Inkjet printing (IJP) of polymer solar cells is ideal for small‐area off‐grid electronics with low power consumption. However, IJP is quite a complex technique compared with techniques such as spin coating or doctor blading. The IJP of polymer blends is reported based on ITIC derivatives as non‐fullerene acceptors (NFAs) using non‐halogenated solvents. The results show that fluorination of NFA is essential to form highly stable inks in o‐xylene, because ITIC has significantly insufficient solubility compared with ITIC‐4F. The importance of tetralin as a multifunctional co‐solvent for printing highly efficient PM6:ITIC‐4F blends is demonstrated, as even at very low concentrations, tetralin not only improves ink jettability and open nozzle time, but also improves drying behavior of the blend layer, resulting in blends with homogeneous micro‐ and nanoscale morphology. The resulting solar cells using inkjet‐printed polymer blends show a maximum efficiency of 10.1%. Moreover, IJP produces significant changes in the nanoscale and microscale morphology. In particular, the formation of a thin PM6 capping layer on the blend surface along with improved phase separation and crystallinity in both the donor and acceptor greatly reduces the recombination of charge carriers in thick blends, making inkjet‐printed photoactive films very promising for industrial applications.
A systematic study of the intrinsic photostability of ITIC, ITIC-Th and ITIC-4F in solution, in layers and in blends with donor polymers is done. The temperature effect blends show that the amorphous to crystalline transition promotes stability.
Thick-film organic photovoltaics (OPVs) are key for scalable manufacturing, but increasing active-layer thickness usually lowers power conversion efficiency (PCE) due to charge recombination and limited carrier extraction. We report high-efficiency thick-film OPVs fully processed in air by doctor blading using non-halogenated solvents (o-xylene with 3.5% tetralin) for two non-fullerene acceptor systems: PM6:ITIC-4F and PTQ-10:ITIC-4F. Active layers (100–500 nm) were fabricated by adjusting the coating speed while keeping the ink concentration and gap constant. Under mild drying (40 °C, 2 min), both systems exhibited significant efficiency losses at 1 sun (AM1.5G) as the thickness increased, whereas performance was largely preserved under indoor LED illumination (200 lx and 1000 lx), enabling high performance for thick films. Short thermal post-annealing (80–140 °C, 2 min) further improved PCE by reducing bimolecular recombination and enhancing nanostructure. Optimized PM6:ITIC-4F devices reached 10.2% (300 nm) under 1 sun and 14.78% at 200 lx; PTQ-10:ITIC-4F achieved 11.3% (500 nm) under 1 sun and up to 15.71% at 200 lx. Morphological and structural analysis indicates that the superior thick-film performance of PTQ-10:ITIC-4F is linked to favorable phase behavior, polymer-rich surface composition, and preferential face-on molecular orientation, promoting charge collection. These results demonstrate that low-cost PTQ-10 and non-halogenated air processing can enable industrially relevant, high-performance thick-film OPVs.