In this article, the results of research on a NiTi alloy with a high nickel content (51.7 at.%), produced using the additive technology SLM method and subjected to isothermal ageing after solution annealing, are presented. The study involved the determination of the sequence of phase transformations occurring using differential scanning calorimetry (DSC) and the determination of the temperature range of these transformations. In parallel, the phase composition was determined using the XRD method; the hardness and the Young’s modulus were also determined. The analysis of the DSC results obtained indicates the following characteristic features of the NiTi alloy, which change with ageing time: (1) During cooling (from +150 °C to −50 °C), the type of transformation changes from a one-step transformation after solution annealing to a two-step transformation after the ageing process over 1, 20, and 100 h at 500 °C; (2) during heating (from −50 °C to +150 °C) for all the samples, regardless of the ageing time, only a one-step transformation from martensite M(B19′) to austenite A(B2) is observed; (3) the temperature at which the transformation starts increases with the ageing time; (4) the width of the total temperature range of the transformation M(B19′) → A(B2) during heating changes from large (ΔT = 49.7 °C), after solution annealing, to narrow (ΔT = 19.3 °C and ΔT = 17.9 °C after 20 h and 100 h of ageing); and, most importantly, (5) a comparison with the literature data shows that, irrespective of the composition of the NiTi alloy and the manufacturing technology of the alloy samples (regardless of whether this was traditional or additive technology), a sufficiently long ageing process period leads to the occurrence of the martensite → austenite transformation in the same temperature range.
16 June 2016 in Journal of Thermal Analysis and Calorimetry
The main goal of this study was to analyze the application possibilities of modulated temperature thermomechanical analysis (MT TMA) for the evaluation of thermomechanical interactions in substrate/PVD coating systems on the example of examination of influence of changes in thickness of a coating on internal stress evolution in these systems. As an indicator of the stress state in the coating at a given measurement temperature, the changes in a value of the equivalent thermal expansion coefficient of the system αAC, which is calculated based on registered changes in temperature and elongation of the sample, were assumed. Independently, numerical simulations of the residual thermal stresses were carried out using finite element method. The objects of research were systems composed of substrates of HS6-5-2 steel and a single layer of chromium nitride CrN with thickness 2, 4, 8 and 10 µm, deposited on the substrate by cathodic arc evaporation method. In order to determine the effect of the CrN coating thickness on evolution of thermomechanical interactions in the system, the samples were annealed according to the assumed curve comprising nine-step isothermal annealing in the range of 150–500 °C. Obtained results have shown that MT TMA is useful to study the thermomechanical interactions in substrate/PVD coating systems. In particularly, obtained values of αAC, calculated on the basis of measured elongation changes for substrate/PVD coating systems, are lower than for the substrate without coatings, and they increase with the thickness of the deposited coating. This means that there is a decrease in compressive stresses in the coatings with increasing coating thickness. It was also found that with increasing temperature there is a local maximum value of αAC, which indicates the temperature of deposition of the coating. This is a key parameter from a technological point of view of the PVD processes.
One of the key components of the designing procedure of a structure of hard anti-wear coatings deposited via Physical Vapour Deposition (PVD) is the analysis of the stress and strain distributions in the substrate/coating systems, initiated during the deposition process and by external mechanical loads. Knowledge of residual stress development is crucial due to their significant influence on the mechanical and tribological properties of such layer systems. The main goal of the work is to find the optimal functionally graded material (FGM) coating’s structure, composed of three functional layers: (1) adhesive layer, providing high adhesion of the coating to the substrate, (2) gradient load support and crack deflection layer, improving hardness and enhancing fracture toughness, (3) wear-resistant top layer, reducing wear. In the optimisation procedure of the coating’s structure, seven decision criteria basing on the state of residual stresses and strains in the substrate/coating system were proposed. Using finite element simulations and postulated criteria, the thickness and composition gradients of the transition layer in FGM coating were determined. In order to verify the proposed optimisation procedure, Zr-C coatings with different spatial distribution of carbon concentration were produced by the Reactive Magnetron Sputtering PVD (RMS PVD) method and their anti-wear properties were assessed by scratch test and ball-on-disc tribological test.
1 June 2017 in Archives of Metallurgy and Materials
The aim of the research was to investigate the influence of nitriding of the substrate made of 42CrMo4 steel on thermal stability of the antiwear CrCN coating deposited on its surface using Cathodic Arc Evaporation method. Samples of non-nitrided and nitrided substrate/CrCN coating systems were tested with Modulated Temperature Thermodilatometry, which program included system annealing in 26 h, temperature of 290°C and argon atmosphere. Recorded during tests, changes in substrate elongation in response for changes of sample temperature, enabled qualitative determination of changes in stress states in the coatings as a result of samples annealing. Annealing of the system with nitrided substrate resulted in smaller change in residual stress in coating than for the system with non-nitrided substrate, which can indicate its better thermal stability. Values of residual stresses in coatings calculated by sin2ψ method before and after annealing on the basis of tests performed using X-Ray diffraction, agree with results of dilatometric tests.
The main problem with using modified allotrophic forms of carbon with nanodiamond particles in the production of food packaging is establishing the boundary between safety, as it affects the human body, and the adequate and effective action of the substances. One vital area of concern is the transmission of pathogens in food into the body. The aim of this study was to evaluate the cytotoxicity and bacteriostatic biological activity of two different modifications of diamond nanoparticles: pure detonation nanodiamond particles (DND) obtained by Danienko and plasma-chemically modified detonation nanodiamond particles obtained by the microwave plasma activated chemical vapor deposition method in a rotary chamber (MDP1) An indirect method was used to evaluate the cytotoxicity effect in accordance with ISO 10993–5. The viability of the L929 fibroblast cell line used as a control was 98.5%, for DND 95.14%, and the lowest level of viability for MDP1 was 88.63%. Escherichia coli and Staphylococcus aureus bacteria were used in bacteriostatic tests and the degree of cytotoxicity of the tested materials was classified as low. The in vitro cytotoxicity results indicate no toxic effect on L929 cells nor any effect on any of the samples tested against the bacterial strains us
The research presented in this article concerns Zr–C coatings which were deposited on 304L steel by reactive magnetron sputtering from the Zr target in an Ar–C2H2 atmosphere at various acetylene flow rates, resulting in various atomic carbon concentrations in the coating. The article describes research covering the change in the antibacterial and anticorrosive properties of these coatings due to the change in their chemical and phase composition. The concentration of C in the coatings varied from 21 to 79 at.%. The coating morphology and the elemental distribution in individual coatings were characterized using field emission scanning electron microscopy with an energy-dispersive X-ray analytical system. X-ray diffraction and Raman spectroscopy were used to analyze their microstructure and phase composition. Parallel changes in the mechanical properties of the coatings were analyzed. Based on the obtained results, it was concluded that the wide possibility of shaping the mechanical properties of Zr–C coatings in combination with relatively good antibacterial properties after exceeding 50 at.% of carbon concentration in coatings and high protective potential of these coatings make them a good candidate for medical applications. In particular, corrosion tests showed the high anti-pitting potential of Zr–C coatings in the environment of artificial saliva.