Background/Objectives: This study aimed to investigate the microtensile bond strength (µTBS) of composite-based (Cerasmart), polymer-infiltrated (Vita Enamic), and feldspathic (Cerec) CAD/CAM blocks luted to dentin using a dual-cure resin cement (LinkForce), as well as micro-hybrid (G-aenial) and flowable composites (G-aenial Universal Flo), and evaluate the microhardness (HV) of luting materials through the CAD/CAM blocks. Methods: Cerasmart, Enamic, and Cerec were luted to dentin using three luting materials; LinkForce, G-aenial, and Universal Flo (n = 5). For HV, 117 disk-shaped specimens from LinkForce, G-aenial, and Universal Flo (n = 13) were polymerized through 3 mm thick CAD/CAM. Thirty-nine light-cured specimens without CAD/CAM were used as control. Following 24 h storage, the µTBS and HV were evaluated. Data were analyzed using the two-way ANOVA and post hoc Tukey tests (p < 0.05). Results: The µTBS to dentin and HV were significantly influenced by the type of luting material and CAD/CAM material. With all the CAD/CAM materials, LinkForce and Universal Flo exhibited a significantly similar µTBS to that of dentin (p > 0.05). Compared with the control group, all the HV values of the luting materials decreased significantly (p < 0.05). Conclusions: Heavily filled flowable composites exhibit a bonding effectiveness similar to that of dual-cure resin cements. All the luting materials showed similar HV when polymerized through the polymer-infiltrated CAD/CAM material.
This study assessed the repair shear bond strength (SBS; MPa) and surface roughness (Ra; μm) of aged hybrid ceramic (Cerasmart270, GC) and nano-hybrid ceramic (Grandio Blocs, Voco) CAD/CAM blocks after different surface pretreatment methods. In this study, 2 mm thick Cerasmart270 and Grandio Blocs were cut into slabs (Isomet; n = 80 per group). Following aging for six months, the specimens in each CAD/CAM material were randomly divided into four groups (n: 20 each) according to the surface pretreatments: control (no pretreatment), Er:YAG laser, sandblasting, and bur grinding. A total of 10 specimens in each CAD/CAM material pretreatment group were used for Ra evaluation (Perthometer Mahr), while the other 10 were for SBS. After the application of a silane primer (G-Multi Primer, GC) and universal adhesive (G2-Bond, GC), composite build-ups (Filtek Z250; 3MESPE) were performed for the SBS evaluation. After storage in distilled water for 24 h, SBS was evaluated with a universal testing machine (Instron). SBS and Ra data were analyzed with two-way ANOVA and Tukey’s post hoc tests (p < 0.05). SBS was significantly affected by the surface pretreatment methods (p = 0.0001) and by the types of CAD/CAM material (p = 0.005). Bur grinding showed the highest SBS for both CAD/CAM materials, while the control groups yielded significantly lower SBS than bur grinding and sandblasting (p < 0.05). Er:YAG lasers did not significantly enhance the SBS compared to the control group. Sandblasting presented significantly higher SBS than lasers only in Grandio Blocs (p < 0.05). The surface pretreatment methods significantly influenced Ra (p = 0.0001); however, no significant interaction was found between the types of CAD/CAM material and the surface pretreatments (p > 0.05). Control groups exhibited, significantly, the lowest Ra for both materials (p = 0.0001), while no significant differences were observed between the other pretreatment methods. Bur grinding was identified as the most effective pretreatment method for repairing hybrid ceramic CAD/CAM materials.
This study aimed to evaluate the effect of preheating on the push-out bond strength (PBS) and microhardness (HV) of fiber-reinforced flowable and injectable composites and to compare them with dual-cure resin–cement for post cementation. Fifty premolars were endodontically treated, and post spaces were prepared. Specimens were divided into five groups (n = 10) based on the resin luting material. After adhesive application, fiber posts were luted with dual-cure resin–cement (LinkForce), fiber-reinforced flowable composites (EverX Flow; non-heated/preheated), and injectable composites (G-aenial Universal Injectable; non-heated/preheated). After 24 h, roots were sectioned (coronal, middle, apical) for PBS testing (Instron). For HV, 10 specimens per resin luting material were prepared, and top/bottom microhardness was measured to assess the depth of cure. Data were analyzed with two-way ANOVA and post hoc Tukey tests (p < 0.05). Both types of resin luting material and preheating significantly affected PBS and HV (p = 0.0001). Preheated EverX Flow showed significantly higher PBS and HV than LinkForce, while G-aenial Injectable exhibited the lowest values (p < 0.05). Within each resin luting material, PBS significantly decreased from the coronal to the apical region (p = 0.0001). Preheated fiber-reinforced flowable composites demonstrate improved microhardness and adhesion, offering a reliable alternative to the dual-cure resin–cements for fiber post cementation.