The article provides a brief overview of technologies and methods for processing dispersed metallic waste generated during ferroalloy production, including high-carbon ferrochrome (HCFeCr). It is noted that the most cost-effective and rational method for reusing metallic dust is briquetting. Considering the development of briquetting technologies, as well as the latest equipment and binder materials involved in this process, aspiration dust from ferrochrome crushing can be fully utilized in metallurgical recycling. To verify this assumption, laboratory studies were conducted using polymer-based binders and liquid glass as a baseline option. The methodology of briquetting using both laboratory and industrial presses is described, along with an assessment of the mechanical properties of the briquettes. The studies indicate that the introduction of an inert filler (gas-cleaning dust) into the metallic dust composition improves the briquetting ability of the mixture by enhancing adhesion between metal particles and the binder. The obtained industrial briquette samples exhibit high mechanical strength, ensuring their further use in metallurgical processing. The study concludes that semi-dry briquetting using hydraulic vibropresses is a promising approach for the utilization of dispersed ferroalloy waste.
This study presents the results of laboratory experiments on the processing of lateritic nickel ores mixed with coal and CaO, followed by the use of the obtained product for the smelting of nickel-containing ferroalloy by the metallothermic method. The study analyzed the thermodynamic effects of complex reductant concentration (silicon- and aluminum-containing alloy) on the reduction degree of nickel and iron. An experimental process resulted in a product containing Nitotal (2.60%) and Fetotal (60.52%), obtained through reduction roasting of lateritic nickel ore mixed with coal and an addition of 20 g of CaO at a temperature of 1150 °C. Under laboratory conditions, a nickel-containing ferroalloy was successfully obtained using the product after reduction roasting and a complex alloy as the reducing agent. The following optimal process parameters were determined: reductant consumption of 20 g per 100 g of the reduction roasting product, smelting temperature of 1600 °C, and slag basicity (CaO/SiO2) of 0.5. In this case, a nickel-containing ferroalloy with 72% iron, 15% nickel, and up to 5% chromium was successfully obtained through silicon and aluminum reduction using a complex alloy. A microstructural analysis of the nickel-containing alloy was conducted using an electron probe microanalyzer (JXA-8230) in combination with scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS). The results showed that silicon and iron were the dominant elements in all particles. Nickel was detected at concentrations of up to 15.02 wt. %, while chromium reached 3.47 wt. %. Depending on the silicon concentration, the nickel-containing ferroalloy is recommended for corrosion-resistant steel production (Si < 5%) and as a reducing agent for ferronickel production (Si > 5%).
Fine classes of metal dust generated during the production of ferroalloys increase the likelihood of irretrievable losses, creating the prerequisites for the development of rational methods for processing this material. One of the known technologies for recycling dispersed raw materials in metallurgical processing is their direct remelting. Although this technology is easily feasible, it has several significant drawbacks, among which the main problem remains the high dust carryover of fine material by ascending gas-thermal flows. A potential solution could be the preliminary preparation of raw materials through agglomeration. Domestic enterprises producing various types of ferroalloys have the necessary infrastructure and equipment for agglomerating dispersed ore materials, but the lack of experience and resource-saving technologies for processing metal dust prevents their full integration into metallurgical processing. In this regard, there is significant interest and demand from ferroalloy enterprises for the development of new methods to involve dispersed metal production waste in secondary recycling, adapted to existing agglomeration equipment. Numerous studies have shown that the cheapest method of agglomeration is briquetting. Given the advancement of briquetting technologies, as well as the use of the latest equipment and binding materials in this process, it can be assumed that this will allow for more complete integration of aspiration dust from ferrochrome crushing into metallurgical processing. To test this assumption, studies were conducted on the physicochemical properties of aspiration dust from ferrochrome crushing, assessing the possibility of obtaining an agglomerated product with the required strength parameters. The results of these studies demonstrated the fundamental possibility of producing high-carbon ferrochrome from briquetted material made from aspiration dust of ferrochrome crushing.
In the process of producing ferroalloys, a large amount of secondary raw materials is formed, including slag, aspiration dusts and sludge. The recycling of secondary raw materials can create resources and bring environmental and economic benefits. Wet secondary raw materials (WSRMs) are characterized by a high chromium oxide content (averaging 24%), but due to their high moisture levels, they cannot be directly used in arc furnaces. As a strategic approach, mixing WSRMs with drier, more chromium-rich dusts (up to 45% Cr2O3) has been proposed. This not only reduces the overall moisture content of the mixture but also enhances the metallurgical value of the charge material. This paper presents the results of laboratory studies on the agglomeration of secondary wet raw materials using briquetting, extrusion and pelletizing methods. The main factors influencing the quality of the resulting product were analyzed, including the method of agglomeration, the composition of the mixture, as well as the type and dosage of the binder component. The strength characteristics of the finished agglomerated samples were evaluated in terms of resistance to splitting, impact loads and falling. Notably, the selected binders are organic and polymer substances capable of complete combustion under metallurgical smelting conditions.
This study addresses the problem of efficient utilization of aspiration dust (AD) generated during crushing of high-carbon ferrochrome (HCFeCr). To solve this issue, a briquetting technology was proposed, involving aspiration dust blended with dry gas-cleaning dust (20 wt.% as filler) and an organic polymer binder (3 wt.%). The produced briquettes demonstrated high mechanical strength (average 195 kg per briquette in splitting strength and 98% drop resistance), ensuring maximum integrity during transportation and handling. Pilot-industrial remelting of 35 tons of briquettes in a 1.8 MVA direct current electric arc furnace (DC EAF) confirmed the effectiveness of the proposed technology for HCFeCr production. Chromium recovery into the alloy reached 94%, which is 3–4% higher compared to remelting of loose dust. The specific electric energy consumption was 1600 kWh/t, representing a 29% reduction compared to loose dust processing. The produced metal met commercial grades FeCr800–FeCr900 specifications. Additional advantages included elimination of dust formation, reduction in fines generation during crushing of the final metal to 15%, and improved environmental performance. The developed technology represents an economically and environmentally viable solution for comprehensive recycling of ferroalloy dust waste.