Aim: This in vitro study aimed to evaluate the marginal and internal fit of three monolithic CAD/CAM zirconia ceramics with different Y-TZP contents, prepared with chamfer and rounded shoulder finish lines. Methods. Sixty monolithic zirconia crowns were fabricated and divided into three groups (n = 20) based on their yttria content: (1) multilayer zirconia consisting of a dentin layer of 3 mol% yttria-stabilized tetragonal zirconia polycrystal (3Y-TZP) and an incisal layer of 5 mol% partially stabilized zirconia (5Y-PSZ), (2) shade-gradient zirconia fully composed of 3Y-TZP, and (3) shade-gradient zirconia containing 4 mol% partially stabilized zirconia (4Y-PSZ). Each group was further divided into two finish line configurations (chamfer and rounded shoulder). Marginal and internal gaps were measured using the silicone replica technique under a stereomicroscope by a single operator. Data were analyzed using three-way ANOVA followed by Tukey’s post hoc test (α = 0.05). Marginal and internal gaps were assessed using the silicone replica technique under a stereomicroscope by a single operator. Statistical analysis was performed with three-way ANOVA and Tukey’s post hoc test (p < 0.05). Results: The occlusal region exhibited the largest gap values, while the axial region showed the smallest across all groups. Mean marginal and internal gaps were 33.79 µm for chamfer and 43.37 µm for rounded shoulder finish lines. Zirconia with higher Y-TZP content demonstrated significantly greater gap values than those with lower percentages (p < 0.05). Significant interactions were found among finish line design, material type, and measurement region (p < 0.05), with rounded shoulder margins showing larger gaps (p = 0.001). Conclusions: Y-TZP content significantly affects marginal and internal adaptation, with higher percentages associated with increased gap values. Both finish line types produced clinically acceptable fits, although chamfer margins provided superior adaptation.
Background: Zirconia ceramics are generally used in monolithic restorations, and their microstructural, mechanical, and optical properties continue to improve. Several factors affect the mechanical properties of these restorations; however, the combined effects of yttria content and margin design on the fracture resistance remain unclear. Methods: Sixty monolithic zirconia crowns were fabricated and assigned to six groups (n = 10) based on three different yttria contents (strength-gradient multilayer zirconia containing 3 mol% yttria tetragonal zirconia polycrystals in the dentin region and 5 mol% yttria-partially stabilized zirconia in the occlusal region: 3Y-TZP/5Y-PSZ [ZP], 3 mol% yttria tetragonal zirconia polycrystals: 3Y-TZP [HTML], and 4 mol% yttria-partially stabilized zirconia: 4Y-PSZ [STML]), and two different margin designs (chamfer and rounded shoulder). Crowns were adhesively bonded to standardized 3-dimensional-printed resin dies and subjected to thermal and mechanical aging (10,000 thermocycles at 5–55 °C, and 1.2 million mechanical cycles at 50 N, 1.6 Hz). Fracture resistance values were recorded in Newtons, and fracture types were evaluated. Data were analyzed using a two-way analysis of variance (ANOVA), and Bonferroni adjustment was used for multiple comparisons (α = 0.05). Results: A significant interaction between yttria content and margin design was found (p = 0.005). In the chamfer margin design groups, ZP (2208.5 ± 501.9 N) and HTML (2069.6 ± 463.3 N) showed significantly higher fracture resistance than STML (1444 ± 303.2 N) (p < 0.05). In the rounded shoulder margin design groups, no significant differences were observed among ZP (1662.8 ± 293.8 N), HTML (1940.9 ± 341.6 N), and STML (1795.6 ± 529.6 N) (p > 0.05). ZP and HTML showed higher fracture resistance values with the chamfer margin design, while STML showed higher fracture resistance with the rounded shoulder margin design. Conclusions: The fracture resistance of zirconia restorations is influenced by both the margin design and the yttria content. Designing the margin geometry based on the type of zirconia to be used can enhance the mechanical properties of the restorations and support clinical decision-making.
Background/Objectives: Patient-specific subperiosteal implants are increasingly used to treat severely atrophic ridges due to advances in digital planning and additive manufacturing. This study aimed to evaluate the effects of material type and implant configuration on stress distribution in subperiosteal implant systems and to compare their overall biomechanical performance using a multi-criteria decision framework. Methods: A three-dimensional model of a severely atrophic maxilla was reconstructed to simulate four clinical scenarios combining two configurations (one-piece and two-piece) and two materials (titanium and 60% carbon fiber-reinforced polyetheretherketone). Finite element analysis was conducted to assess stress distribution within the implant body, fixation screws, prosthetic framework, and surrounding bone under vertical and oblique loading conditions. Maximum and minimum principal stresses were evaluated in bone, whereas von Mises stresses were calculated for implant components. The resulting biomechanical indicators were subsequently integrated using an entropy weight–TOPSIS multi-criteria decision analysis. Results: Principal stresses in the surrounding bone showed minimal variation between titanium and 60% carbon fiber-reinforced polyetheretherketone across all configurations. Implant configuration had a more pronounced effect on implant body stress. Under oblique loading, the two-piece configuration demonstrated substantially higher implant stresses than the one-piece design, whereas under vertical loading, lower implant stresses were observed in the two-piece configuration. The multi-criteria analysis ranked the one-piece titanium model highest under oblique loading and the two-piece titanium model highest under vertical loading. Conclusions: Implant configuration and loading direction influenced biomechanical behavior more than material selection in patient-specific subperiosteal implants.
Aim: This in vitro study aimed to evaluate the marginal and internal fit of three monolithic CAD/CAM zirconia ceramics with different Y-TZP contents, prepared with chamfer and rounded shoulder finish lines. Methods. Sixty zirconia crowns were fabricated and equally divided into three material groups, each further subdivided into chamfer and rounded shoulder designs. Marginal and internal gaps were assessed using the silicone replica technique under a stereomicroscope by a single operator. Statistical analysis was performed with three-way ANOVA and Tukey’s post hoc test (p < 0.05). Results: The occlusal region exhibited the largest gap values, while the axial region showed the smallest across all groups. Mean marginal and internal gaps were 33.79 µm for chamfer and 43.37 µm for rounded shoulder finish lines. Zirconia with higher Y-TZP content demonstrated significantly greater gap values than those with lower percentages (p < 0.05). Significant interactions were found among finish line design, material type, and measurement region (P < 0.05), with rounded shoulder margins showing larger gaps (p = 0.001). Conclusions: Y-TZP content significantly affects marginal and internal adaptation, with higher percentages associated with increased gap values. Both finish line types produced clinically acceptable fits, although chamfer margins provided superior adaptation.