresses the fatigue resistance, fracture behavior, and damage tolerance of a new type of ultrahigh-strength bar for prestressing concrete made of a low-alloy lath martensitic steel. The fracture tests show that the bar steel has a medium-high fracture toughness of 75 MPa m1/2 and a fatigue cracking resistance that fits the Paris-Erdogan Law as most of Eurocode 3 structural steels. The damage tolerance analysis combines two failure assessment diagrams (FADs), the first focused on the damage level and the second on toughness and yielding capacity as material properties of the bar steel, whose influence and interaction are determinant for failure. The location of the experimental failure data in the FADs indicates that the steel is endowed with a combination of strength, ductility, and toughness able to prevent unexpected failures. The damage micro-mechanisms revealed from the examination of broken specimens differ from fatigue to fracture cracking, but in a manner consistent with the observed mechanical behavior and microstructure of the bar steel.
The paper addresses the fatigue resistance, fracture behavior and damage tolerance of a new type of ultrahigh-strength bar for prestressing concrete made of a low-alloy lath martensitic steel. The fracture tests showed that the bar steel has a medium-high fracture toughness of 75 MPa√m and a fatigue cracking resistance that fits the Paris-Erdogan Law as most of Eurocode 3 structural steels. The damage tolerance analysis combines two Failure Assessment Diagrams – FADs, respectively involving the damage level and the toughness, and yielding capacity influences on the failure of the bar steel. The location of the experimental failure data in the FADs indicate that the steel is endowed with a combination of strength, ductility and toughness able to prevent unexpected failures. The damage micro-mechanisms revealed from the examination of broken specimens differ from fatigue to fracture cracking, but in a manner consistent with the observed mechanical behavior and microstructure of the bar steel.
This paper assesses experimentally and theoretically the hydrogen-assisted cracking sensitivity of an ultrahigh-strength lath martensitic steel, recently used to manufacture tendon rods for structural engineering. The experimental values of the J-integral were obtained by tensile testing up to failure precracked SENT specimens in air, as an inert environment and in a thiocyanate aqueous solution, as a hydrogen-promoter medium. In parallel, the theoretical resources necessary to apply the Dugdale cohesive model to the SENT specimen were developed from the Green function in order to predict the J-integral dependency on the applied load and the crack size, with the cohesive resistance being the only material constant concerning fracture. The comparison of theoretical and experimental results strongly supports the premise that the cohesive crack accurately models the effect of the mechanisms by which the examined steel opposes crack propagation, both when in hydrogen-free and -embrittled conditions. The identification of experimental and theoretical limit values respectively involving a post-small-scale-yielding regime and unstable extension of the cohesive zone allowed for the value of the cohesive resistance to be determined, its condition as a material constant in hydrogen-free medium confirmed, and its strong decrease with hydrogen exposure revealed.
This research work addresses the mechanical and metallurgical characterisation, as well as the failure features, of two types of lap-fillet autogenous laser-welded joints made of ultra-thin sheets by applying an appropriate welding technology for producing sound welds and flawless joints. Both welded samples, one made only of stainless steel (SS-SS) sheets, and the other made of stainless steel and carbon steel (SS-CS) plates, were subjected to tensile–shear loads that are representative of the in-service conditions. The experimental research was focused on determining, by the digital image correlation (VIC-2D) method, the strain field and the rotation angle of the welded joints that were developed during loading tests of the welded specimens. Comparing to the classical testing method applied to study the joint overall mechanical properties, the novelty of this research consists of local mechanical behaviour assessment of relevant zones from similar and dissimilar welded joints, by using the innovative technique VIC-2D. Based on the analysis of the experimental results, it was found that the maximum rotation angle is 2.5 times higher in the SS-SS similar welded joint, in comparison with the SS-CS dissimilar welded joint. Despite this finding, the SS-CS specimen failed in the CS base material, far from the weld, with the failure phenomenon being preceded by the material yielding and necking. This failure mode is consistent with the detected strength mismatch of the SS-CS joint, with respect to the CS base material. In contrast, the quasi-ductile fracture of the SS-SS welded joint occurred by plastic exhaustion at the boundary between the narrow Heat-Affected Zone (HAZ) of SS and the Fuzion Zone (FZ). These outcomes are consistent with the hardness profile, microstructural heterogeneities found in the lap-fillet welded joints, and the load versus elongation curves that are determined and discussed in this paper. This research provides new insight and original information on the materials’ response to the autogenous laser welding, which will contribute to improving the knowledge on the ultra-thin lap-fillet welded similar and dissimilar steels.