In heavy metal industrial areas, the issue of insulation flashover caused by metal contamination on the external insulation of transmission lines has become increasingly prominent. This paper investigates the U160B/155 porcelain insulator, examining how iron, copper and zinc metal contaminations affect its AC flashover characteristics. Furthermore, combining with leakage current, the flashover mechanism of the insulators under the influence of metal particles is analysed. The research results indicate that as the metal content increases, the insulator's flashover gradient ( EL ) decreases by up to 2.3%–17.2%. Different metal compositions exhibit consistent mechanisms, similarly impacting insulator's dielectric strength with copper showing slightly weaker effect. And then, based on the mechanism of metal particles' influence on the insulator's AC flashover, a formula for calculating EL is proposed and the calculated results are basically consistent with the experimental conditions. Finally, different metal compositions have similar effects on the leakage current, with an increase in metal content leading to an increase in the critical leakage current, which gradually tends to saturation. The research findings of this paper can provide references for AC flashover prediction, assessment and prevention of external insulation in areas with metal contaminants in pollution sources.
5 August 2025 in IEEE Transactions on Dielectrics and Electrical Insulation
The utilization of epoxy resin insulators for high voltage insulation continues to expand; however, surface flashover remains its significant challenge. Conventional methods for improving surface flashover voltage in epoxy insulators basically focus on physical and chemical changes while neglecting environmental and sustainability concerns involving petroleum epoxy resins. In this study, eco-friendly castor oil is incorporated into the epoxy matrix to enhance surface flashover voltage while promoting reduction of overreliance on finite petroleum resources. The successful integration of castor oil into the epoxy matrix is confirmed by Fourier Transform Infrared Spectroscopy, whereas the Atomic Force Microscopy and Scanning Electron Microscopy reveal smooth surfaces of composites at relatively low concentrations of castor oil, while higher concentrations beyond 30% lead to an increase in roughness. Samples’ relative permittivities are analyzed by using a Novocontrol spectrometer, which reveals the decrease in relative permittivity with the addition of castor oil into epoxy matrix. Notably, the positive and negative flashover voltages are enhanced by 17.47% and 18.49% respectively, at a castor oil concentration of 30 wt% with respect to epoxy resin, which is attributed to moderate trap parameters alongside favorable charge carrier mobility. These findings suggest that epoxy-castor oil biocomposite is a potential high voltage insulation material with reduced petroleum quantity and enhanced flashover voltage.
The operation status of transmission line insulators, such as damage, zero-value, pollution, and deterioration, affect the safe operation of power grids. Non-contact detection technology judges the operating status of transmission line insulators through indirect means such as electrical, thermal, acoustic, and image signals. Due to its advantages of rapidity and high efficiency, it has been widely accepted by operation departments. This paper summarizes existing non-contact detection technologies for transmission line insulator conditions, including acoustic wave detection, electric field detection, infrared/ultraviolet imaging detection and spectral detection. It analyzes the principle, characteristics, and application scenarios of each non-contact detection technology. Combined with the rapid development of artificial intelligence technology, the paper looks forward to future new detection methods, such as those integrating deep learning, multi-component comprehensive detection, and multi-source data-driven detection. Finally, the challenges faced by the detection of Ultra-High Voltage (UHV) transmission lines are analyzed. This study provides a reference for the research and development of non-contact detection technology for transmission line insulators.
9 June 2025 in IEEE Transactions on Dielectrics and Electrical Insulation
The contamination on the surface of insulators in metal industrial areas contains a significant amount of metal dust. The impact of insoluble metal dust on insulator pollution flashover is a matter of great concern for power grid operation departments. This paper takes U160B/155 porcelain insulators as the research object and experimentally investigates the influence of insoluble metal iron dust with different ratios and particle sizes in non-soluble deposit density (NSDD) on their AC pollution flashover voltage. The mechanism of its influence on AC pollution flashover of insulators is analyzed in combination with the distribution of metal particles and leakage current. The results indicate that as the ratio of metal iron dust (K) in NSDD increases, the AC pollution flashover voltage of the insulator string decreases, and the critical leakage current increases. Compared with NSDD without metal dust, the pollution flashover voltage is approximately 5.3%~17.2% lower, and the critical leakage current increases by approximately 3.4%~20.0%. Under the same mass of metal dust, the smaller the metal particle size, the lower the pollution flashover voltage. The influence of metal dust on the pollution flashover voltage of insulator strings is similar to short-circuiting the creepage distance of the insulator strings. For areas with pollution sources containing metal dust, the impact of metal deposits on insulator pollution flashover should be considered separately. The findings of this paper can provide a reference for external insulation design and pollution flashover early warning in areas with pollution sources containing metal components.
The severe atmospheric environment at high altitudes and the variability in electrode shapes of power equipment complicate the insulation design of air gaps. In this paper, switching impulse discharge tests were carried out on 1‒5 m gaps of 15 different electrodes in 5 categories under the natural environment at an altitude of 1500 m. It is verified that the influence of electrode shape on the switching impulse 50% breakdown voltage (U50) of air gaps is independent of the gap distance (d) and absolute humidity (H). The electrode shape can cause the U50 of the 4 m gap to fluctuate in 1051.3‒1178.0 kV. Then, combined with finite element simulation, the spatial electric field non-uniformity of different electrode gaps was studied. The results show that with the increase of non-uniformity, the breakdown voltage of the gap decreases rapidly first, and then tends to be stable. Finally, the mathematical relationship among U50, d, H and electrode curvature radius (r) is obtained, which verifies that the atmospheric factors have the most significant influence on U50, followed by d and r. On this basis, gap factors (0.972–1.083) for different electrode gaps are proposed. The error between the U50 evaluation based on the gap factors and the experimental values is less than 5%.