As an asphalt modifier, waste battery powder (WBP) has been proven to be possible. This paper studies the modification effect of WBP on asphalt. The Flight Test Instrumentation Requirements (FITR) of WBP, Dynamic Shear Rheology (DSR) test, and Full Section Fracture Energy Test (FSFET) of asphalt are carried out. The high-temperature rheological properties and low-temperature properties of WBP modified asphalt are analyzed. The high-temperature stability, low-temperature crack resistance and water stability of WBP modified asphalt mixture are tested. The research results show that the modification of asphalt by WBP is essentially physical modification but the mixing of WBP has a certain enhancement effect on the bond energy of the methylene group, which is helpful to improve the technical performance of modified asphalt. The proportion of elastic components in asphalt can be significantly increased by adding WBP, thus enhancing the deformation resistance of asphalt under high-temperature conditions. The dynamic shear modulus of 10% waste battery powder is about 1.5–2.0 times that of 0% waste battery powder. The mixing of WBP reduces the proportion of viscous components in asphalt which is unfavorable to the crack resistance under low temperatures. The greater the amount of WBP, the smaller the fracture energy density, the content of WBP is 6% and 10%, the fracture energy density is about 60–80% and 40–60% of the original asphalt, and the low temperature cracking resistance of asphalt decreases. The modification effect of WBP on asphalt is much lower than that of SBS.
Colored pavements are widely applied to improve road aesthetics and driving safety. Nevertheless, conventional colored pavement technologies suffer from limitations in cost, environmental performance, durability, and skid resistance, and cannot satisfy the demand for bright color and high skid resistance of mountainous roads. This study develops a relatively eco-friendly, durable waterborne colored anti-skidding seal coat with high skid resistance. The optimal pigment dosage of the binder was determined based on color characteristics, tensile strength, and elongation at break. The type and particle size of colored fine aggregates were selected by evaluating particle roundness, interfacial adhesion, skid resistance, and abrasion performance. The binder spreading rate and aggregate spreading rate were further optimized according to adhesion strength, and the skid resistance and water permeability of the seal coat were verified. The results show that the binder with 5% pigment dosage achieves the closest color to the standard value with minimum color difference, and maintains well-preserved mechanical properties. Colored ceramic particles with high roundness and adhesion are the preferred aggregate. The mixed aggregate combining 1 mm and 2 mm particles at a ratio of 3:2 balances skid resistance and abrasion resistance. The optimal binder spreading rate is 1.2 kg/m2, corresponding to the best adhesion and skid resistance. The prepared waterborne colored anti-skidding seal coat presents excellent skid resistance and waterproof performance, favorable water resistance, and certain oil contamination resistance. Short-term gasoline contamination will reduce skid resistance, while its color shows only minor drift under long-term petroleum contaminant erosion.