We report the effect of N2O post-fabrication annealing (PFA) on the electrical stability of dual gate, active split amorphous indium gallium zinc oxide (a-IGZO) thin-film transistor (TFT). Optimized N2O PFA at 360 °C for 3 h results in threshold voltage (VTH) close to zero and an increase in the on-current almost 2 times than as-fabricated TFT. N2O annealed TFT exhibited robust VTH stability under positive bias temperature stress at 60 °C and negative bias illumination stress, exhibiting ΔVTH of 0.1 V, and –0.1 V, respectively, whereas as-fabricated TFT showed large ΔVTH of ~ 10 V and – 3 V. The X-ray photoelectron spectroscopy depth profile reveals the origin of such improvement as the increasing metal-oxide bonds and the reduction in oxygen vacancy/OH related defects.
High‐performance, coplanar amorphous In0.5Ga0.5O (a‐IGO) thin film transistor (TFT) on a polyimide (PI) substrate deposited by spray pyrolysis (SP) is reported. The SP a‐IGO film deposited at 370 °C has less than 8% nanocrystalline‐In2O3 dots and a mass density of 6.6 g cm−3. The a‐IGO TFT on PI exhibits linear mobility over 30 cm2 V−1 s−1 and a negligible shift in threshold voltage (ΔVTH = 2.3 MHz) with a low propagation delay time of ≈30 ns per stage at a supply voltage (VDD) of 15 V. The fabricated gate shift register circuit works up to the last stage without any decrement of the input voltage (15 V) with rising and falling times less than 0.8 µs. Therefore, the coplanar a‐IGO TFT by SP deposited at 370 °C is a promising candidate for low‐cost, flexible TFT backplanes of foldable electronics.
We report the dual gate (DG) amorphous Indium-Gallium-Zinc-Oxide (a-IGZO) thin-film transistor (TFT) with a top-gate (TG) drain offset ( $\text{L}_{\text {TG(Off)}}$ ) structure under dual-gate driving. The TFT shows an on/off current ratio of $\sim 10^{{7}}$ , subthreshold swing of 0.23 V/dec, and field-effect mobility ( $\mu _{\text {FE}}$ ) of 14.6 cm 2 /Vs when $\text{L}_{\text {TG{(}Off{)}}}$ is 5 $\mu \text{m}$ , which is 30% reduction compared to the conventional DG TFT with no drain offset ( $\mu _{\text {FE}}=20.9$ cm 2 /Vs). The Technology computer-aided design simulation indicates the electron concentration of $\sim 10^{{16}}$ /cm 3 at the offset region near top gate insulator/a-IGZO interface when $\text{L}_{\text {TG{(}Off{)}}}$ is 5 $\mu \text{m}$ . The fabricated TFT exhibits stable performance under positive bias temperature stress with a threshold voltage shift of +0.1 V.
We investigated the effect of Ar plasma treatment on the crystallization of indium-gallium-oxide (IGO) thin films. Ar plasma treatment accelerates the crystallization of amorphous IGO at $350~^{\circ }$ C, as confirmed by XRD analysis. The crystalline IGO TFT using Ar plasma treatment exhibited field-effect mobility ($\mu $ $_{\text {FE}}\text {)}$ of 43.2 cm2/V$\cdot $ s and subthreshold swing (SS) of 0.11 V/dec. In addition, IGO TFTs showed excellent operation stabilities under both positive bias temperature stress (PBTS) and negative bias temperature stress (NBTS) conditions. These results demonstrate that Ar plasma treatment is a promising technique for achieving high-performance IGO TFTs at low temperature, making it suitable for flexible display application.
We report highly sensitive temperature sensing circuits using low temperature polysilicon oxide (LTPO) thin-film transistors (TFTs) on a glass substrate. The sensor has the LTPO operational amplifier (Op-Amp) made of dual gate (DG) amorphous InGaZnO (a-IGZO) and low temperature poly-Si (LTPS) TFTs by blue laser annealing process. The DG a-IGZO TFTs-based sensing circuit exhibits a sensitivity of 37.9±3 mV/°C and it can be further boosted to 223.33±8 mV/°C by incorporating LTPO Op-Amp for body temperature detection (35~40 °C). The DG a-IGZO TFT exhibits robust threshold voltage stability ( $\Delta {\rm V}_{Th}$ = −0.16 V) with temperature, which is essential for the practical development of the proposed LTPO differential temperature sensor (TS) to accurately measure the human body temperature.