Here, we fabricate poly(vinylidene fluoride-co-hexafluoropropene) (PVDF-co-HFP) by electrospinning for a gel polymer electrolyte (GPE) for use in flexible Li-ion batteries (LIBs). As a solvent, we use N-methyl-2-pyrrolidone (NMP), which helps produce the cross-linked morphology of PVDF-co-HFP separator, owing to its low volatility. The cross-linked PVDF-co-HFP separator shows an uptake rate higher than that of a commercialized polypropylene (PP) separator. Moreover, the PVDF-co-HFP separator shows an ionic conductivity of 2.3 × 10−3 S/cm at room temperature, comparable with previously reported values. An LIB full-cell assembled with the PVDF-co-HFP-based GPE shows capacities higher than its counterpart with the commercialized PP separator, confirming that the cross-linked PVDF-co-HFP separator provides highly efficient ionic conducting pathways. In addition, we integrate a flexible LIB cell using the PVDF-co-HFP GPE with a flexible organic light emitting diode (OLED), demonstrating a fully flexible unit of LIB and OLED.
LTO (Li4Ti5O12) has been highlighted as anode material for next-generation lithium ion secondary batteries due to advantages such as a high rate capability, excellent cyclic performance, and safety. However, the generation of gases from undesired reactions between the electrode surface and the electrolyte has restricted the application of LTO as a negative electrode in Li-ion batteries in electric vehicles (EVs) and energy storage systems (ESS). As the generation of gases from LTO tends to be accelerated at high temperatures (40–60 °C), the thermal stability of LTO should be maintained during battery discharge, especially in EVs. To overcome these technical limitations, a thin layer of Al2O3 (~2 nm thickness) was deposited on the LTO electrode surface by atomic layer deposition (ALD), and an electrochemical charge-discharge cycle test was performed at 60 °C. The capacity retention after 500 cycles clearly shows that Al2O3-coated LTO outperforms the uncoated one, with a discharge capacity retention of ~98%. TEM and XPS analyses indicate that the surface reactions of Al2O3-coated LTO are suppressed, while uncoated LTO undergoes the (111) to (222) phase transformation, as previously reported in the literature.