The efficiency of titanium dioxide (TiO2)-based film solar cells fabricated by combined spray and electroplating methods was improved by forming metal bridges in the pores between TiO2 nanoparticles. The interfaces between TiO2 nanoparticles and metal bridges formed Schottky contacts, which minimized recombination of electron-hole pairs and increased electron transfer. A maximum efficiency of 4.38% was achieved for cells plated at 50 mA and 55 °C. This efficiency is higher than that reported for solar cells with a similar structure [Saehana et al., AIP Conf. Proc. 1284, 154 (2010); 1415, 163 (2011); IJBAS/IJENS 11, 15 (2011)]. We also identified that both current and temperature influence the morphology of the metal bridges and efficiency of the solar cell.
In this paper we have grown pure Ba0.25Sr0.75TiO3 (BST) and BST doped by Ferric Oxide Fe2O3 (BFST) with doping variations of 5%, 10%, and 15% above type-p Silicon (100) substrate using the chemical solution deposition (CSD) method with spin coating technique at rotation speed of 3000 rpm, for 30 seconds. BST thin film are made with a concentration of 1 M 2-methoxyethanol and annealing temperature of 850oC for the Si (100) substrate. Characterization of the thin film is performed for the electrical properties such as the current-voltage (I-V) curve using Keithley model 2400 as well as dielectric constant, time constant, pyroelectric characteristics, and depth measurement. The results show that the thin film depth increases if the concentration of the Ferric Oxide doping increases. The I-V characterization shows that the BST and BFST thin film has photodiode properties. The dielectric constant increases with the addition of doping. The maximum dielectric constant value is obtained for 15 % doping concentration namely 83.1 for pure BST and 6.89, 11.1, 41.63 and 83.1, respectively for the Ferric Oxide doping based BST with concentration of 5%, 10%, and 15%. XRD spectra of 15% of ferric oxide doped BST thin film tetragonal phase, we carried out the lattice constant were a = b = 4.203 Å; c = 4.214 Å; c/a ratio = 1.003. Received: 01 February 2010; Revised: 04 October 2011; Accepted: 02 November 2011
The growth of Mg-doped GaN thin films by metalorganic chemical vapor deposition (MOCVD) using NH3 and Cp2Mg as a source of nitrogen and Mg, respectively, usually produces Mg–H complexes, which hinder the activation of Mg as shallow acceptor centers. Therefore, post-growth treatments are commonly required to activate these acceptor centers. The presence of Mg dopants in GaN films induces various defect-related emissions whose characteristics depend on the growth method. For this study, we prepared Mg-doped GaN thin films by plasma-assisted MOCVD. A nitrogen-plasma, instead of NH3, served as a nitrogen source to minimize the formation of Mg–H complexes, thereby eliminating the requirement for post-growth treatment. The emission characteristics were obtained by measuring the photoluminescence of the as-grown room-temperature films. Yellow, green, blue, and ultraviolet emission bands are produced by Mg-doped samples with different Mg concentrations produced by Cp2Mg flow rates of 2%, 5%, and 10% of the total flow rate. Low-Mg concentration leads to nitrogen and gallium vacancies, which results in yellow photoluminescence. At higher Mg concentration, the yellow photoluminescence is suppressed and the blue photoluminescence is enhanced because of the incorporation of vacancies by Mg atoms. The analysis of the photoluminescence spectra leads to the proposed band diagrams for Mg-doped GaN with varying Mg concentration.