In this paper, the local structure of silicon-containing diamond-like carbon (Si-DLC) films is discussed based on the measurement of C K-edge and Si K-edge near-edge x-ray absorption fine structure (NEXAFS) spectra using the synchrotron radiation of 11 types of Si-DLC film fabricated with various synthesis methods and having different elemental compositions. In the C K-edge NEXAFS spectra of the Si-DLC films, the σ* band shrunk and shifted to the lower-energy side, and the π* peak broadened with an increase in the Si content in the Si-DLC films. However, there were no significant changes observed in the Si K-edge NEXAFS spectra with an increase in the Si content. These results indicate that Si–Si bonding is not formed with precedence in Si-DLC film.
12 April 2004 in Journal of Vacuum Science & Technology A
Chromium oxynitride (Cr-N-O) thin films have been successfully prepared by using pulsed laser deposition (PLD). The oxygen content in the thin films (x) was controlled by changing experimental conditions. The Cr-N-O thin films with x = 30at. %, which had NaCl (B1) structure at room temperature (RT), maintained B1 phase even at T= 800°C. Moreover, Vickers hardness of such thin films was clarified to be approximately 3000 in the T ranging from RT to 800°C.
The effect of soft X-ray irradiation on hydrogenated silicon-containing diamond-like carbon (Si-DLC) films intended for outer space applications was investigated by using synchrotron radiation (SR). We found that the reduction in film thickness was about 60 nm after 1600 mA·h SR exposure, whereas there was little change in their elemental composition. The reduction in volume was attributable to photoetching caused by SR, unlike the desorption of hydrogen in the case of exposure of hydrogenated DLC (H-DLC) film to soft X-rays. The ratio of the sp2 hybridization carbon and sp3 hybridization carbon in the hydrogenated Si-DLC films, sp2/(sp2 + sp3) ratio, increased rapidly from ~0.2 to ~0.5 for SR doses of less than 20 mA·h. SR exposure significantly changed the local structure of carbon atoms near the surface of the hydrogenated Si-DLC film. The rate of volume reduction in the irradiated hydrogenated Si-DLC film was 80 times less than that of the H-DLC film. Doping DLC film with Si thus suppresses the volume reduction caused by exposure to soft X-rays.