Anton Muhin

Anton Muhin

Auto-generated profile, based on publicly available information

Anton Muhin

Institute of Solid State Physics Technische Universität Berlin Hardenbergstraße 36 10623 Berlin Germany

Research Focus & Metrics

Academic Career Length

14Years (2013-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
8 May 2023 in Applied Physics Letters
Verified
Journal Article
Open access
PDF file
TKTim Kolbe
Tim Kolbe
AKArne Knauer
Arne Knauer
JRJens Rass
Jens Rass
HCHyun Kyong Cho
Hyun Kyong Cho
SHSylvia Hagedorn
Sylvia Hagedorn
MWMarkus Weyers
Markus Weyers
Far-ultraviolet-C (far-UVC) light-emitting diodes (LEDs) with an emission wavelength of 234 nm with different polarization-doped AlGaN hole injection layers (HILs) are compared regarding their emission power, voltage, and leakage current. The influence of the thickness of the polarization-doped layer (PDL), an additional Mg doping of the PDL, as well as a combination of a PDL with a conventionally Mg-doped AlGaN HIL will be discussed. The different PDL thicknesses show nearly no influence on the emission power or voltage. However, the leakage current of the LEDs below the turn-on voltage decreases with an increasing thickness of the PDL. In contrast, an additional Mg doping of the PDL ([Mg] ∼ 1.5 × 1019 cm−3) results in a fivefold decrease in the emission power at an unchanged voltage and leakage current. Finally, a combination of a PDL and a conventionally Mg-doped AlGaN layer ([Mg] ∼ 1.5 × 1019 cm−3) as a HIL shows also a similar emission power and voltage compared to the single PDL, but the leakage current increases. Based on these optimizations, 234 nm LEDs were realized with a maximum external quantum efficiency of 1% at 20 mA, an emission power of 4.7 mW, and a voltage of 9.0 V at 100 mA. This shows that the polarization doping concept is well suited to realize far-UVC LEDs with improved performance compared to LEDs with a conventionally Mg-doped p-side.

17 April 2023 in Applied Physics Letters
Verified
Journal Article
Open access
PDF file
NRNicola Roccato
Nicola Roccato
Francesco PivaFrancesco Piva
Francesco Piva
Carlo De SantiCarlo De Santi
Carlo De Santi
Matteo BuffoloMatteo Buffolo
Matteo Buffolo
Manuel FregolentManuel Fregolent
Manuel Fregolent
Matteo MeneghiniMatteo Meneghini
Matteo Meneghini
The long-term stability of ultraviolet (UV)-C light-emitting diodes (LEDs) is of major importance for many applications. To improve the understanding in this field, we analyzed the degradation of AlGaN-based UVC LEDs and modeled the variation of electrical characteristics by 2D simulations based on the results of deep-level optical spectroscopy (DLOS). The increase in the forward leakage current observed during ageing was ascribed an increase in trap-assisted tunneling. The analysis of the degradation kinetics suggests the role of a defect diffusion process, possibly involving impurities coming from the p-type layers.

30 November 2020 in Applied Physics Letters
Verified
Journal Article
Closed access
PDF file
HFHumberto M. Foronda
Humberto M. Foronda
DHDaniel A. Hunter
Daniel A. Hunter
MPMike Pietsch
Mike Pietsch
LSLuca Sulmoni
Luca Sulmoni
AMAnton Muhin
Anton Muhin
MKMichael Kneissl
Michael Kneissl
In this work, the growth and conductivity of semipolar AlxGa1−xN:Si with (11-22) orientation are investigated. AlxGa1−xN:Si (x = 0.60 ± 0.03 and x = 0.80 ± 0.02) layers were grown with different SiH4 partial pressures, and the electrical properties were determined using Hall measurements at room temperature. The aluminum mole fraction was measured by wavelength dispersive x-ray spectroscopy and x-ray diffraction, and the Si-concentration was measured by wavelength dispersive x-ray spectroscopy and secondary ion mass spectroscopy. Layer resistivities as low as 0.024 Ω cm for x = 0.6 and 0.042 Ω cm for x = 0.8 were achieved. For both aluminum mole fractions, the resistivity exhibits a minimum with the increasing Si concentration, which can be explained by compensation due to the formation of cation vacancy complexes at high doping levels. The onset of self-compensation occurs at larger estimated Si concentrations for larger Al contents.

