Fiber reinforced composites materials have been much more attention in the materials system by the researchers since their unique performance in various structural applications. The addition of fiber and various chemical treatments produces the best mechanical properties of the composite material. However, several authors have described the working mechanism in mechanical composites. Recently researchers have started to investigate the free vibrational behavior of the composites and to find the suitable applications in industry. It is indeed important to represent the vibrational response of the fiber reinforced composites (FRC) toward the anti-vibration applications. Thus, an attempt was made to review the vibration behaviors on natural fiber, synthetic fiber, and filler incorporated natural/synthetic fiber composites. Discussions on the comparison of the natural frequency and damping ratio of various composites bring comprehensive knowledge on vibrational behaviors of various fiber reinforced composites.
The present study looks into the effect of WEDM process parameters on the material removal rate (MRR) and surface roughness (SR) responses when machining hybrid composites (Al-Si12/boron carbide/fly ash) using the Taguchi technique. Fly ash and boron carbide (B4C) particles were used for reinforcement (3, 6, and 9 by weight), and aluminium alloy (Al-Si12) was used as a matrix material. ANOVA was used to find out the importance of machining factors that affect the quality features of the WEDM process, as well as the relative role of input parameters in determining the WEDM process responses. The greatest impact on the response is finalised by the signal-to-noise (S/N) ratio response analysis. However, as a last step, a confirmation experiment with the best combination was carried out to predict and validate the accuracy of the observed values. As the pulse on time and reinforcement increases, MRR also increases. As the gap voltage, wire feed, and pulse off time decrease, it increases. SR is increased by increasing the gap voltage, pulse on time, and pulse off time, wire feed, and reinforcement. The maximum MRR of 38.01mm3/min and the minimum SR of 3.24μm were obtained using optimal machining conditions.
1 January 2018 in International Journal of Computer Aided Engineering and Technology
In this work, dynamic mechanical analysis (DMA) of untreated luffa fibre composites has been carried out. Composites are produced using luffa fibre mat and polyester resin. Compression moulding is done at 5MPa pressure from 30 to 50% for varying fibre loading. Temperature ramped dynamic mechanical analysis is done to understand the fibre loading effects on dynamic properties. Results show, that increase in fibre loading significantly increase the storage modulus of the composites without any change in mechanical characteristics. Cole-Cole plot is drawn to understand the elastic-plastic behaviours and results reveal that, the more fibre is mixed content the more the elastic behaviour is found.
The work addresses the cutting performance of luffa cylindrica fiber–reinforced composite by abrasive water jet machining (AWJM). The composite (30, 40, and 50 wt. % fiber) is prepared using the compression molding technique. The extracted fiber morphology and the composite properties were analyzed, as per ASTM. The influence of machining parameters, such as jet pressure (P), traverse speed (TS), and standoff distance (SoD) over the taper angle (TA) and surface roughness (Ra), were analyzed. Based on the experimental results, it was observed that a higher value of P and lower TS and SoD resulted with minimum TA and Ra. The developed multilinear regression model confirms the goodness-of-fit at 95 % confidence interval. The optimum condition to set (P at 25 MPa, SoD at 1.1414 mm, and TS at 20 mm/min) for attaining minimum TA and Ra were determined by desirability analysis. Further, the analysis of variance (ANOVA) of TA depicted a contribution of 41.71 % by SoD, followed by TS and P by 27.33 % and 23.74 %, respectively. Similarly, the ANOVA of Ra resulted with a contribution of 16.72 % by P, 39.15 % by SoD, and 30.73 % by TS. Finally, the cut surface morphology of the composite was analyzed at optimum condition, and the results are revealed.