Growing crack-free, epitaxial ultrawide-bandgap semiconductor films on cost-effective, large-area substrates, such as AlN on Si, poses a significant challenge due to substantial lattice and thermal expansion mismatches. We introduce an approach to mitigate tensile strain or reverse strain signs between the substrate and the AlN layer, thereby suppressing crack formation during the heteroepitaxial growth of thick III-N films. This approach introduces ductile metallic interlayers, specifically Au, to change the strain state of AlN from in-plane tensile to compressive, without initiating cracks. Furthermore, the Au interlayer is grown epitaxially as a single crystal, which prevents the transfer of tensile strain into the AlN film, as confirmed by x-ray diffraction and transmission electron microscopy. We demonstrate crack-free AlN films exceeding 1 μm in thickness. These findings hold significant promise for advancing the field of ultrawide-bandgap semiconductor materials, with potential applications in electronic, optoelectronic, sensing, and energy device applications.
Time-resolved cathodoluminescence using 30 keV ultrafast electron pulses has been used to perform direct measurements of the minority hole lifetime τh as a function of 3.7 MeV α-particle fluence in high-quality free-standing n-type GaN substrates. The lifetime damage factor K calculated from these measurements was found to monotonically decrease from 6.9 × 10−2 to 6.4 × 10−4 cm2 s−1 ion−1 with increasing α-fluence from 108 to 1012 cm−2, implying a reduction in trap cross section and/or an aggregation of α-induced traps. The small, ∼200–300 nm, hole diffusion length estimated from the minority hole lifetime for the highest α-fluence necessitates the deployment of α-voltaic device strategies and architectures that emphasize depletion and drift over diffusion for effective charge collection and optimal power conversion efficiency.
29 July 2026 in Journal of Vacuum Science & Technology A
We have grown two sets of 500-nm-thick n+-Al0.85Ga0.15N layers on AlN templates at various substrate temperatures between 700 and 875 °C by plasma-assisted molecular beam epitaxy, differing only in the detailed surface treatment prior to growth. In one set, Ga deposition and desorption (Ga D&D) on the template surface is performed at the substrate temperature used for growth prior to film deposition, while in the other set, the Ga D&D is performed at 875 °C for all the samples. These layers were doped with Si at a nominal concentration of 3 × 1019 cm−3. We observe significantly red-shifted (∼850 meV) photoluminescence for sub-bandgap optical pumping, the intensity of which increases as the growth temperature of the layer increases. We attribute this sub-bandgap emission to the presence of nanoscale compositional inhomogeneities in the layers and speculate that they contribute to the reduced Hall mobility. Reciprocal space mapping indicates that most of the AlGaN layers are under compressive strain and are pseudomorphic to the AlN template, while the samples with the highest Hall mobility and least intense sub-bandgap emission are under smaller tensile strain. We attribute the presence of tensile strain to layer growth on a Ga-rich compliant pseudosubstrate that presents for Ga D&D and growth at 700 and 750 °C, for which Ga desorption is incomplete prior to growth initiation.
21 August 2025 in IEEE Transactions on Nuclear Science
Absolute light yield and radiation damage resilience were calculated and measured in ten scintillators suitable for use in alpha-photovoltaic energy conversion devices. The scintillators were exposed to alpha fluences of 1010 - 1015 ions/cm2 to experimentally measure long-term damage to these materials. Scintillator light yield was calculated from IV curves in a calibrated InGaP photovoltaic diode. CsI:Tl had the largest initial light yield (4.8 kph/MeV) of all scintillators evaluated. An alpha fluence of 8.6 × 1014 ions/cm2 reduced the light yield by 90% in CsI:Tl. The initial system efficiency of CsI:Tl on InGaP was measured to be 0.23%. Alpha-photovoltaic energy conversion devices with this initial system efficiency comprised of 1 mCi (3.7 × 107 alphas/s) of 241Am on CsI:Tl scintillators mounted on InGaP PIN photovoltaic diodes will produce 747.9 nW of electrical power. The power output from alpha stimulated CsI:Tl is 50% better than the conventional ZnS:Ag scintillator when used with an InGaP energy converter.