With the background of the fossil fuel energy crisis, the development of self-healing and recyclable polymer materials has become a research hotspot. In this work, a kind of cross-linking agent with pendent furan groups was first prepared and then used to produce the Polyurethane elastomer based on Diels–Alder chemistry (EPU–DA). In addition, in order to further enhance the mechanical properties of the elastomer, cellulose nanofibers (CNFs) were added into the Polyurethane system to prepare a series of composites with various contents of CNF (wt% = 0.1~0.7). Herein, the FTIR and DSC were used to confirm structure and thermal reversible character. The tensile test also indicated that the addition of CNF increased the mechanical properties compared to the pure Polyurethane elastomer. Due to their reversible DA covalent bonds, the elastomer and composites were recycled under high-temperature conditions, which extends Polyurethane elastomers’ practical applications. Moreover, damaged coating can also be repaired, endowing this Polyurethane material with good potential for application in the field of metal protection.
In the present work, different aging treatments were performed to investigate the pre-aging effect on the formation of Ω phase and mechanical properties in Al-Cu-Mg-Ag alloy. The results showed that pre-strain could inhibit the formation of Ω phases, which was detrimental to the alloy strength. Due to the introduction of pre-aging treatment before pre-strain, the adverse effect of pre-strain on the precipitation of the Ω phase was reduced, and the alloy strength was increased by at least 15 MPa. Besides this, increasing the pre-aging temperature promoted the precipitation of Ω phases, inhibited the formation of θ′ phases, and improved the alloy strength. This was because the higher pre-aging temperature promoted more pre-precipitated Ω phases in the pre-aging process, and most of the pre-precipitated Ω phases could be retained and grew in the subsequent aging process. As a result, the tensile strength of the alloy increased from 523 MPa to 540 MPa. In addition, pre-aging with a higher temperature consumed more solute atoms, leading to less residual solute atoms in the matrix. Thus, the adverse effects of pre-strain, which inhibit the formation of clusters by the segregation of solute atoms, were reduced.