Wood is a natural material that presents a great variation of properties. Many treatments have been developed in order to extend the service life of wood products. Nowadays, products with low toxicity and economic viability are a challenge to researchers. Nanotechnology has been indicated as a solution to this issue, since wood preservatives can be utilized in low concentration, promoting satisfactory results in terms of protection with no color changes. The main goal of this review is to present nanotechnology advances on wood protection. Self-cleaning surfaces, scratch and weathering resistance, and biocides properties have been achieved through nanoparticles (NPs) applications. Studies evaluating the performance of NPs from silver (Ag), boron (B), copper (Cu), zinc (Zn), zinc oxide (ZnO), zinc borate (B2O6Zn3), and titanium dioxide (TiO2) on wood protections have reported promising findings. Tests performed against termites, rot, mold and stain fungi, and UV degradation have demonstrated that some biocides have their properties improved in nanoscale. Controlled release and encapsulation technologies are another important matter once it can increase the effectiveness of wood treatments. NPs risk assessment for human health and the environment are still incipient. Despite of that, some products as nanozinc oxide (nanoZnO) and titanium dioxide (nanoTiO2) present encouraging potential. NanoZnO and NanoTiO2 have been reported as promising antifungals, antibacterials, and antiviral agents; beyond theirs biocides properties, low ecotoxicity impacts to the environment are expected. Based on this review, we consider that wood treatments based on NPs may play an important role in the next generation of wood protection systems.
22 October 2021 in Nordic Pulp & Paper Research Journal
The accumulation of petroleum polymers compromises biodiversity and causes environmental problems. Nanocellulose enhances biodegradability and can improve the physical-mechanical performance of materials. The objective was to produce and characterize hybrid films composed of bacterial cellulose (BC) and plant nanocellulose from Eucalyptus (Euc) or Pinus (Pin). Films were produced by the casting method using filmogenic suspensions with different cellulose nanofibrils (CNFs) proportions from both the sources (0, 25, 50, 75 and 100 %). CNFs suspensions were characterized by transmission electron microscopy. The morphology of the films was analyzed using scanning electron microscopy. In addition, the transparency, contact angle, wettability, oil and water vapor barrier and mechanical properties were also evaluated. The contact angles were smaller for films with BC and the wettability was greater when comparing BC with plant CNFs (0.10 ° s − 1 {\text{s}^{-1}} for 75 % Euc/25 % BC and 0.20 ° s − 1 {\text{s}^{-1}} for 25 % Euc/75 % BC). The water vapor permeability (WVP) of the 100 % BC films and the 25 % Euc/75 % BC composition were the highest among the studied compositions. Tensile strength, Young’s modulus and puncture strength decreased considerably with the addition of BC in the films. More studies regarding pre-treatments to purify BC are needed to improve the mechanical properties of the films.
29 January 2022 in Nordic Pulp & Paper Research Journal
The accumulation of petroleum products causes damage to ecosystems, which can be avoided with cellulose-based products. The influence of different ratios of cellulose micro/nanofibrils (MFC/NFC) on the properties of hydroxypropyl methylcellulose (HPMC) films was evaluated. Films were prepared using proportions of 0, 25, 50, 75 and 100 % (w/w) of MFC/NFC from Pinus sp. in relation to HPMC. Physical, barrier, surface, optical, morphological and mechanical properties were evaluated. Solids content, basis weight and density values increased with higher amount of MFC/NFC and thickness and porosity were reduced. SEM images showed that films with more than 50 % MFC/NFC had a more granular surface, which decreased transparency from 80 to 65 %. Water vapor penetration did not differ between films and degradation in water was reduced from 40 to 5 % with MFC/NFC addition. There were no differences in contact angle and wettability, but all films showed high resistance to fat penetration. Films with MFC/NFC content between 75 and 100 % showed higher values for tensile strength (50 to 65 MPa) and Young’s modulus (6 to 10 MPa) and lower elongation at break (1 to 2 %). The experimental results indicated that films with MFC/NFC content above 50 % have potential to be used as packaging material.
This work aimed to evaluate the physical and mechanical behavior of glued laminated timber (GLT) - glulam pieces of Hevea brasiliensis treated with chromed copper arsenate (CCA), chromed copper borate (CCB) and pyrethroid in the production of GLT. The pieces were produced using three wooden laminae with dimensions of 60 x 20 x 1200 mm, (width x thickness x length), joined with epoxy adhesive under 1.0 MPa pressure for 24h at room temperature. The rubberwood had an apparent density of 0.624 g cm-3, a value close to that of Eucalyptus grandis wood, a species traditionally used in the manufacture of GLT. Regarding the GLT parts, it was observed that the preservative treatment with CCA and CCB influenced negatively the values of the mechanical properties. For resistance modulus (MOR), a reduction of 75.44 MPa to 62.36 and 58.57 MPa was found for the parts untreated and treated with CCA and CCB, respectively. There was no statistical difference for surface treatment with pyrethroid. The photomicrographs of the glue line showed that the reduction in these values was mainly due to the penetration of preservative solutions into the wood structure (cell lumens and vessels or pores), impairing the anchoring of the adhesive.
The glued laminated timber (glulam) is a composite material obtained from the bonding of wood laminae arranged with parallel fibers put together. The purpose of this paper was to evaluate the influence of the number of laminae on the mechanical behavior of glulam of Toona ciliata produced with vegetable-based polyurethane adhesive. The glulam beams were produced with lamellae in the dimensions of 6.0 x 1.5 x 120.0 cm, with 3 beams being made per treatment, which were structurally composed by 5, 7 and 9 laminae. The polyurethane adhesive based on castor oil was used, applying a grammage of 350 g m-². For the technological characterization of the wood the moisture in the dry base, bulk density, chemical characterization, compressive strength parallel to the fibers, shear and modulus of elasticity (MOE) and rupture (MOR) in the static bending test. While the properties of modulus of elasticity (MOE), modulus of rupture (MOR), shear strength, delamination and visualization of the glue line through photomicrographs of the laminated wood samples were determined for glulam beams. The results showed that the beams with 5 laminae presented values similar to solid wood. The increase in the number of laminae provided lower values for stiffness and strength of the beams. The photomicrographs showed the quality of the bonding and the satisfactory values for shear strength and delamination, indicating the viability of the species under study for situations with high moisture content.
The aim of this study was to evaluate the method of neuroevolution of augmenting topologies (NEAT) to adjust the weights and the topology of artificial neural networks (ANNs) in the estimation of tree height in a clonal population of eucalyptus, and compare with estimates obtained by a hypsometric regression model. To estimate the total tree height (Ht), the RNAs and the regression model, we used as variables a diameter of 1.3 m height (dbh) and the dominant height (Hd). The RNAs were adjusted and applied to the computer system NeuroForest, varying the size of the initial population (the genetic algorithm parameter) and the density of initial connections. Estimates of the total height of the trees obtained with the use of RNA and the regression model were evaluated based on the correlation coefficient, the percentage of errors scatter plot, the percentage frequency histogram of percentage errors, and the root mean square error (root mean square error - RMSE). Various settings which resulted in superior statistics to the hypsometric regression model were found. Connections had the highest correlation and the lowest RMSE% with a population size value of 300 and an initial density of 0.1 RNA. The NEAT methodology proved effective in estimating the height of trees in clonal population of eucalyptus.