This article deals with the assessment of the hazards of dust waste generated by modern CNC (computer numerical control) technologies from the processing of resin-containing plastic composites. The change of the original material into dusty waste predicts the emergence of new hazardous characteristics such as flammability, explosiveness and adverse effects on employee health. The aim of this article is to determine the experimental measurement of dust particle size, its thermal degradation and safety characteristics. Sieve analysis showed that the representative sample contained a 93.8% weight of particles with a size of less than 0.4 mm. Three degrees of thermal degradation of industrial dust samples and heat production (exo reaction ∑ΔH = 9172.9 J/g) were determined by TG (thermogravimetry), DTA (differential thermal analysis) and DSC (differential scanning calorimetr) methods. The measurement safety characteristics such as the lower explosion limit, the maximum explosion pressure, the maximum pressure rise rate, and the calculated cubic constant confirmed that the dust is an explosive, and is determined as explosion class St1 (determined by Cubic constant).
The issue of the formation of wood dust particles in the work environment is still an actual topic in terms of its impact on employee health and the risk of fire or explosion in a woodworking operation. This article deals with the characteristics of spruce dust (Picea abies Karst. (L.)), which was taken from several types of wood technology. Experimental samples of spruce dust were taken from four types of sawing technologies, including grinding, briquetting and from the suction device container. The physical parameters of the samples taken were monitored and the particle size analysis was determined. The granulometric composition of the samples is significantly different. The sample of spruce wood dust from sawing has the most numerous fraction (250 µm), while the sample from grinding has the most numerous fraction 63–250 µm (87%).The aim of the paper was to monitor the minimum ignition temperature of the settled spruce dust layer and to look for a significant dependence of the minimum ignition temperature and ignition time on the type of spruce dust sample. A significant dependence was not confirmed. Significant moisture dependence of the samples was confirmed; the highest humidity was observed in the container, the lowest in sawing.
1 January 2013 in TRANSACTIONS of the VŠB – Technical University of Ostrava, Safety Engineering Series
This study investigated spruce wood (Picea abies Karst. L.) dust generated during sanding in a woodworking company, focusing on its health, explosion, and fire hazards. Microscopic analyses revealed that dust particles ranged from 2.38 μm × 1.69 μm to 499.71 μm × 403.30 μm, with an average size of 73.2 μm × 37.98 μm. Smaller particles exhibited a spherical morphology, while larger ones were elongated and fibrous. Sieve analysis confirmed that particles sized 63–75 μm formed the largest fraction (46.74%), with 71% of the total dust being airborne (<100 μm), including 5% PM10 and 1% PM2.5. Explosion tests identified a lower explosion limit (LEL) of 80 g·m−3, with dust classified as highly explosive (ST 2). Smaller particles were found to significantly reduce the LEL, increasing explosion susceptibility. These findings highlight the dual risk of inhalation exposure and explosion potential. Practical safety recommendations include ensuring efficient local dust extraction, mandatory use of respiratory protection, and restricted worker movement near sanders. Furthermore, organizational measures aligned with ATEX standards—such as daily cleaning, removal of settled dust layers, use of explosion-safe industrial vacuum cleaners, and installation of automatic explosion suppression systems in extraction units—are essential.
This study investigates particle size distribution and fine dust generation from sanding six tropical wood species (Red Meranti, Iroko, Zebrano, Bubinga, Ipe, and Wenge) using sieve analysis and laser diffraction. The wood species produced different dust particles, primarily influenced by wood density. Bubinga, Zebrano, and Wenge generated the highest proportion of particles in the 125–250 μm range, while Ipe and Iroko produced more dust in the 63–125 μm fraction. Low-density Red Meranti formed the greatest share of coarse particles (10.54% over 549.5 μm), whereas high-density Ipe generated the largest proportion of respirable dust, including PM10 (8.80%), PM2.5 (2.93%), and PM1 (0.88%). Statistical analysis confirmed a significant effect of density on both coarse and fine dust fractions, with finer particles increasing consistently as density increased. Laser diffraction showed ultrafine particles down to approximately 0.7 μm in all species except Red Meranti. Microscopy confirmed elongated fibrous fragments, particularly in Wenge and Red Meranti. Overall, denser tropical hardwoods exhibited greater potential to produce hazardous fine dust during sanding, posing health risks and explosion hazards. These findings emphasize the need for effective dust extraction and high-efficiency respiratory protection and contribute to improved understanding of dust formation mechanisms in tropical wood processing.
The fire response of cross-laminated timber (CLT) sandwich wall assemblies depends on interactions among the structural core, lining, cavities and secondary timber members. This study examines the thermal roles of these layers under medium-scale radiant exposure. The thermogravimetric mass change, mass-loss rate and heat-flow response were obtained for CLT, Fermacell® gypsum–fiber board and timber stud specimens by simultaneous thermal analysis. One complete, artifact-free record per material group was selected for mechanistic comparison; the data were not used to characterize material variability statistically. The degradation intervals were compared qualitatively with temperatures, visual observations and post-test damage recorded during a 90 min exposure of the wall assembly at 20 kW/m2. Fermacell® retained 77.8% of its initial mass; CLT and stud specimens retained 22.5% and 20.8%, respectively. The largest mass loss of both wood-based materials occurred at 280–430 °C, with mass-loss-rate peaks at 372.1 °C for the CLT and 359.4 °C for the stud. The lining initially delayed heat transfer. After board cracking, cavity heating was followed by the degradation and glowing of the timber stud. Layer-specific thermal analysis supports the mechanistic interpretation of the tested assembly, but it neither predicts event timing nor replaces standardized fire resistance testing or classification.