This study investigated the structural properties and catalytic performance of cobalt-based hybrid bifunctional catalysts incorporating mesoporous ZSM-23 zeolites for Fischer–Tropsch (FT) synthesis. The zeolite was pretreated with 0.1–0.5 M NaOH solutions to introduce mesoporosity, and the resulting catalysts were prepared by mixing the zeolite with a Co–Al/SiO2 FT catalyst and a boehmite binder. The porous structure, surface acidity, phase composition, and reducibility of the zeolite and catalyst samples were characterized by N2 adsorption–desorption, IR spectroscopy, X-ray diffraction (XRD), and hydrogen temperature-programmed reduction (H2-TPR). Alkaline treatment increased mesopore volume and Lewis acid site concentration while decreasing microporosity and Brønsted acid site concentration. Catalytic performance was evaluated in a fixed-bed reactor at 250°C, 2.0 MPa, and a gas hourly space velocity (GHSV) of 1000 h–1. The catalyst containing ZSM-23 treated with 0.25 M NaOH achieved the highest yield of C5–C18iso-alkanes (47.6 wt %). These findings demonstrate that the selectivity of hybrid FT catalysts toward valuable engine-fuel components can be selectively enhanced by tuning ZSM-23 porosity.
The effect of palladium addition to a hybrid Co/SiO2 + HZSM-5 + Al2O3 catalyst on the combined Fischer–Tropsch (FT) synthesis and hydrocarbon hydroconversion process was studied. Catalysts with a Pd content of 0.075–0.3 wt.% were characterized by a complex of physicochemical methods, including synchrotron radiation X-ray diffraction (SR-XRD), temperature-programmed reduction with hydrogen (H2-TPR), temperature-programmed desorption of hydrogen with oxygen titration (H2-TPD/O2 titration), IR spectroscopy of adsorbed pyridine, and STEM-EDX analysis. It was found that the addition of palladium decreases the cobalt oxide reduction temperature due to interphase hydrogen transfer. Tests in hydrocarbon synthesis at 240–250 °C, a pressure of 2 MPa, and an H2/CO ratio of 2 showed that the sample with 0.15% Pd exhibits the highest selectivity for C5+ hydrocarbons (66.8% at 240 °C) and stability for 150 h. Analysis of the synthesis products revealed a fivefold decrease in the proportion of alkenes and an increase in isoalkanes with increasing Pd concentration. This effect enables the in situ hydroprocessing of primary FT products in a single reactor. The results demonstrate that the targeted introduction of palladium into the hybrid system is an effective strategy for regulating its functionality, allowing for the one-stage production of high-quality fuels with a controlled hydrocarbon composition from syngas.
Thermal pyrolysis of polyethylene (PE) under pressure and hydroisomerization over Pt/SAPO-11 are known separately; this work examines their integration. PE was pyrolyzed at 400–550 °C and constant pressures of 0.1–2.0 MPa, and the 140–280 °C fraction (pyrolysis kerosene) was hydroisomerized over 0.5 wt% Pt/SAPO-11. The yield of the 140–280 °C fraction decreases with temperature and increases with pressure, reaching 45.3 wt% at 400 °C and 1.0 MPa (27.4 wt% at 0.1 MPa); a control run under these conditions gave a directly measured gas yield of 13.2 wt% and a mass balance closure of 99.3%. The pyrolysis kerosene contains 47.6 wt% alkenes and 20.0 wt% cycloalkanes. Hydroisomerization at 6 MPa and a liquid hourly space velocity of 3 h−1 gives 91.1–93.4 wt% of the kerosene fraction (>140 °C) at 290–300 °C, with near-complete alkene hydrogenation; at 330 °C, the freezing point falls below −90 °C (pyrolysis kerosene: −13 °C), but hydrocracking reduces the yield to 72.4 wt%. The kerosene fraction obtained at the selected temperature of 300 °C (57.2% isoalkanes, 25.1% cycloalkanes, 0.1% aromatics) meets all measured GOST 10227-86 requirements for Russian RT jet fuel except density. The overall kerosene yield is 41.3 wt% of PE (40.0–40.4 wt% within the 140–280 °C boundaries). A preliminary estimate shows that the heat and hydrogen demand of the process corresponds to 68–97% of the energy of the pyrolysis gases.