High-crystalline-quality wide-bandgap metal halide perovskite materials that achieve superior performance in perovskite solar cells (PSCs) have been widely explored. Precursor concentration plays a crucial role in the wide-bandgap perovskite crystallization process. Herein, we investigated the influence of precursor concentration on the morphology, crystallinity, optical property, and defect density of perovskite materials and the photoelectric performance of solar cells. We found that the precursor concentration was the key factor for accurately controlling the nucleation and crystal growth process, which determines the crystallization of perovskite materials. The precursor concentration based on Cs0.05FA0.8MA0.15Pb(I0.84Br0.16)3 perovskite was controlled from 0.8 M to 2.3 M. The perovskite grains grow larger with the increase in concentration, while the grain boundary and bulk defect decrease. After regulation and optimization, the champion PSC with the 2.0 M precursor concentration exhibits a power conversion efficiency (PCE) of 21.13%. The management of precursor concentration provides an effective way for obtaining high-crystalline-quality wide-bandgap perovskite materials and high-performance PSCs.
15 December 2020 in Journal of Materials Chemistry A
Two benzotrithiophene-based two-dimensional non-fullerene acceptors (NFAs) were designed and synthesized to investigate the effects of a fused or unfused NFA molecular backbone on the performance of organic solar cells.
Perovskite solar cells (PSCs) can utilize the residual photons from indoor light and continuously supplement the energy supply for low-power electron devices, thereby showing the great potential for sustainable energy ecosystems. However, the solution-processed perovskites suffer from serious defect stacking within crystal lattices, compromising the low-light efficiency and operational stability. In this study, we designed a multifunctional organometallic salt named sodium sulfanilate (4-ABS), containing both electron-donating amine and sulfonic acid groups to effectively passivate the positively-charged defects, like under-coordinated Pb ions and iodine vacancies. The strong chemical coordination of 4-ABS with the octahedra framework can further regulate the crystallization kinetics of perovskite, facilitating the enlarged crystal sizes with mitigated grain boundaries within films. The synergistic optimization effects on trap suppression and crystallization modulation upon 4-ABS addition can reduce energy loss and mitigate ionic migration under low-light conditions. As a result, the optimized device demonstrated an improved power conversion efficiency from 22.48% to 24.34% and achieved an impressive efficiency of 41.11% under 1000 lux weak light conditions. This research provides an effective defect modulation strategy for synergistically boosting the device efficiency under standard and weak light irradiations.
Flexible perovskite solar cells (F-PSCs) have the advantages of high power-per-weight, solution processability, and bending durability and have emerged as a competitive photovoltaic technology for various applications. As the core electron transport layer (ETL) in n-i-p-type device configurations, the solution-processed SnO2 generally suffers from serious defect stacking on films, compromising the charge transport properties and the performance of resulting devices. Herein, we proposed a media-filling strategy to optimize the contact quality at the buried interface by introducing Al2O3 nanoparticles on the SnO2 surface. Rather than forming a compact insulating layer, the Al2O3 can fill the grain boundaries of SnO2 and smooth the substrate surface. Optimized interfacial contact under careful concentration control can rationally minimize the contact area of the perovskite with the surface imperfections of SnO2 to mitigate trap-assisted charge recombination. Furthermore, the reduced surface roughness of SnO2 facilitates the uniform deposition and oriented growth of upper perovskite film. As a result, the target F-PSCs achieved an impressive efficiency of 23.83% and retained 80% of the initial performance after 5000 bending cycles at a radius of four mm.
Hot-spot generation is critical to the performance and lifespan of photovoltaic (PV) modules; however, the underlying mechanisms of hot-spot formation have not been fully elucidated. This work conducted a localized shading test on a PV module, measured the micro-electrical characteristics and temperature distributions of both the shaded and unshaded cells, calculated the heat-source power densities, and then predicted the occurrence and locations of hot and cold spots via numerical simulations. It was found that, under an irradiance of 750 W/m2, when one cell in a PV module is shaded by 1/2, the unshaded area within the shaded cell exhibited a hot spot, with the temperature reaching up to 77.66 °C, approximately 22.5 °C higher than the surrounding cells. The intrinsic mechanism for the occurrence of the hot spot is that, compared with the unshaded cells, the unshaded portion of the shaded cell can generate an extra significantly large Joule heat power density, about 1079.62 W/m2. The reason for generating such a large Joule heat power density is that this portion is in a reverse-bias state with a high current density flowing through it, according to our measurements. In contrast, the shaded portion forms a cold spot, about 7.5 °C cooler than the surrounding cells. This is because the shaded portion can only generate a Joule heat power density of about 46.98 W/m2 due to the small reverse-bias current density flowing through it and fails to absorb heat from solar irradiance, which is about 645 W/m2. Moreover, this work demonstrates that the hot-spot temperature initially rises and then decreases with increasing shading ratio, with the highest temperatures and the most pronounced temperature changes occurring around a shading ratio of 1/2. The presented method can be also used to evaluate the performance and reliability of various other PV modules under local shading conditions.