Ceramic solid solutions Bi4(V1−xZrx)2O11−z (I), (Bi1−yLay)4V2O11−z (II) and (Bi1−yLay)4(V0.96Zr0.05)2O11−z (III) with x < 0.30, y < 0.20, were prepared by the solid state reaction method and were investigated by means of various experimental techniques. The low temperature ferroelectric α-phase exists in the solid solutions with x, y ≤ 0.05. The phase transition to paraelectric β-phase was revealed in these compositions by the dielectric spectroscopy, SHG and DTA/DSC methods. Dielectric permittivity measurements confirmed an effect of the domain walls “pinning” due to the presence of oxygen vacancies inherent to the bismuth vanadate based structures. Switching of ferroelectric domains by an external electric field was observed in Piezoresponse Force Microscopy experiments.
Ceramic solid solutions (1-x)(Bi0.9Nd0.1)(Sc0.9B0.1)O3 - xPbTiO3 (x = 0.60–0.66; B - Lu, Yb, Er, Y) based on the compositions close to the morphotropic boundary, have been prepared. To improve the phase content and the resistance of ceramics, Bi2O3 and MnO2 additives were used. Phase composition, structure, microstructure, phase transitions, ferroelectric and piezoelectric properties have been studied. The 1st order ferroelectric phase transitions are marked by peaks near 700–750 K in dielectric permittivity and dielectric loss temperature dependences. Effect of dielectric relaxation was observed, its relation to composition of ceramics determined. The Curie temperature TC increase was observed with increasing the PbTiO3 constituent, while the TC decrease is typical of the A- or B-cations doped compositions. Introduction of MnO2 and/or Bi2O3 additives lead to the decrease of total conductivity and dielectric losses to more than one order at elevated temperatures. Enhanced d33 and kt values were measured in modified ceramics.
1 August 2011 in Bulletin of the Russian Academy of Sciences: Physics
The ferroelectric and piezoelectric properties of ceramic solid solutions having a composition of (1−x)(Bi0.9Nd0.1)(Sc0.9B0.1)O3 − xPbTiO3 (x = 0.60–0.66; B = Lu, Yb, Er, Y) and obtained by solid state reaction were studied. An increase in the Curie temperature was found upon an increase in the concentration of lead titanate, while a drop occured upon the doping of the A and B sublattices. It was shown that at high temperatures, MnO2 and Bi2O3 additives lead to a reduction in the total conductivity and a dielectric loss of less than one order of magnitude. In modified ceramics, an increase in the d33 and kt piezoelectric coefficients was observed as well. The effects of dielectric relaxation that are determined by the composition of the ceramics were revealed.
To establish the connection between structure, conductivity and luminescence properties, the Na3Sc2−xRx(PO4)3 (R = Eu, Tb, Dy; 0 ≤ x ≤ 0.2) compounds have been studied. Solid solutions with a NASICON-type structure were formed at 0 ≤ x ≤ 0.1.