We present a coplanar amorphous InGaZnO (a-IGZO) synaptic thin film transistor (TFT) with counterclockwise hysteresis using an aluminum oxide (Al $_{\text{2}}$ O $_{\text{3}}\text{)}$ /SiO $_{\text{2}}$ gate insulator (GI). The excitatory postsynaptic current (EPSC), paired-pulse facilitation (PPF), short-term plasticity (STP), and long-term plasticity, which are biological synaptic characteristics, are demonstrated by positive charge trapping in the Al $_{\text{2}}$ O $_{\text{3}}$ layer. Long retention time can be possible by surface charge in the SiO $_{\text{2}}$ , a charge-blocking layer. As a result, multi-level channel conductance can be modulated with positive and negative gate pulses. These results prove synaptic a-InGaZnO TFT with Al $_{\text{2}}$ O $_{\text{3}}$ /SiO $_{\text{2}}$ stack GI for high-density neuromorphic devices.
We investigated the effect of Ar plasma treatment on the crystallization of indium-gallium-oxide (IGO) thin films. Ar plasma treatment accelerates the crystallization of amorphous IGO at $350~^{\circ }$ C, as confirmed by XRD analysis. The crystalline IGO TFT using Ar plasma treatment exhibited field-effect mobility ($\mu $ $_{\text {FE}}\text {)}$ of 43.2 cm2/V$\cdot $ s and subthreshold swing (SS) of 0.11 V/dec. In addition, IGO TFTs showed excellent operation stabilities under both positive bias temperature stress (PBTS) and negative bias temperature stress (NBTS) conditions. These results demonstrate that Ar plasma treatment is a promising technique for achieving high-performance IGO TFTs at low temperature, making it suitable for flexible display application.
The dynamic gate pulse stress effect on the electrical performance of single gate (SG) and dual gate (DG) thin-film transistors (TFTs) is reported. The stress is implemented with rising and falling pulses of 1 and $0.1 ~\mu \text{s}$ respectively with positive gate pulse (0 to +30V). The DG TFT under slow switching ( $1 ~\mu \text{s}$ ) shows stable TFT performance with a small threshold voltage shift ( $\Delta {V}_{\text{TH}}$ ) of 1.3 V than SG TFT ( $\Delta {V}_{\text{TH}}$ of 2.4 V) for 24 h stress at room temperature. Under a fast switching of $0.1 ~\mu \text{s}$ , DG TFT exhibits a 1.8 V shift, and SG TFT shows a 3.0 V shift. The recovery behavior of the transfer curves is also checked by keeping the TFTs unbiased for 24 h after applying stress, resulting in the DG TFTs showing complete recovery while SG TFTs exhibiting partial recovery. The lifetime of DG TFTs is found to be 7.5 times longer than that of SG TFTs under dynamic gate pulse stress.
18 March 2025 in IEEE Transactions on Electron Devices
In this work, we developed a high-performance, coplanar crystalline InGaSnO (C-IGTO) thin-film transistor (TFT). An amorphous indium gallium tin oxide (IGTO) film was deposited with reactive sputtering with H2 introduction, followed by an O2 post-deposition crystallization at 500 ∘C, resulting in a highly oriented crystal with smooth surface. The transfer characteristics of the C-IGTO TFT exhibit negligible temperature dependency up to 150 ∘C and endure up to 400 ∘C post-fabrication annealing in air. The gate shift register (GSR) and ring oscillator (RO) circuits made of C-IGTO TFTs exhibit outstanding performance. A 24-stage, GSR operates effectively with the TFTs of 1.3 μm channel length. These circuits maintain excellent operational stability without degradation at 100 ∘C. In addition, The RO exhibits a low propagation delay of 2.14 ns. To evaluate the applicability for high-density memory devices, we fabricated a capacitorless, two-transistor (2T0C) dynamic random access memory (DRAM) cell. This shows a long retention time over 2000 s with extremely low OFF-current (4.5 × 10-20 A/μm). The successful demonstrations of DRAM cell and integrated circuits using the C-IGTO TFTs highlight the potential for integration of memory and TFT circuits for next-generation memory and IT applications.
1 September 2026 in IEEE Transactions on Electron Devices
We report amorphous InGaZnO (a‐IGZO)/crystalline InGaO (C‐IGO)/a‐IGZO stack, thin‐film transistors (TFTs). The IGZO could not be crystallized but the IGO could be crystallized at 450°C. We fabricated dual‐gate C‐IGO TFTs with a‐IGZO layers interfaced with both the top and bottom gate insulators. Owing to the differences in optical bandgap and work function between a‐IGZO and C‐IGO, conduction band offsets is formed at the heterointerfaces, resulting in the formation of 2D electron gas (2DEG) in C‐IGO. The a‐IGZO/C‐IGO/a‐IGZO TFT demonstrates excellent electrical characteristics, exhibiting a threshold voltage (V TH ) of −0.8 V, field‐effect mobility (µ FE ) of 53.81 cm 2 V −1 s −1 , and subthreshold swing (SS) of 0.18 V/dec with excellent bias stability in dual‐sweep (DS) mode. Technology Computer Aided Design (TCAD) simulations reveal that electron transport is dominated by dual 2DEGs formed at the top and bottom heterointerfaces of the C‐IGO layer under dual‐gate operation.