1 May 2023 in Applied Physics Letters
Verified
Journal Article
Open access
PDF file
Francesco PivaFrancesco Piva
Francesco Piva
MPM. Pilati
M. Pilati
Matteo BuffoloMatteo Buffolo
Matteo Buffolo
NRNicola Roccato
Nicola Roccato
NSN. Susilo
N. Susilo
Matteo MeneghiniMatteo Meneghini
Matteo Meneghini
The lifetime of deep-ultraviolet light-emitting diodes (LEDs) is still limited by a number of factors, which are mainly related to semiconductor defects, and still need to be clarified. This paper improves the understanding of UV LED degradation, by presenting an analysis based on combined deep-level transient spectroscopy (C-DLTS), electro-optical characterization, and simulations, carried out before and during a constant current stress test. The original results of this paper are (i) C-DLTS measurements allowed us to identify three traps, two associated with Mg-related defects, also detected in the unaged device, and one related to point defects that were generated by the ageing procedure. (ii) Based on these results and on TCAD simulations, we explain the variation in the forward I–V by the degradation of the p-contact, due to Mg passivation. (iii) On the other hand, optical degradation is ascribed to an increase in defectiveness of the active region and surrounding areas, which led to a decrease in injection efficiency, to an increase in non-radiative recombination, and to an increase in trap-assisted tunneling processes.

7 May 2013 in IEEE Photonics Technology Letters
Verified
Journal Article
Closed access
LRLuca Redaelli
Luca Redaelli
AMAnton Muhin
Anton Muhin
SESven Einfeldt
Sven Einfeldt
PWPeter Wolter
Peter Wolter
LWLeonhard Weixelbaum
Leonhard Weixelbaum
MKMichael Kneissl
Michael Kneissl
The electrical properties of different metal systems for ohmic contacts on the nitrogen-face of c-plane n-type GaN substrates are investigated. The metal contacts are compatible with the fabrication process and the packaging technology for group III-nitride laser diodes. The metal system Ti/Al/Mo/Ti/Ni/Au/Ti/Pt is determined as the best suitable, since it is ohmic already after annealing at a temperature of 450°C for 60 s. This annealing temperature is high enough to make the contact insensitive against later soldering on a heat-sink at 330°C. At the same time, the temperature is low enough that the Pd-based p-contact, previously annealed at 530°C, does not degrade. In addition, the Ti/W/Al and Pd/Ti/Al metal systems form low-resistance ohmic contacts, too, although they require a longer annealing time of several minutes or a higher temperature of 500°C.

8 December 2022 in Physica Status Solidi (a)
Verified
Journal Article
Open access
AMAnton Muhin
Anton Muhin
MGMartin Guttmann
Martin Guttmann
VMVerena Montag
Verena Montag
NSNorman Susilo
Norman Susilo
EZEviathar Ziffer
Eviathar Ziffer
MKMichael Kneissl
Michael Kneissl
The electro‐optical characteristics of deep ultraviolet light‐emitting diodes (DUV LEDs) emitting at 265 nm and grown on AlN/sapphire templates with different threading dislocation densities, i.e., high‐temperature annealed (HTA) AlN, epitaxially laterally overgrown (ELO) AlN, and HTA‐ELO AlN are analyzed. The external quantum efficiency of each individual device is separated into maximum radiative recombination efficiency, carrier injection efficiency, and light extraction efficiency. This is achieved by combining an ABC‐model‐based fit of the current‐dependent external quantum efficiency together with calibrated Monte Carlo ray‐tracing simulations. A maximum radiative recombination efficiency between 50% and 60% is estimated for DUV LEDs grown on ELO and HTA‐ELO AlN/sapphire, whereas the values for devices grown on HTA AlN/sapphire are around 45%. The extracted radiative recombination efficiency does not scale with the measured threading dislocation density (TDD), even when accounting for the inhomogeneous TDD in the AlN base layers. This discrepancy is attributed to the formation of dislocation half‐loops introduced by additional compressive strain caused by the HTA process and may result in the formation of additional nonradiative recombination centers in the AlGaN multi‐quantum well region. In addition, the carrier injection efficiency values ranging from 45% to 55% are determined for devices grown on all three templates.