In order to improve the performance of the investment casting shell, ceramic and nylon fiber was added to the silica sol slurry to study the effect of ceramic and nylon fiber on the liquidity of the silica sol slurry and the bending strength of the investment casting shell. Meanwhile, the fracture surface of shell sample was observed by SEM. The experiment results indicate that the movement viscosity of slurry increases with ceramic and nylon fiber content, increasing from 0 to 0.75 wt.%. The movement viscosity of ceramic fiber composite slurry is higher than nylon fiber composite slurry. The wet and high strength of shell firstly increases then decreases, with an increase of ceramic and nylon fiber content. When the ceramic and nylon fibers’ contents are 0.6 wt.%, the maximum wet strengths are 3.56 MPa and 3.84 Mpa respectively, increasing by approximately 38% and 43%. Moreover, the high strength of shell achieves its highest value, 5.08 Mpa, when the ceramic fiber content is 0.6 wt.%; however, when the nylon fiber content was more than 0.3%, the high strength of the nylon fiber reinforced shell was decreased sharply. Therefore, an addition of ceramic and nylon fiber to silica sol slurry distinctly influences the wet and high strength of investment casting shell.
The effect of ultrasonic temperature on density, microstructure and mechanical properties of vacuum counter-pressure casting ZL114A alloy during solidification was investigated by optical microscopy (OM), scanning electron microscope (SEM) and a tensile test. The results show that compared with the traditional vacuum counter-pressure casting aluminum alloy, the primary phase and eutectic silicon of the alloy with ultrasonic treatment has been greatly refined due to the dendrites broken by ultrasonic vibration. However, the refining effect of ultrasonic treatment on vacuum counter-pressure casting aluminum alloy will be significantly affected by ultrasonic temperature. When the ultrasonic temperature increases from 680 °C to 720 °C, the primary phase is gradually refined, and the morphology of eutectic silicon also changes from coarse needle-like flakes to fine short rods. With a further increase in the ultrasonic temperature, the microstructure will coarse again. The tensile strength and elongation of vacuum counter-pressure casting ZL114A alloy increases first and then decreases with the increase of ultrasonic temperature. The optimal mechanical properties were achieved with tensile strength of 327 MPa and the elongation of 5.57% at ultrasonic temperature of 720 °C, which is 6.3% and 8.2%, respectively, higher than that of alloy without ultrasonic treatment.
Understanding the distinct roles of representative alloying elements, including rare-earth (RE) solutes such as Gd and Y and non-rare-earth (non-RE) solutes such as Al and Zn, in regulating microstructural evolution and mechanical response is essential for developing high-strength Mg sheets. In this study, Gd and Y are typical RE solutes, whereas Al and Zn are common non-RE alloying elements, and were individually added to pure Mg at an identical concentration of 0.3 at.% to enable a controlled comparison of their effects on microstructural evolution and mechanical response during hot rolling and subsequent annealing. The effects of alloying elements on hot-rolling behavior were first investigated. Mg-Al and Mg-Zn exhibited improved hot rollability, whereas Mg-Gd and Mg-Y showed higher edge-cracking susceptibility after 90% hot rolling. The hot-rolled (HR) Mg-Gd and Mg-Y sheets achieved yield strength (YS) values of 235.5 and 226.4 MPa, respectively, exceeding those of Mg-Al (170.0 MPa) and Mg-Zn (162.8 MPa). Combined microstructural characterizations and DFT calculations revealed that RE solutes strongly segregated at grain boundaries, inducing solute drag, suppressing dynamic recrystallization (DRX), and promoting dislocation accumulation. During subsequent annealing, the grain size increased by only ~1.5 times in Mg-Gd/Mg-Y, whereas increases of 2.6–2.96 times were observed in pure Mg and Mg-Al/Mg-Zn alloys. The RE-containing alloys retained a UTS of ~190 MPa and elongations above 12% after annealing at 500 °C for 240 min. The identical atomic fraction design (0.3 at.%) enabled a direct comparison of the element-specific effects of different alloying elements, providing insights into alloy design and thermomechanical processing strategies for high-performance Mg sheets.