The optimized design of multilayer-coated blazed gratings (MLBG) for high-flux tender X-ray monochromators was systematically studied by numerical simulations. The resulting correlation between the multilayer d-spacing and grating blaze angle significantly deviated from the one predicted by conventional equations. Three high line density gratings with different blaze angles were fabricated and coated by the same Cr/C multilayer. The MLBG with an optimal blaze angle of 1.0° showed a record efficiency reaching 60% at 3.1 keV and 4.1 keV. The measured efficiencies of all three gratings were consistent with calculated results proving the validity of the numerical simulation and indicating a more rigorous way to design the optimal MLBG structure.
Pd/Y multilayer mirrors operating in the soft X-ray region are characterized by a high theoretical reflectance, reaching 65% at normal incidence in the 8-12 nm wavelength range. However, a severe intermixing of neighboring Pd and Y layers results in an almost total disappearance of the interfaces inside the multilayer structures fabricated by direct current magnetron sputtering and thus a dramatic reflectivity decrease. Based on grazing incidence X-ray reflectometry and X-ray photoelectron spectroscopy, we demonstrate that the stability of the interfaces in Pd/Y multilayer structures can be essentially improved by adding a small amount of nitrogen (4-8%) to the working gas (Ar). High resolution transmission electron microscopy shows that the interlayer width is only 0.9 nm and 0.6 nm for Y(N)-on-Pd(N) and Pd(N)-on-Y(N) interfaces, respectively. A well-defined crystalline texture of YN (200) is observed on the electron diffraction pattern. As a result, the measured reflectance of the Pd(N)/Y(N) multilayer achieves 30% at λ = 9.3 nm. The peak reflectivity value is limited by the remaining interlayers and the formation of the YN compound inside the yttrium layers, resulting in an increased absorption.
Ru/B4C multilayer mirrors are used for hard X-ray monochromators with moderate spectral resolution and high integral flux. To overcome the problem of large compressive stress inherent in Ru/B4C multilayers, a reactive sputtering technique using a mixture working gas of argon and nitrogen with different partial pressures was tested, and the fabricated multilayers had a period of 3 nm. The intrinsic stress was essentially reduced after nitridation and relaxed to zero value at approximately 15% partial pressure of nitrogen in the working gas. Interface roughness was slightly increased which can be caused by the polycrystalline structure inside the nitridated samples. More importantly, the nitridated multilayers showed an enhanced reflectance (67% at 8.04 keV photon energy) as compared with the one fabricated with pure Ar (54%). The structure analysis with transmission electron microscopy and X-ray photoelectron spectroscopy demonstrated that nitrogen incorporated into a multilayer structure was mostly located in the B4C layers forming BN compounds, which suppressed the diffusion of boron, stabilized the interfaces and enhanced the reflectance.
B4C/Pd multilayers with small d-spacing can easily degrade in the air, and the exact degradation process is not clear. In this work, we studied the chemical modification of B4C films and B4C/Pd double layers stored in four different environments: a dry nitrogen environment, the atmosphere, a dry oxygen-rich environment, and a wet nitrogen environment. The XANES spectra of the B4C/Pd layers placed in a dry oxygen-rich environment showed the most significant decrease in the σ* states of the B–C bonds and an increase in the π* states of the B–O bonds compared with the other samples. X-ray photoelectron spectroscopy (XPS) measurements of the samples placed in a dry oxygen-rich environment showed more intensive B-O binding signals in the B4C/Pd layers than in the single B4C film. The results of the Fourier-transform infrared spectroscopy (FTIR) showed a similar decrease in the B–C bonds and an increase in the B–O bonds in the B4C/Pd layers in contrast to the single B4C film placed in a dry oxygen-rich environment. We concluded that the combination of palladium catalysis and the high content of oxygen in the environment promoted the oxidization of boron, deteriorated the B4C composition.
Chemical–mechanical polishing (CMP) is widely adopted as a key bridge between fine rotation grinding and ion beam figuring in super-smooth monocrystalline silicon mirror manufacturing. However, controlling mid- to short-spatial-period errors during CMP is a challenge owing to the complex chemical–mechanical material removal process during surface morphology formation. In this study, the nature of chemical and mechanical material removal during CMP is theoretically studied based on a three-system elastic–plastic model and wet chemical etching behavior. The effect of the applied load, material properties, abrasive size distribution, and chemical reaction rate on the polishing surface morphology is evaluated. A microscale material removal model is established to numerically predict the silicon surface morphology and to explain the surface roughness evolution and the source of nanoscale intrinsic polishing scratches. The simulated surface morphology is consistent with the experimental results obtained by using the same polishing parameters tested by employing profilometry and atomic force microscopy. The PSD curve for both simulated surface and experimental results by profilometry and atomic force microscopy follows linear relation with double-logarithmic coordinates. This model can be used to adjust the polishing parameters for surface quality optimization, which facilitates CMP manufacturing.