Fiber glass waste (FGW) was subjected to alkali activation in an aqueous solution with different concentrations of sodium/potassium hydroxide. The activated materials were fed into a methane–oxygen flame with a temperature of around 1600 °C. X-ray diffraction analysis confirmed the formation of several hydrated compounds, which decomposed upon flame synthesis, leading to porous glass microspheres (PGMs). Pore formation was favored by using highly concentrated activating alkali solutions. The highest homogeneity and yield of PGMs corresponded to the activation with 9 M KOH aqueous solution.
The present COVID-19 emergency has dramatically increased the demand for pharmaceutical containers, especially vials. End-of-life containers, however, cannot be easily recycled in the manufacturing of new articles. This paper presents some strategies for upcycling of pharmaceutical glass into various porous ceramics. Suspensions of a fine glass powder (70 vol%) are used as a starting material. Highly uniform cellular structures may be easily prepared by vigorous mechanical stirring of partially gelified suspensions with added surfactant, followed by drying and firing at 550–650 °C. Stabilization of the cellular structures at temperatures as low as the glass transition temperature (Tg) of the used glass is facilitated by thermal decomposition of the gel phase, instead of viscous flow sintering of glass. This finding enabled the preparation of glass membranes (∼78 vol% open porosity), by direct firing of hardened suspensions, avoiding any surfactant addition and mechanical stirring. The powders obtained by crushing of hardened suspensions, even in unfired state, may be used as a low-cost sorbent for dye removal.
Both vitrified bottom ashes (VBAs) and waste glasses are forms of inorganic waste material that are widely landfilled, despite having some economic potential. Building on previous studies, we prepared glass-ceramic foams by the combination of VBA with either soda-lime glass (SLG) or borosilicate glass (BSG). Suspensions of fine powders in weakly alkaline solution underwent gelation, followed by frothing at nearly room temperature. Hardened “green” foams were sintered, with concurrent crystallization, at 850–1000 °C. All foams were highly porous (>70%), with mostly open porosity. The glass addition was fundamental in both gelation (promoting the formation of carbonate and silicate hydrated phases) and firing steps. While SLG addition enhanced the viscous flow sintering, without a significant impact on the crystallization of gehlenite, the main crystalline phase from the devitrification of VBA, BSG addition caused a reactive sintering, with remarkable changes in the phase assemblage. The glass addition generally also allowed lower sintering temperatures and yielded products with excellent crushing strength. However, only specific conditions resulted in the complete immobilization of pollutants (e.g., Cr3+ ions).
Additive manufacturing (AM) technologies enable the fabrication of objects with complex geometries in much simpler ways than conventional shaping methods. With the fabrication of recyclable filters for contaminated waters, the present work aims at exploiting such features as an opportunity to reuse glass from discarded pharmaceutical containers. Masked stereolithography-printed scaffolds were first heat-treated at relatively low temperatures (680 and 730 °C for 1 h) and then functionalized by alkali activation, with the formation of zeolite and sodium carbonate phases, which worked as additional adsorbing centers. As-sintered and activated scaffolds were characterized in terms of the efficiency of filtration and removal of methylene blue, used as a reference dye. The adsorption efficiency of activated printed glass was 81%. The 3D-printed adsorbent can be easily separated from the solution for reuse.
The present study illustrates the manufacturing method of hierarchically porous 3D scaffolds based on åkermanite as a promising bioceramic for stereolithography. The macroporosity was designed by implementing 3D models corresponding to different lattice structures (cubic, diamond, Kelvin, and Kagome). To obtain micro-scale porosity, flame synthesized glass microbeads with 10 wt% of silicone resins were utilized to fabricate green scaffolds, later converted into targeted bioceramic phase by firing at 1100 °C in air. No chemical reaction between the glass microspheres, crystallizing into åkermanite, and silica deriving from silicone oxidation was observed upon heat treatment. Silica acted as a binder between the adjacent microspheres, enhancing the creation of microporosity, as documented by XRD, and SEM coupled with EDX analysis. The formation of ‘spongy’ struts was confirmed by infiltration with Rhodamine B solution. The compressive strength of the sintered porous scaffolds was up to 0.7 MPa with the porosity of 68–84%.