Seed layer engineering in ferroelectric (FE) Hf0.5Zr0.5O2 (HZO) film has been investigated systematically in this work. Among four kinds of seed layers (ZrO2, HfO2, Al2O3, and TiO2), the HZO capacitor with TiO2 seed layer achieves preferable performance (larger Pr, smaller Ec, and nearly wakeup-free). It is considered that the suppression of interfacial defects by seed layers could be a key for wakeup-free achievement. For further understanding, with reliability characterizations and theoretical calculations, it is found that defects (oxygen vacancy $\text{V}_{\text {O}}^{+}$ ) generation at the TiN/HZO interface and their migration into inner film could be dominant reasons for the leakage and Pr degradation in cycling, while $\text{V}_{\text {O}}^{+}$ at the TiO2/TiN interface can attribute to the imprint effect. Thereby, a novel asymmetric stress field cycling (ASFC) scheme is proposed to suppress Pr fatigue by keeping defects at one-side interface rather than migrating into the inner film.
To achieve HfO 2 -based ferroelectric (FE) devices with robust reliabilities, the impacts of re-annealing on 7nm FE-Hf 0.5 Zr 0.5 O 2 (HZO) capacitors are comprehensively studied in this work. Impressively, the re-initialization phenomenon can be clearly observed by re-annealing cycled HZO capacitors. It is found that FE properties (remanent polarization (Pr), coercive electric field (E C ), polarization switching speed, wakeup/fatigue effect, and symmetry) can be obviously improved after re-annealing. With in-depth discussions, it is considered that temperature-dependent phase transition and non-switchable region repairing could be the dominant mechanisms. Our results indicate that re-annealing could effectively improve FE-HZO performance and shed light on reliability optimizations.
23 May 2024 in IEEE Transactions on Electron Devices
The impacts of Si doping in Hf $_{\text{0.7}}$ Zr $_{\text{0.3}}$ O $_{\text{2}}$ films are studied in this work. Compared with the standard Hf $_{\text{0.5}}$ Zr $_{\text{0.5}}$ O $_{\text{2}}$ (HZO) films, the samples with Si-doped Hf $_{\text{0.7}}$ Zr $_{\text{0.3}}$ O $_{\text{2}}$ film show higher relative permittivities and lower leakages. More importantly, a high breakdown electric field ( E $_{\text{BD}}$ 4.3 MV/cm) and a low coercive field ( E $_{\text{c}}$ 0.64 MV/cm) have been achieved experimentally. In this way, E $_{\text{c}}$ / E $_{\text{BD}}$ could be reduced from 32% to 15%, and this benefits the endurance property effectively. Specifically, compared with the HZO samples, better endurance and weaker fatigue ( $>$ 10 $^{\text{12}}$ cycles at 2.5 MV/cm) have been observed in Si-doped Hf $_{\text{0.7}}$ Zr $_{\text{0.3}}$ O $_{\text{2}}$ devices. The average switching time with three electrode sizes is smaller than that of the standard HZO group. Our data strongly indicate that Si doping in Hf $_{\text{0.7}}$ Zr $_{\text{0.3}}$ O $_{\text{2}}$ film is a feasible way to fabricate ferroelectric devices with better performances and robust reliabilities.
31 July 2024 in IEEE Transactions on Electron Devices
To address the concerns on the retention loss of HfO2-based ferroelectric (FE) devices in versatile applications, we conduct a comprehensive wide temperature range (250–400 K) characterization on a 9-nm Hf0.5Zr0.5O2 (HZO) film. It reveals that the retention will be damaged by the high temperature and incomplete polarization (fast speed and low amplitude operation). The dominant mechanism is believed to be the imprint effect, which occurs due to the migration of charged defects to the interface along the internal field caused by incomplete polarization. By addressing the intricacies of imprint behaviors and incomplete polarization, this work illuminates crucial aspects of retention loss in FE-HZO thin films.
To gain insight into the ferroelectric mechanisms under reduced thermal budget and thickness scaling, a 4.6 nm ultra-thin ferroelectric Hf0.5Zr0.5O2 capacitor compatible with back-end-of-line (BEOL) processes (all conducted at temperatures ≤350 °C) is investigated in this work. Through O3 pretreatment at the bottom electrode (BE) interface and controlled temperature modulation of the crystalline phase, the capacitor exhibits exceptional ferroelectric (FE) properties following low-temperature (350 °C) and long-term (300 s) rapid thermal annealing (RTA). These properties include high remanent polarization (2Pr ∼ 28.53 μC/cm2), low coercive voltage (Vc ∼ 0.43 V), effective leakage suppression, robust endurance (∼1010 cycles without hard breakdown), and a desirable high dielectric constant. The main mechanisms identified include tetragonal phase nucleation under enhanced tensile stress via the oxidized BE layer (TiO2), crystalline growth controlled through RTA temperature modulation, and phase transition to the ferroelectric orthorhombic phase under electric field cycling. This research provides valuable insights for the development of BEOL-compatible nonvolatile FE memories.
HfO2-based ferroelectric materials offer a promising alternative for next-generation memory technology. Atomic layer deposition (ALD) temperature can significantly influence the physical and chemical properties of films, enabling compatibility with back-end-of-line (BEOL) thermal budgets; however, it also inevitably affects polarization switching dynamics, warranting further investigation. In this work, BEOL-compatible Hf0.5Zr0.5O2 (HZO) films are fabricated at various ALD temperatures, and their polarization switching dynamics is characterized using the nucleation-limited switching model. Higher ALD temperatures result in faster polarization switching speeds and reduced asymmetry during program and erase stages, while lower ALD temperatures promote uniform polarization, although capacitors across all temperatures display similar remnant polarization (Pr) values after wakeup. Detailed analysis suggests that the influence of ALD temperature on preexisting oxygen vacancies (Vo) may be the underlying factor.