In the pursuit of low-impact and renewable construction materials, various by-products from agriculture, forestry, and the wood processing industry are being explored as potential bio-based infill materials for wall assemblies. This study presents an experimental assessment of the fire performance of timber wall systems composed of block units filled with different lignocellulosic materials, subjected to radiative heat exposure. These assemblies are representative of external walls in contemporary timber-framed buildings. Two configurations were examined: one with sawdust infill and the other with wood pellet infill. Both samples were exposed to radiant heat from the interior side for 60 min, simulating conditions of a fully developed compartment fire. The applied heat flux was 20 kW·m−2, delivered by a calibrated radiant panel. The results indicate that even minor design variations—particularly the choice of infill material—can significantly influence the thermal response, degradation kinetics of wood-based components, and the overall fire resistance of the wall assembly. The sawdust-filled system exhibited superior performance, achieving an estimated fire resistance rating of 60 min (60 REI). It showed reduced internal thermal degradation compared to the pellet-filled variant, which experienced greater charring depth due to internal voids between pellets, although it maintained structural integrity.
Cross-laminated timber (CLT) is increasingly used in multi-story timber construction, but its combustible nature requires reliable fire protection, particularly in layered wall assemblies with concealed cavities. This study compares two medium-scale cross-laminated timber (CLT) sandwich wall assemblies exposed to radiant heat flux of 20 kW/m2 for 90 min: an uncoated reference assembly and an assembly with PROMADUR® intumescent coating applied to the CLT surfaces. Both specimens consisted of a 90 mm three-ply CLT panel encapsulated with 12.5 mm gypsum-fiber boards fixed to a wooden stud frame forming a 40 mm installation cavity. Fire-test observations were supplemented by simultaneous thermal analysis (STA), i.e., thermogravimetry (TG)/differential thermogravimetry (DTG)/differential scanning calorimetry (DSC), of uncoated and coated CLT specimens under oxidative conditions. During the applied medium-scale radiant exposure, the unexposed-face temperatures of both assemblies remained below the insulation temperature-rise limits defined in STN EN 1363-1; however, these limits were used only as a comparative benchmark and the test does not represent a formal fire-resistance classification. The coated assembly showed improved thermal protection during the early and intermediate stages of exposure, delaying a critical thermal event near the wooden stud by approximately 35 min. However, flaming combustion of the stud occurred at about 75 min and led to degradation of the intumescent char within the cavity. In contrast, the uncoated assembly reached higher early CLT surface temperatures but showed no flaming combustion during the test. STA results supported the fire-test interpretation: the coated specimen showed a 37% reduction in peak DTG rate, a higher residual mass at the end of the test, and substantially greater mass loss in the 150–280 °C range, consistent with intumescent activation and volatile release. The results indicate that, under the tested medium-scale exposure, the intumescent coating improved early and intermediate thermal protection of the CLT surface, but did not prevent late-stage cavity flaming involving the wooden stud. Therefore, the behavior of intumescent-coated CLT in partially enclosed cavities with combustible framing should be validated under replicated, standardized and larger-scale fire exposure.
The fire response of cross-laminated timber (CLT) sandwich wall assemblies depends on interactions among the structural core, lining, cavities and secondary timber members. This study examines the thermal roles of these layers under medium-scale radiant exposure. The thermogravimetric mass change, mass-loss rate and heat-flow response were obtained for CLT, Fermacell® gypsum–fiber board and timber stud specimens by simultaneous thermal analysis. One complete, artifact-free record per material group was selected for mechanistic comparison; the data were not used to characterize material variability statistically. The degradation intervals were compared qualitatively with temperatures, visual observations and post-test damage recorded during a 90 min exposure of the wall assembly at 20 kW/m2. Fermacell® retained 77.8% of its initial mass; CLT and stud specimens retained 22.5% and 20.8%, respectively. The largest mass loss of both wood-based materials occurred at 280–430 °C, with mass-loss-rate peaks at 372.1 °C for the CLT and 359.4 °C for the stud. The lining initially delayed heat transfer. After board cracking, cavity heating was followed by the degradation and glowing of the timber stud. Layer-specific thermal analysis supports the mechanistic interpretation of the tested assembly, but it neither predicts event timing nor replaces standardized fire resistance testing or classification.