The fatigue behavior of pearlitic steels in wheel-rails is correlated to the microstructure. However, existing models do barely take this correlation into account. In this work, we propose a hierarchical meshing to describe the microstructure of pearlitic steels. The mesh includes grain and block/colony boundaries, lamellae orientations, and orientation perpendicular to lamellae. We use the Voronoi Tessellation method to generate elements with the specific area fraction distribution for pearlite colony areas. The colony and block information is obtained from SEM and EBSD measurements of R260 steel to construct the mesh that represents the microstructure. Finally, we obtained the deformed microstructure via simple geometrical shearing. This meshing method is the first step for modeling fatigue crack growth anisotropy due to plastic deformation.
Fatigue-induced crack initiation and propagation are a major concern in pearlitic railway rails and wheels. Rails and wheels undergo significant plastic deformation on their near-surface layers during service, leading to the initiation and propagation of cracks within the deformed region. Existing models typically use finite element models (FEMs) to describe these kinds of fatigue phenomena. However, they fail to establish a strong connection between the microstructure of the undeformed and the deformed materials and their corresponding fatigue properties. Therefore, a model based on the soft-contact discrete element method (DEM) was developed that considers microstructural details such as prior austenite grains (PAGs), pearlite blocks, pearlite colonies, and lamellar orientation of the ferrite–cementite structure of the pearlite. The Voronoi Tessellation method was used to generate a hierarchical mesh to represent these microstructural details, considering the distribution of microstructural details. Crack propagation is simulated by applying damage laws on the microstructural interface level that degrade the stiffness of the fibers connecting the mesh elements. The model’s crack growth predictions are compared with experimental results from the literature to validate its accuracy for different deformation degrees. The developed model can be used in the designing and material selection phase in the railway industry to help select the material with optimum microstructural features. Also, it can be used for the selection of the optimum heat treatment process considering materials resistance to the fatigue crack growth.
Severe changes in the profiles of the crossing nose are caused by large dynamic contact forces. To predict these forces as well as the profile evolution, the Whole System Model (WSM) was developed. However, it uses computationally expensive FE simulations. As a replacement, the semi-physical plasticity and wear model (SPPW) has been developed, thus majorly enhancing the overall performance of the WSM. The SPPW considers the influence of wear, plasticity, and wheel-profile-related effects. Its results have shown an overall good correlation with FE results, laboratory data for different materials, and field data from a real crossing. Due to the semi-physical nature of the model, the required computational time for the predictions was significantly reduced compared to FE simulations: minutes instead of weeks. The SPPW will be useful for time-efficient rail damage prediction, like wear and plastic deformation, and, as part of the WSM, contribute to a fast holistic track damage prognosis.
19 September 2025 in Advanced Engineering Materials
Rail and wheel steels undergo significant plastic deformation near the surface during service, contributing to wear and crack initiation. This region is exposed to a large deformation gradient, which affects the microstructure and local mechanical properties. This work models and predicts the plastic behavior of pearlitic steels based on microstructural features like phase fraction, interlamellar spacing, cementite thickness, and dislocation densities. A hypoeutectoid steel is heat‐treated to produce diverse microstructures, and the impact of proeutectoid ferrite, pearlite block size, interlamellar spacing, and cementite thickness on mechanical response is analyzed. Compression tests at room temperature and various strain rates, along with microscopy, characterize the samples. A mesoscale model is developed to describe plastic deformation at room temperature. Results show that lower austenitization temperature reduces grain and pearlite block size, while cooling rate inversely affects interlamellar spacing, cementite thickness, and proeutectoid ferrite. Tests indicate low strain rate sensitivity, with flow stress mainly controlled by cooling rate. Rapid cooling produces structures with strength over 1 GPa, while prior austenite grain size and block size have minimal effect on the strength of the pearlitic steel.
Fatigue-induced crack initiation and propagation is a major concern in pearlitic railway rails and wheels. Rails and wheels undergo significant plastic deformation on their surface-near layers during service, leading to the initiation and propagation of cracks within the deformed region. Existing models typically use finite element models (FEM) to describe these kind of fatigue phenomena. However, they fail to establish a strong connection between the microstructure of the undeformed and the deformed materials and their corresponding fatigue properties. Therefore, we developed a model based on the soft-contact Discrete Element Method (DEM) that considers microstructural details such as prior austenite grains (PAG), pearlite blocks, pearlite colonies, and lamellar orientation of the ferrite-cementite structure of the pearlite. The Voronoi Tessellation method was used to generate a hierarchical mesh to represent these microstructural details, considering the distribution of microstructural details. The crack propagation is simulated by applying damage laws on the microstructural interface level that degrades the stiffness of the fibers connecting the mesh elements. The model's crack growth predictions are compared to experimental results from the literature to validate its accuracy for different deformation degrees.
Rail and wheel steels undergo significant plastic deformation near the surface during service, producing wear on the surface with a few millimeters of a deformation gradient toward the center. However, the microstructure of the bulk also influences the mechanical properties. The microstructure is a consequence of the processing route. This study aims to characterise and describe the impact of heat treatments on the microstructure and plastic deformation behaviour of pearlitic steels. We subjected a 0.60 wt%C hypoeutectoid steel to different heat treatment processes to produce diverse microstructures. We discuss the influence of the heat treatment on the morphology and the amount of proeutectoid ferrite ([[EQUATION]]) as well as pearlite characteristics such as pearlite block size, interlamellar spacing (λ), and thickness of cementite ([[EQUATION]]). To assess the influence of the microstructural features on the mechanical response of the specimens, we conducted compression tests at room temperature and strain rates of 1 s-1 and 0.01 s-1, up to a strain of 0.7, followed by hardness measurements on the deformed samples. We characterised the microstructures using light optical microscopy (LOM) and scanning electron microscopy (SEM). The results revealed that reducing the austenitisation temperature decreases the prior austenite grain size (PAGS) and the pearlite block size. Furthermore, the cooling rate inversely affects the interlamellar spacing and the amount of [[EQUATION]]. We concluded that microstructural characteristics such as PAGS, pearlite block size, interlamellar spacing, and [[EQUATION]] content directly impact the mechanical resistance of the material. The cooling rate influences the microstructural features as well as the morphology of [[EQUATION]]. Fast cooling, results in less [[EQUATION]], shorter interlamellar spacing and thinner cementite layers, which in turn enhance the strength of the material. Furthermore, refined PAGs decrease the strength and hardness compared to coarser initial austenite microstructure due to a higher grain boundary area, a favourable site for [[EQUATION]]nucleation. The results of deformed specimens revealed that deformation grade influences interlamellar spacing as well as the hardness of the material. Increasing strain reduces the interlamellar spacing and increases the hardness. The cementite lamellae started kinking specifically those aligned in the direction of loading. No fragmentation of cementite was detected in the investigated deformed microstructures.