David Medveď

Mr. David Medveď


Research Focus & Metrics

Academic Career Length

7Years (2020-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
6 July 2022 in International Journal of Applied Ceramic Technology
Verified
Journal Article
Closed access
DMDavid Medveď
David Medveď
MIMichal Ivor
Michal Ivor
AKAlexandra Kovalčíková
Alexandra Kovalčíková
EMErika Múdra
Erika Múdra
TCTamás Csanádi
Tamás Csanádi
JDJán Dusza
Ján Dusza

20 April 2021 in Molecules
Verified
Journal Article
Open access
PDF file
PMParchovianský Milan
Parchovianský Milan
IPIvana Parchovianská
Ivana Parchovianská
PŠPeter Švančárek
Peter Švančárek
DMDavid Medveď
David Medveď
MLMateus Lenz Leite
Mateus Lenz Leite
Dušan GalusekDušan Galusek
Dušan Galusek
This work is aimed at the development and investigation of the oxidation behavior of ferritic stainless-steel grade AISI 441 and polymer-derived ceramic (PDC) protective coatings. Double-layer coatings of a PDC bond coat below a PDC top coat with glass and ceramic passive fillers’ oxidative resistance were studied at temperatures up to 1000 °C in a flow-through atmosphere of synthetic air and in air saturated with water vapor. Investigation of the oxide products formed at the surface of the samples in synthetic air and water vapor atmospheres, at different temperatures (900, 950, 1000 °C) and exposure times (24, 96 h) was carried out on both uncoated steel and steel coated with selected coatings by scanning electron microscopy (SEM) and X-Ray diffraction (XRD). The Fe, Cr2O3, TiO2, and spinel (Mn,Cr)3O4 phases were identified by XRD on oxidized steel substrates in both atmospheres. In the cases of the coated samples, m- ZrO2, c- ZrO2, YAG, and crystalline phases (Ba(AlSiO4)2–hexacelsian, celsian) were identified. Scratch tests performed on both coating compositions revealed strong adhesion after pyrolysis as well as after oxidation tests in both atmospheres. After testing in the water vapor atmosphere, Cr ions diffused through the bond coat, but no delamination of the coatings was observed.

9 January 2024 in International Journal of Applied Ceramic Technology
Verified
Journal Article
Closed access
ANAnnamária Naughton‐Duszová
Annamária Naughton‐Duszová
DMDavid Medveď
David Medveď
LĎLenka Ďaková
Lenka Ďaková
AKAlexandra Kovalčíková
Alexandra Kovalčíková
PŠPeter Švec
Peter Švec
JDJán Dusza
Ján Dusza

17 July 2025 in Lubricants
Verified
Journal Article
Open access
PDF file
JAJana Andrejovská
Jana Andrejovská
DMDavid Medveď
David Medveď
MVMarek Vojtko
Marek Vojtko
RSRichard Sedlák
Richard Sedlák
PKPiotr Klimczyk
Piotr Klimczyk
Ján DuszaJán Dusza
Ján Dusza
To elucidate the key material parameters governing the tribological performance of ceramic composites under dry sliding against steel, this study presents a comprehensive comparative assessment of the microstructural characteristics, mechanical performance, and tribological behavior of two alumina–zirconia (Al2O3–ZrO2) ceramic composites, each reinforced with a 42 vol.% carbide phase: zirconium carbide (ZrC) and tungsten carbide (WC). Specifically, tungsten carbide (WC) was selected for its exceptional bulk mechanical properties, while zirconium carbide (ZrC) was chosen to contrast its potentially different interfacial reactivity against a steel counterface. ZrC and WC were selected as reinforcing phases due to their high hardness and distinct chemical and interfacial properties, which were expected to critically affect the wear and friction behavior of the composites under demanding conditions. Specimens were consolidated via spark plasma sintering (SPS). The investigation encompassed macro- and nanoscale hardness measurements (Vickers hardness HV1, HV10; nanoindentation hardness H), elastic modulus (E), fracture toughness (KIC), coefficient of friction (COF), and specific wear rate (Ws) under unlubricated reciprocating sliding against 100Cr6 steel at normal loads of 10 N and 25 N. The Al2O3–ZrO2–WC composite exhibited an ultrafine-grained microstructure and markedly enhanced mechanical properties (HV10 ≈ 20.9 GPa; H ≈ 33.6 GPa; KIC ≈ 4.7 MPa·m½) relative to the coarse-grained Al2O3–ZrO2–ZrC counterpart (HV10 ≈ 16.6 GPa; H ≈ 27.0 GPa; KIC ≈ 3.2 MPa·m½). Paradoxically, the ZrC-reinforced composite demonstrated superior tribological performance, with a low and load-independent specific wear rate (Ws ≈ 1.2 × 10−9 mm3/Nm) and a stable steady-state COF of approximately 0.46. Conversely, the WC-reinforced system exhibited significantly elevated wear volumes—particularly under the 25 N regime—and a higher, more fluctuating COF. Scanning electron microscopy coupled with energy-dispersive X-ray spectroscopy (SEM–EDX) of the wear tracks revealed the formation of a continuous, iron-enriched tribofilm on the ZrC composite, derived from counterface material transfer, whereas the WC composite surface displayed only sparse tribofilm development. These findings underscore that, in steel-paired tribological applications of Al2O3–ZrO2–based composites, the efficacy of interfacial tribolayer generation can supersede intrinsic bulk mechanical attributes as the dominant factor governing wear resistance.

19 May 2023 in Ceramics International
Verified
Journal Article
Closed access
BPBeatrice Plešingerová
Beatrice Plešingerová
DMDavid Medveď
David Medveď
PVPavol Vadász
Pavol Vadász
GSGabriel Sučik
Gabriel Sučik
VPVladimír Petrov
Vladimír Petrov
Robert DzurnakRobert Dzurnak
Robert Dzurnak

17 July 2023 in Materials
Verified
Journal Article
Open access
PDF file
MTMarianna Trebuňová
Marianna Trebuňová
DKDaniel Kottfer
Daniel Kottfer
Karol KyziolKarol Kyziol
Karol Kyziol
MKMaria Kanuchova
Maria Kanuchova
DMDavid Medveď
David Medveď
MCMária Csatáryová
Mária Csatáryová
This article presents a comparative study of WC and CrC coatings deposited by the plasma-enhanced chemical vapor method using the hexacarbonyls of W and Cr as precursors. The measured thicknesses of the WC and CrC coatings are equal to ca. 1.5 µm. The WC coating consists of microcolumns with a conical end, with gaps between the microcolumns up to approximately 100 nm, and their structure is formed by nanoparticles in the shape of globules with a diameter of up to 10 nm. In the case of the CrC coating, a cauliflower structure with gaps ranging from 20 to 100 nm was achieved. The diameter of cauliflower grains is from 50 nm to 300 nm. The C content in the WC and CrC coating is 66.5 at.% and 75.5 at.%. The W content is 1.4 at.% and the Cr content in the CrC coating is 1.2 at.%. The hardness and Young’s modulus of the WC coating are equal to 9.2 ± 1.2 GPa 440.2 ± 14.2 GPa, respectively. The coefficients of friction and wear volume of the WC coating are equal to 0.7 and −1.6 × 106/+3.3 × 106 µm3, respectively. The hardness and Young’s modulus of the CrC coating are 7.5 ± 1.2 GPa and 280 ± 18.5 GPa, respectively. The coefficients of friction and wear volume of the CrC coating are 0.72 and −18.84 × 106/+0.35 × 106 µm3, respectively.
1