Hybrid processes are an efficient solution for shortening process chains and improving performance. As an example a process combination of sheet metal forming and polymer injection molding is introduced and investigated. The merging of forming and moulding processes into a single step process allows generating potential cost-savings, especially for medium to large production volumes. Based on the technological comparison between the conventional and the new process chain, the determination of the energy consumption and the detected impacts concerning the process efficiency are presented, showing that approx. 20% less energy is required due to using only one tempered tooling and reduction of handling operation.
In contrast to other cutting processes, adiabatic blanking typically features high blanking velocities (>3 m/s), which can lead to the formation of adiabatic shear bands in the blanking surface. The produced surfaces have excellent properties, such as high hardness, low roll-over, and low roughness. However, details about the qualitative and quantitative influence of significant process parameters on the quality of the blanked surface are still lacking. In the presented study, a variable tool is used for a systematic investigation of different process parameters and their influences on the blanked surface of a hardened 22MnB5 steel. Different relative clearances (1.67% to 16.67%), velocities (7 to 12.5 m/s), and impact energies (250 J to 1000 J) were studied in detail. It is demonstrated that a relative clearance of ≤6.67% and an impact velocity of ≥7 m/s lead to adiabatic shear band formation, regardless of the impact energy. Further, an initiated shear band results in the formation of an S-shaped surface. Unexpectedly, a low impact energy results in the highest geometric accuracy. The influence of the clearance, the velocity, and the impact energy on the evolution of adiabatic shear band formation is shown for the first time. The gained knowledge can enable a functionalization of the blanked surfaces in the future.
After conventional forming processes, the residual stress distribution in wires is frequently unfavorable for subsequent processes, such as bending operations. High tensile residual stresses typically occur near the wire surface and normally limit further processability of the material. Additional heat treatment operations or shot peening are often used to influence the residual stress distribution in the material after conventional manufacturing, which is time- and energy-consuming. This paper presents an approach for influencing the residual stress distribution by modifying the forming process, especially regarding die geometry. The aim is to reduce the resulting tensile stress levels near the surface. Specific forming elements are integrated into the dies to achieve this residual stress reduction. These modifications in the forming zone have a significant influence on process properties, such as plastic strain and deformation direction, but typically do not influence product geometry. This paper describes the theoretical approach and model setup, the FE simulation, and the results of the experimental tests. The characterization of the residual stress states in the specimen was carried out through X-ray diffraction using the sin2Ψ method.
Advanced high-strength steel (AHSS) is subject to a high deformation in geometry due to spring-back and high forces during forming. Therefore, dieless single-point incremental forming supported by induction heating was introduced. When a HCT980C steel part was studied, it was observed that the geometrical accuracy increased by forming using a 15 kW induction power, whereas a high deviation in profile geometry was observed by forming using a 5 kW induction power. The forming forces decreased by 66.63% compared with those resulting from forming at room temperature. At the same time, the HCT980C steel part cracked and failed to reach its designed depth when forming at room temperature. Regulating the tensile strength and hardness of the formed part and preventing their reduction was achieved by increasing the feed rate continuously as a function of the formed part’s growing depth. Moreover, the distribution of the induction heating temperature was reduced by introducing the new forming strategy. A cone wall angle of 70° was flexibly formed from a HCT980C steel sheet when the new strategy was applied.
As a result of conventional wire-forming processes, the residual stress distribution in wires is frequently unfavorable for subsequent forming processes such as bending operations. High tensile residual stresses typically occur in the near-surface region of the wires and can limit further application and processability of the semi-finished products. This paper presents an approach for tailoring the residual stress distribution by modifying the forming process, especially with regard to the die geometry and the influence of the drawing velocity as well as the wire temperature. The aim is to mitigate the near-surface tensile residual stresses induced by the drawing process. Preliminary studies have shown that modifications in the forming zone of the dies have a significant impact on the plastic strain and deformation direction, and the approach can be applied to effectively reduce the process-induced near-surface residual stress distributions without affecting the diameter of the product geometry. In this first approach, the process variant using three different drawing die geometries was established for the metastable austenitic stainless steel X5CrNi18-10 (1.4301) using slow (20 mm/s) and fast (2000 mm/s) drawing velocities. The residual stress depth distributions were determined by means of incremental hole drilling. Complementary X-ray stress analysis was carried out to analyze the phase-specific residual stresses since strain-induced martensitic transformations occurred close to the surface as a consequence of the shear deformation and the frictional loading. This paper describes the setup of the drawing tools as well as the results of the experimental tests.
In this study, the influence of thermal treatments on the properties of the martensitic stainless steel X30Cr13 (EN 10088-3: 1.4028) were investigated. These steels are characterized by a high hardness as well as corrosion resistance and can be specifically adjusted by heat treatment. In particular, the austenitizing temperature and cooling rate affect the hardness and corrosion properties of martensitic stainless steels. In order to investigate these influences, the Jominy end quench tests were performed at varying austenitizing temperatures. The aim is to determine the hardness and corrosion properties as a function of the austenitizing temperature and the cooling rate. The austenitizing temperature strongly influences the solubility of alloying elements within the austenitic lattice as well as the grain size, and thus affects both precipitation and phase transformation kinetics. In consequence, different austenitizing temperatures lead to different macroscopic material properties, like hardness and pitting corrosion potential. The heat treatment was simulated using finite element (FE) method and compared with time-temperature sequences measured at different locations of the Jominy end quench sample using thermocouples. That allows determining the cooling rate between 800 and 500 and to assign it to each location of the Jominy end quench sample. The numerical estimations were in close conformity with the experimental values. By assigning the hardness and pitting corrosion potentials to the respective cooling rates as a function of the austenitizing temperature, it is possible to determine optimum process windows for the required properties.